Determination of silicon carbide and aluminum nitride in the sealing material on the basis of nickel

Titov V.I., Goundobin N.V., Pilipenko L.V., Dvoretskov R.M.
Titov V.I., Goundobin N.V., Pilipenko L.V., Dvoretskov R.M. Determination of silicon carbide and aluminum nitride in the sealing material on the basis of nickel // Proceedings of VIAM. 2014. No. 5. DOI: 10.18577/2307-6046-2014-0-5-3-3. URL: https://www.viam-works.ru/en/journal/2014/5/3
Abstract

A method for determination of silicon carbide and aluminum nitride in uplotnitel′nom material based on nickel. Error of definition of these components does not exceed 5% RH.

Reference list
  1. Migunov V.P. Materialy dlja uplotnenij protochnoj chasti GTD [Sealants flowing part of GTD] /V sb. Voprosy aviacionnoj nauki i tehniki. Ser. Aviacionnye materialy. Vyp. Up-lotnitel'nye materialy dlja protochnoj chasti GTD. M.: VIAM. 1992. S. 5–8.
  2. Migunov V.P., Farafonov D.P., Degovec M.L., Stupina T.I. Uplotnitel'nye materialy dlja protochnogo trakta GTD [Sealing materials for flow path GTE] //Aviacionnye materialy i tehnologii. 2012. №S. S. 94–97.
  3. Kuznecov E.G., Majler D.P., Pochuev V.P. Primenenie istiraemyh uplotnenij v pro-tochnoj chasti GTD [Application abradable seals in the running part of GTE] /V sb. Vo-prosy aviacionnoj nauki i tehniki. Ser. Aviacionnye materialy. Vyp. Uplotnitel'nye ma-terialy dlja protochnoj chasti GTD. M.: VIAM. 1992. S. 8–13.
  4. Kablov E.N. Strategicheskie napravlenija razvitija materialov i tehnologij ih pererabotki na period do 2030 goda [Strategic directions of development of materials and technolo-gies to process them for the period up to 2030] //Aviacionnye materialy i tehnologii. 2012. №S. S. 7–17.
  5. Ospennikova O.G. Strategija razvitija zharoprochnyh splavov i stalej special'nogo naznachenija, zashhitnyh i teplozashhitnyh pokrytij [The development strategy of sup-eralloys and special steel, protective and thermal barrier coatings] //Aviacionnye mate-rialy i tehnologii. 2012. №S. S. 19–36.
  6. Kablov E.N., Petrushin N.V., Svetlov I.L., Demonis I.M. Nikelevye zharoprochnye splavy novogo pokolenija [Nickel superalloys new generation] //Aviacionnye materialy i tehnologii. 2012. №S. S. 36–52.
  7. Kablov E.N., Mubojadzhjan S.A. Zashhitnye pokrytija lopatok turbin perspektivnyh GTD [Protective coating turbine blades looking GTE] //GTT. 2001. №3 (12). S. 30–32.
  8. Budinovskij S.A., Mubojadzhjan S.A., Gajamov A.M., Stepanova S.V. Ionno-plazmennye zharostojkie pokrytija s kompozicionnym bar'ernym sloem dlja zashhity ot okislenija splava ZhS36-VI [Ion-plasma heat-resistant composite coating with a barrier layer to prevent the oxidation of the alloy ZHS36-VI] //MiTOM. 2011. №1. S. 34–49.
  9. Mubojadzhjan S.A. Osobennosti osazhdenija iz dvuhfaznogo potoka mnogokomponent-noj plazmy vakuumno-dugovogo razrjada, soderzhashhego mikrokapli isparjaemogo materiala [Features deposition of two-phase flow of a multicomponent plasma vacuum arc containing microdroplets of the evaporated material] //Metally. 2008. №2. S. 20–34.
  10. Mubojadzhjan S.A., Aleksandrov D.A., Gorlov D.S. Ionno-plazmennye i nanoslojnye jerozionnostojkie pokrytija na osnove karbidov i nitridov metallov [Ion-plasma and Nanolayer erosionproofed coatings based on carbides and nitrides] //Metally. 2010. №5. S. 39–51.
  11. Mubojadzhjan S.A., Lucenko A.N., Aleksandrov D.A., Gorlov D.S., Zhuravleva P.L. Issledovanie svojstv nanoslojnyh jerozionnyh pokrytij na osnove karbidov i nitridov metallov [Investigation of the properties nanolayer erosion coatings based on carbides and nitrides] //Metally. 2011. №4. S. 91–101.
