Corrosion-resistant coating for protection of GTE details made of high-strength maraging constructional steel with operating temperature up to 450°C

Galoyan A.G., Muboyadzhyan S.A., Egorova L.P., Bulavintseva E.E.
Galoyan A.G., Muboyadzhyan S.A., Egorova L.P., Bulavintseva E.E. Corrosion-resistant coating for protection of GTE details made of high-strength maraging constructional steel with operating temperature up to 450°C // Proceedings of VIAM. 2014. No. 6. DOI: 10.18577/2307-6046-2014-0-6-3-3. URL: https://www.viam-works.ru/en/journal/2014/6/3
Abstract

This article provides results of developing corrosion-resistant coating and application technology for protecting GTE details made of high-strength maraging constructional steel VKS-170 from salt corrosion at up to 450°C. Results of corrosion-resistance, heat-resistance, creep rupture strength and high-cycle fatigue tests, as well as metallographic analysis of specimens after testing are provided.

Reference list
  1. Kablov E.N. Strategicheskie napravleniya razvitiya materialov i tehnologiy ih pererabotki na period do 2030 goda [Strategic directions of development of materials and technologies to process them for the period up to 2030] //Aviatsionnye materialy i tehnologii. 2012. №S. S. 7–17.
  2. Muboyadzhyan S.A. Perspektivnye pokrytiya dlya detaley aviadvigateley [Promising coatings for aircraft engine parts] //Voennyj parad. 2009. №1 (91). S. 33.
  3. Budinovskiy S.A., Kablov E.N., Muboyadzhyan S.A. Primenenie analiticheskoy modeli opredeleniya uprugih napryazheniy v mnogosloynoy sisteme pri reshenii zadach po sozdaniyu vysokotemperaturnyh zharostoykih pokrytiy dlya rabochih lopatok aviatsionnyh turbin [Application of the analytical model of elastic stresses in a multilayer system with the task of building high-temperature coatings for aviation turbine blades workers] //Vestnik MGTU im. N.E. Baumana. Ser. «Mashinostroenie». 2011. №SP2. S. 26–37.
  4. Muboyadzhyan S.A., Lutsenko A.N., Aleksandrov D.A., Gorlov D.S. Issledovanie vozmozhnosti povysheniya sluzhebnyh harakteristik lopatok kompressora GTD metodom ionnogo modifitsirovaniya poverhnosti [Research opportunities to improve service characteristics of the compressor blades GTE ion-surface modification] //Trudy VIAM. 2013. №1. St. 02 (viam-works.ru).
  5. Kablov E.N. Razrabotki VIAM dlya gazoturbinnyh dvigateley i ustanovok [VIAM development for gas turbine engines and installations] //Kryl'ya rodiny. 2010. №4. S. 31–33.
  6. Muboyadzhyan S.A., Aleksandrov D.A., Gorlov D.S. Nanosloynye uprochnyayuschie pokrytiya dlya zaschity stal'nyh i titanovyh lopatok kompressora GTD [Nanolayer strengthening coatings for protection of steel and titanium turbine engine compressor blades] //Aviatsionnye materialy i tehnologii. 2011. №3. S. 3–8.
  7. Sposob alitirovaniya poverhnosti vnutrenney polosti lopatki turbiny iz zharoprochnogo splava [Method aluminizing the inner cavity surface of a turbine blade of a superalloy]: pat. 2382830 Ros. Federatsiya; opubl. 13.08.2008.
  8. Muboyadzhyan S.A., Aleksandrov D.A., Gorlov D.S., Egorova L.P., Bulavintseva E.E. Zaschitnye i uprochnyayuschie ionno-plazmennye pokrytiya dlya lopatok i drugih otvetstvennyh detaley kompressora GTD [Protecting and strengthening the ion-plasma coatings for blades and other critical parts of the compressor turbine engine] //Aviatsionnye materialy i tehnologii. 2012. №S. S. 71–81.
  9. Lutsenko A.N., Muboyadzhyan S.A., Budinovskiy S.A. Promyshlennye tehnologicheskie protsessy ionnoy obrabotki poverhnosti [Industrial processes ionic surface treatment] /V sb.: Aviatsionnye materialy i tehnologii. M.: VIAM. 2005. №1. S. 30–40.
