Abstract

New heat-resistant coating for protection against high-temperature oxidation of tur-bine parts made of intermetallic nickel-based superalloy working at 1100–1200°С is developed. Research of heat-resistance, evolution of composition and structure of doped ion-plasma coatings for intermetallic superalloy is made.

Reference list
  1. Kablov E.N. Strategicheskie napravlenija razvitija materialov i tehnologij ih pererabotki na period do 2030 goda [Strategic directions of development of materials and technologies to process them for the period up to 2030] //Aviacionnye materialy i tehnologii. 2012. №S. S. 7–17.
  2. Inozemcev A.A., Nihamkin M.A., Sandrackij V.L. Osnovy konstruirovanija aviacionnyh dvigatelej i jenergeticheskih ustanovok [Basis for designing aircraft engines and power plants]. M.: Mashinostroenie. 2008. T. 2. S. 159–192.
  3. Kablov E.N., Sidorov V.V., Kablov D.E., Rigin V.E., Gorjunov A.V. Sovremennye tehnologii poluchenija prutkovyh zagotovok iz litejnyh zharoprochnyh splavov novogo pokolenija [Modern technologies for bar stock of casting superalloys new generation] //Aviacionnye materialy i tehnologii. 2012. №S. S. 97−105.
  4. Kablov E.N., Ospennikova O.G., Vershkov A.V. Redkie metally i redkozemel'nye jelementy – materialy sovremennyh i budushhih vysokih tehnologij [Rare metals and rare earth elements – materials of current and future high-tech] //Trudy VIAM. 2013. №2. St. 01 (viam-works.ru).
  5. Kablov E.N., Petrushin N.V., Svetlov I.L., Demonis I.M. Nikelevye litejnye zharoprochnye splavy novogo pokolenija [Casting nickel superalloys new generation] //Aviacionnye materialy i tehnologii. 2012. №S. S. 36–52.
  6. Bazyleva O.A., Arginbaeva Je.G., Turenko E.Ju. Zharoprochnye litejnye intermetallidnye splavy [Heat-resistant casting intermetallic alloys] //Aviacionnye materialy i tehnologii. 2012. №S. S. 57–60.
  7. Kablov E.N., Bondarenko Ju.A., Echin A.B., Surova V.A., Kablov D.E. Razvitie processa napravlennoj kristallizacii lopatok GTD iz zharoprochnyh i intermetallidnyh splavov s monokristallicheskoj strukturoj [The development process of directional solidification of high-temperature gas turbine engine blades and intermetallic alloys with a single-crystal structure] //Vestnik MGTU im. N.Je. Baumana. Ser. «Mashinostroenie». 2011. №SP2. S. 20–25.
  8. Splav na osnove intermetallida Ni3Al [Alloy based on Ni3Al intermetallic]: pat. 2434067 Ros. Federacija; opubl. 01.07.2010.
  9. Splav na osnove intermetallida Ni3Al [Alloy based on Ni3Al intermetallic]: pat. 2434068 Ros. Federacija; opubl. 05.10.2010.
  10. Zharoprochnyj splav na nikelevoj osnove dlja monokristallicheskogo lit'ja [Superalloy based on nickel single crystal casting]: pat. 2439184 Ros. Federacija; opubl. 05.10.2010.
  11. Kablov E.N., Ospennikova O.G., Bazyleva O.A. Materialy dlja vysokoteplonagruzhennyh detalej gazoturbinnyh dvigatelej [Materials for high-thermal components of gas turbine engines] //Vestnik MGTU im. N.Je. Baumana. Ser. «Mashinostroenie». 2011. №SP2. S. 13–19.
  12. Kablov E.N., Mubojadzhjan S.A. Zharostojkie i teplozashhitnye pokrytija dlja lopatok turbiny vysokogo davlenija perspektivnyh GTD [Heat-resistant and heat-protective coatings for high-pressure turbine blades looking GTE] //Aviacionnye materialy i tehnologii. 2012. №S. S. 60–70.
  13. Kablov E.N., Mubojadzhjan S.A. Ionnoe travlenie i modificirovanie poverhnosti ot-vetstvennyh detalej mashin v vakuumno-dugovoj plazme [Ion etching and surface modification of critical components of machinery on a vacuum arc plasma] //Vestnik MGTU im. N.Je. Baumana. Ser. «Mashinostroenie». 2011. №SP2. S. 149–163.
  14. Kablov E.N., Muboyadzhyan S.A. Heat-resistant coatings for the high-pressure turbine blades of promising gtes //Russian metallurgy (Metally). 2012. №1. S. 1–7.
  15. Matveev P.V., Budinovskij S.A., Mubojadzhjan S.A., Kos'min A.A. Zashhitnye zharostojkie pokrytija dlja splavov na osnove intermetallidov nikelja [Heat-resistant protective coatings for intermetallic alloys based on nickel] //Aviacionnye materialy i tehnologii. 2013. №2. S. 12–15.
  16. Mubojadzhjan S.A., Aleksandrov D.A., Gorlov D.S., Egorova L.P., Bulavinceva E.E. Zashhitnye i uprochnjajushhie ionno-plazmennye pokrytija dlja lopatok i drugih otvetstvennyh detalej kompressora GTD [Protecting and strengthening the ion-plasma coatings for blades and other parts of responsibility compressor GTE] //Aviacionnye materialy i tehnologii. 2012. №S. S. 71–81.