  12. Mubojadzhjan S.A., Aleksandrov D.A., Gorlov D.S., Egorova L.P., Bulavinceva E.E. Zashhitnye i uprochnjajushhie ionno-plazmennye pokrytija dlja lopatok i drugih ot-vetstvennyh detalej kompressora GTD [Protecting and strengthening the ion-plasma coatings for blades and other critical parts of the compressor turbine engine] //Aviacionnye materialy i tehnologii. 2012. №S. S. 71–81.
  13. Kablov E.N., Mubojadzhjan S.A., Budinovskij S.A, Lucenko A.N. Ionno-plazmennye zashhitnye pokrytija dlja lopatok gazoturbinnyh dvigatelej [Ion-plasma protective coat-ings for gas turbine engine blades] //Metally. 2007. №5. S. 23–34.
  14. Mubojadzhjan S.A., Lucenko A.N., Aleksandrov D.A., Gorlov D.S. Issledovanie vozmozhnosti povyshenija sluzhebnyh harakteristik lopatok kompressora GTD metodom ionnogo modificirovanija poverhnosti [Research opportunities to improve service characteristics of the compressor blades GTE ion-surface modification] //Trudy VIAM. 2013. №1. St. 02 (viam-works.ru).
  15. Kablov E.N., Mubojadzhjan S.A. Teplozashhitnye pokrytija dlja lopatok turbiny vysokogo davlenija perspektivnyh GTD [Thermal barrier coatings for turbine blades of high pressure promising GTD] //Metally. 2012. №1. S. 5–13.
  16. Kablov E.N., Solncev S.S., Rozenenkova V.A., Mironova N.A. Sovremennye poli-funkcional'nye vysokotemperaturnye pokrytija dlja nikelevyh splavov, uplotnitel'nyh metallicheskih voloknistyh materialov i berillievyh splavov [Modern polyfunctional high-nickel alloy coatings, sealing materials and fibrous metal beryllium] //Novosti ma-terialovedenija. Nauka i tehnika. 2013. №1 (materialsnews.ru).
  17. Sposob nanesenija pokrytija dlja zashhity ot vysokotemperaturnogo okislenija pover-hnosti vnutrennej polosti ohlazhdaemyh lopatok turbin iz bezuglerodistyh zharo-prochnyh splavov na osnove nikelja [The method of coating for protection against high-temperature oxidation of the inner cavity cooled turbine blades of carbon-free heat-resistant nickel-based alloys]: pat. 2471887 Ros. Federacija; opubl. 17.10.2011.
  18. Sposob nanesenija kombinirovannogo zharostojkogo pokrytija [Method of application of combined heat-resistant coating]: pat. 2402633 Ros. Federacija; opubl. 31.03.2009.
  19. Dospehi dlja «Burana». Materialy i tehnologii VIAM dlja MKS «Jenergija–Buran» [Armor for the «Buran». Materials and technologies for VIAM ISS «Energia-Buran»] /Pod obshh. red. Kablova E.N. M.: Fond «Nauka i zhizn'». 2013. S. 44.
  20. Samsonov G.V. Fiziko-himicheskie i mehanicheskie svojstva karbidov i nitridov bora i kremnija [Physico-chemical and mechanical properties of the carbides and nitrides of boron and silicon] /V sb. informacionnyh materialov «Metallokeramicheskie materialy i metody ih issledovanija». Kiev: Izd-vo USSR. 1959. S. 36–39.
  21. Himicheskaja jenciklopedija [Chemical encyclopedia]: V 5 tomah. M.: Sovetskaja jenciklopedija. 1988. T. 1. S. 212; T. 2. S. 624; T. 3. S. 508–510.
  22. Storms Je. Tugoplavkie karbidy [Refractory carbides]: Per. s angl. M. 1970. 170 s.
  23. Tot L. Karbidy i nitridy perehodnyh metallov [Carbides and nitrides of transition met-als]: Per. s angl. M. 1974. 260 s.
  24. Bolgar A.S., Litvinenko V.F. Termodinamicheskie svojstva nitridov [Thermodynamic properties of nitrides]. Kiev. 1980. 210 s.
  25. Gnesin G.G. Karbidokremnievye materialy [Silicon carbide materials]. M. 1977. 110 s.