The methods of determination of Al2O3 single-crystal fibers cross-section area for tensile strength calculation

Nikitina V.J., Kolyshev S.G., Kuptsov R.S.
Nikitina V.J., Kolyshev S.G., Kuptsov R.S. The methods of determination of Al2O3 single-crystal fibers cross-section area for tensile strength calculation // Proceedings of VIAM. 2014. No. 2. DOI: 10.18577/2307-6046-2014-0-2-3-3. URL: https://www.viam-works.ru/en/journal/2014/2/3
Abstract

Three methods of determnation of single-crystal fibers cross-section area are pre-sented in this paper, the optimum variants are chosen and the results of fiber strength calculation after room and high-temperature tensile tests are set out. The inaccuracy caused by temperature expansion of the material is estimated.

Reference list
  1. Kablov E.N. Strategicheskie napravlenija razvitija materialov i tehnologij ih pererabotki na period do 2030 goda [Strategic directions of the development of materials and technologies of their processing for the period until 2030] //Aviacionnye materialy i tehnologii. 2012. №S. S. 7–17.
  2. Grashhenkov D.V., Chursova L.V. Strategija razvitija kompozicionnyh i funkcional'nyh materialov [Strategy of development of composite and functional materials] //Aviacionnye materialy i tehnologii. 2012. №S. S. 231–242.
  3. Kablov E.N., Shhetanov B.V., Ivahnenko Ju.A., Balinova Ju.A. Perspektivnye armirujushhie vysokotemperaturnye volokna dlja metallicheskih i keramicheskih kompozicionnyh materialov [Perspective reinforcing high-temperature fibers for metal and ceramic composite materials] //Trudy VIAM. 2013. №2. St. 05 (viam-works.ru).
  4. Erasov V.S. Fiziko-mehanicheskie harakteristiki, kak osnovnye integral'nye pokazateli kachestva aviacionnyh konstrukcionnyh materialov [Physicomechanical characteristics, as main integrated indicators of quality of aviation constructional materials]: Metodich. posob. M.: VIAM. 2011. 16 s.
  5. Shhetanov B.V., Bersenev A.Ju., Selivanov E.A. i dr. Nekotorye osobennosti razrushenija oksidnyh keramicheskih kompozicionnyh materialov [Some features of destruction of oxidic ceramic composite materials] //Aviacionnye materialy i tehnologii. 2003. №3. S. 3–7.
  6. Tinjakova E.V., Grashhenkov D.V. Teploizoljacionnyj material na osnove mullito-korundovyh i kvarcevyh volokon [Heat-insulating material on a basis the mullit-korund and quartz fibers] //Aviacionnye materialy i tehnologii. 2012. №3. S. 43–47.
  7. Orlov M.R. Strategicheskie napravlenija razvitija Ispytatel'nogo centra FGUP «VIAM» [Strategic directions of development of the Test center Federal State Unitary Enterprise VIAM] //Aviacionnye materialy i tehnologii. 2012. №S. S. 387–392.
  8. Rossolenko S.N., Kurlov V.N., Asrjan A.A. Analiz profil'nyh krivyh meniskov dlja processa vyrashhivanija kristallov po sposobu Stepanova [The analysis of profile curve meniscuses for process of cultivation of crystals on a way of Stepanov]. Ch. I. //Materialovedenie. 2008. №9. S. 6–16.
  9. Rossolenko S.N., Kurlov V.N., Asrjan A.A Analiz profil'nyh krivyh meniskov dlja processa vyrashhivanija kristallov po sposobu Stepanova [The analysis of profile curve meniscuses for process of cultivation of crystals on a way of Stepanov]. Ch. II //Materialovedenie. 2008. №10. S. 2–8.
  10. Rossolenko S.N., Kurlov V.N., Asrian A.A. Analysis of the profile curves of the menisci for the sapphire tubes growth by EFG (Stepanov) technique //Crystal Research and Technology. 2009. V. 44. №7. P. 689–700.
  11. Rossolenko S.N., Kurlov V.N., Asrian A.A. Analysis of the profile curves of the menisci for the sapphire capillaries and fibers growth by EFG (Stepanov) technique //Crystal Research and Technology. 2009. V. 44. №7. P. 701–706.
  12. Rossolenko S.N., Kurlov V.N., Asrjan A.A. Issledovanie profil'nyh krivyh meniskov dlja processa vyrashhivanija kristallov po sposobu Stepanova [Research of profile curve meniscuses for process of cultivation of crystals on a way of Stepanov] //Izvestija RAN. 2009. T. 73. №10. S. 1398–1402.
  13. Kablov E.N., Shhetanov B.V. Metody poluchenija monokristallicheskih volokon oksida aljuminija dlja kompozicionnyh materialov [Methods of receiving single-crystal fibers of oxide of aluminum for composite materials] /V sb. materialov 29-j ezhegodnoj Mezhdunarodnoj konf. i seminara «Kompozicionnye materialy v promyshlennosti». Jal-ta: 2009. S. 150–155.
  14. Milejko S.T., Serebrjakov A.V., Kijko V.M., Kolchin A.A., Kurlov V.N., Novohatskaja N.I., Tolstun A.N. Monokristallicheskie volokna mullita, poluchaemye metodom vnutrennej kristallizacii [The single-crystal fibers of mullite received by a method of internal crystallization] //Kompozity i nanostruktury. 2009. №2. S. 47–60.
  15. Shhetanov B.V., Kupcov R.S., Svistunov V.I. Metody poluchenija monokristallicheskih volokon oksida aljuminija dlja sozdanija kompozicionnyh materialov i vysoko-temperaturnoj volokonnoj optiki [Methods of receiving single-crystal fibers of oxide of aluminum for creation of composite materials and high-temperature fiber optics] //Trudy VIAM. 2013. №4. St. 01 (viam-works.ru).
  16. Basargin O.V., Nikitina V.Ju., Shheglova T.M., Kolyshev S.G. Osobennosti provedenija prochnostnyh ispytanij v pechi luchevogo nagreva [Features of carrying out strength tests in the furnace of beam heating] //Steklo i keramika. 2013. №2. S. 6–9.
  17. Uchebnik Photoshop [Textbook Photoshop]. 2009.