  10. Muboyadzhyan S.A. Osobennosti osazhdeniya iz dvuhfaznogo potoka mnogokompo-nentnoy plazmy vakuumno-dugovogo razryada, soderzhaschego mikrokapli isparyae-mogo materiala [Features deposition of two-phase flow of a multicomponent plasma vacuum arc containing microdroplets of the evaporated material] //Metally. 2008. №2. S. 20–34.
  11. Azarovskiy E.N., Muboyadzhyan S.A. Modifitsirovanie poverhnosti detaley iz konstruktsionnyh staley v vakuumno-dugovoy plazme titana [Surface modification of parts made of structural steel in the vacuum arc plasma titanium] //Aviatsionnye materialy i tehnologii. 2013. №3. S. 20–25.
  12. Sposob naneseniya pokrytiya dlya zaschity ot vysokotemperaturnogo okisleniya poverhnosti vnutrenney polosti ohlazhdaemyh lopatok turbin iz bezuglerodistyh zharo-prochnyh splavov na osnove nikelya [The method of coating for protection against high-temperature oxidation of the inner cavity cooled turbine blades of carbon-free heat-resistant nickel-based alloys]: pat. 2471887 Ros. Federatsiya; opubl. 17.10.2011.
  13. Sposob naneseniya kombinirovannogo zharostoykogo pokrytiya [Method of application of combined heat-resistant coating]: pat. 2402633 Ros. Federatsiya; opubl. 31.03.2009.
  14. Kablov E.N., Muboyadzhyan S.A., Budinovskiy S.A. Ionno-plazmennye zaschitnye pokrytiya dlya lopatok gazoturbinnyh dvigateley [Ion-plasma protective coatings for gas turbine engine blades] //Metally. 2007. №5. S. 23–34.
  15. Belous V.Ya., Varlamova V.E., Muboyadzhyan S.A., Aleksandrov D.A. Ionno-plazmennye pokrytiya dlya zaschity ot korrozii kompressornyh lopatok i drugih detaley GTD, ekspluatiruyuschihsya vo vseklimaticheskih usloviyah [Ion-plasma coatings for corrosion protection of compressor blades and other parts of GTE, operated in all climate conditions] //Korroziya: materialy, zaschita. 2012. №1. S. 20–24.
  16. Ustanovka dlya naneseniya zaschitnyh pokrytiy [Apparatus for applying protective coatings]: pat. 2318078 Ros. Federatsiya; opubl. 26.06.2006.
  17. Sposob polucheniya litogo trubnogo katoda iz splavov na osnove alyuminiya dlya ionno-plazmennogo naneseniya pokrytiy [A method for producing molded pipe cathode aluminum-based alloys for ion-plasma coating]: pat. 2340426 Ros. Federatsiya; opubl. 16.04.2007.
  18. Sposob polucheniya alyuminidnogo pokrytiya na poverhnosti izdeliya iz zharoprochnogo splava [A method of producing aluminide coating on the surface of the superalloy article]: pat. 2348739 Ros. Federatsiya; opubl. 16.04.2007.
  19. Sposob polucheniya lityh trubnyh izdeliy iz splavov na osnove nikelya i/ili kobal'ta [A method for producing tubular products of cast alloys based on nickel and/or cobalt]: pat. 2344019 Ros. Federatsiya; opubl. 16.04.2007.
  20. Kablov E.N., Muboyadzhyan S.A. Ionnoe travlenie i modifitsirovanie poverhnosti ot-vetstvennyh detaley mashin v vakuumno-dugovoy plazme [Ion etching and surface modification of critical components of machinery on a vacuum arc plasma] //Vestnik MGTU im. N.E. Baumana. Ser. «Mashinostroenie». 2011. №SP2. S. 149–163.
  21. Sostav dlya polucheniya korrozionnostoykogo i zharostoykogo pokrytiya na detalyah iz konstruktsionnyh staley ili zharoprochnyh splavov na osnove nikelya [Composition for corrosion and heat-resistant coating on the details of structural steels and superalloys based on nickel]: pat. 2455390 Ros. Federatsiya; opubl. 10.04.2012.
  22. Salahova R.K. Korrozionnaya stoykost' stali 30HGSA s «trehvalentnym» hromovym pokrytiem v estestvennyh i iskusstvennyh sredah [The corrosion resistance of steel with 30KhGSA «trivalent» chromium plated in natural and artificial environments] //Aviatsionnye materialy i tehnologii. 2012. №2. S. 59–66.