Determination of silicon content in heat-resistant nickel alloys

Titov V.I., Goundobin N.V., Pilipenko L.V.
Titov V.I., Goundobin N.V., Pilipenko L.V. Determination of silicon content in heat-resistant nickel alloys // Proceedings of VIAM. 2014. No. 12. DOI: 10.18577/2307-6046-2014-0-12-9-9. URL: https://www.viam-works.ru/en/journal/2014/12/9
Abstract

A possibility of determination of silicon content in heat-resistant nickel alloys (HNA) is surveyed in this work. Silicon in amount >0,4% mass. enriches grain boundaries of the alloy promoting precipitation of plate-shaped M6C carbide films and TCP phase formation and reduction in strength and plastic properties. Rhodamine C was applied at the development of a method for determination of the silicon content in the range of 0,005–0,1% mass. in HNA. The experimental part was to prepare a standard silicon solution, to choose optimal conditions for reaction of «silicon molybdic acid – rhodamine C» complex formation, to verify an influence of environment acidity on the salt formation process of silicon mo-lybdate ions with rhodamine C, the complex stability in time. As a result of the work, a method of direct photometry was developed by which the silicon content can be determined in heat-resistant nickel alloys within the concentration range of 0.005–0.1 % mass.

Reference list
  1. Kablov E.N. Strategicheskie napravlenija razvitija materialov i tehnologij ih pererabotki na period do 2030 goda [Strategic directions of development of materials and technologies to process them for the period up to 2030] //Aviacionnye materialy i tehnologii. 2012. №S. S. 7–17.
  2. Kablov E.N., Sidorov V.V., Kablov D.E. i dr. Sovremennye tehnologii poluchenija prutkovyh zagotovok iz litejnyh zharoprochnyh splavov novogo pokolenija [Modern technology of bar stock from the casting of superalloys new generation] //Aviacionnye materialy i tehnologii. 2012. №S. S. 97–105.
  3. Shmotin Ju.N., Starkov R.Ju., Danilov D.V. i dr. Novye materialy dlja perspektivnogo dviga-telja OAO «NPO „Saturn”» [New materials for advanced engine JSC "NPO" Saturn "»] //Aviacionnye materialy i tehnologii. 2012. №2. S. 6–8.
  4. Kablov E.N., Ospennikova O.G., Bazyleva O.A. Materialy dlja vysokoteplonagruzhennyh detalej gazoturbinnyh dvigatelej [Materials for high-thermal components of gas turbine en-gines] //Vestnik MGTU im. N.Je. Baumana. Ser. «Mashinostroenie». 2011. №SP2. C. 13–19.
  5. Kablov E.N., Bondarenko Ju.A., Kablov D.E. Osobennosti struktury i zharoprochnyh svojstv monokristallov 001> vysokorenievogo nikelevogo zharoprochnogo splava, poluchennogo v uslovijah vysokogradientnoj napravlennoj kristallizacii [Features of the structure and properties of single crystals 001> of high-temperature high-rhenium superalloy, obtained under high-gradient directional solidification] //Aviacionnye materialy i tehnologii. 2011. №4. S. 25–31.
  6. Morozova G.I., Timofeeva O.B., Petrushin N.V. Osobennosti struktury i fazovogo sostava vysokorenievogo zharoprochnogo splava [Features of the structure and phase composition high-rhenium superalloy] //MiTOM. 2009. №2 (644). S. 10–16.
  7. Kablov E.N., Petrushin N.V., Nazarkin R.M. Designing of intermetallic Ni3Al-based sup-eralloy /In: 9-th liege conf. Materials for advanced power engineering. 2010. P. 646–651.
  8. Kablov E.N., Ospennikova O.G., Sidorov V.V., Rigin V.E. Proizvodstvo lityh prutkovyh (shihtovyh) zagotovok iz sovremennyh litejnyh vysokozharoprochnyh splavov [Production of cast semifinished (charge) pieces of modern foundry alloys highly heat] /V sb. trudov nauchn.-tehn. konf. «Problemy i perspektivy razvitija metallurgii i mashinostroenija s ispol'zovaniem zavershennyh fundamental'nyh issledovanij i NIOKR». Ekaterinburg: Nauka Servis. 2011. T. 1. S. 31–38.
  9. Aviacija. Jenciklopedija [Aviation. Encyclopedia]. M.: Bol'shaja Rossijskaja jenciklopedija. 1994. S. 201.
  10. Litye lopatki gazoturbinnyh dvigatelej: splavy, tehnologija, pokrytija [Alloy blades of gas turbine engines: alloys, technology, coverage] /Pod obshh. red. E.N. Kablova. 2-e izd. M.: Nauka. 2006. 632 s.
  11. Kablov E.N., Bondarenko Ju.A., Echin A.B., Surova V.A. Razvitie processa napravlennoj kristallizacii lopatok GTD iz zharoprochnyh splavov s monokristallicheskoj i kompozicionnoj strukturoj [The development process of directional solidification of the gas turbine engine blades superalloys with a single-crystal structure and composition] //Aviacionnye materialy i tehnologii. 2012. №1. S. 3–8.
  12. Petrushin N.V., Svetlov I.L., Ospennikova O.G. Litejnye zharoprochnye nikelevye splavy [Casting nickel superalloys] //Vse materialy. Jenciklopedicheskij spravochnik. 2012. №5. S. 15–19.
  13. Kablov E.N., Petrushin N.V., Svetlov I.L., Demonis I.M. Nikelevye litejnye zharoprochnye splavy novogo pokolenija [Casting nickel superalloys new generation] //Aviacionnye materialy i tehnologii. 2012. №S. S. 36–52.
  14. Ospennikova O.G. Temperaturnyj vzlet dlinoj v polveka [The temperature rise in the long half-century] //Nauka i zhizn'. 2012. №7. S. 26–28.
  15. Sidorov V.V., Morozova G.I., Petrushin N.V., Kuleshova E.A. Fazovyj sostav i termosta-bil'nost' litejnogo zharoprochnogo nikelevogo splava s kremniem [Phase composition and thermal stability of the casting heat-resistant nickel alloy with silicon] //Metally. 1990. №1. S. 94–99.
  16. Kablov E.N., Petrushin N.V., Bronfin M.B., Alekseev A.A. Osobennosti monokristallicheskih zharoprochnyh nikelevyh splavov, legirovannyh reniem [Features single-crystal high-temperature nickel alloys doped with rhenium] //Metally. 2006. №5. S. 47–57.
  17. Ospennikova O.G., Svetlov I.L. Vysokotemperaturnye Nb–Si kompozity – zamena monokristallicheskim nikelevym zharoprochnym splavam [High-Nb-Si composites - replacing single crystal nickel superalloy] //Dvigatel'. 2010. №5(71). S. 36–37.
  18. Kablov E.N., Petrushin N.V., Eljutin E.S. Monokristallicheskie zharoprochnye splavy dlja gazoturbinnyh dvigatelej [Single crystal superalloys for gas turbine engines] //Vestnik MGTU im. N.Je. Baumana. Ser. «Mashinostroenie». 2011. №SP2. S. 38–52.
  19. Titov V.I., Gundobin N.V., Pilipenko L.V., Dvoreckov R.M. Opredelenie karbida kremnija i nitrida aljuminija v uplotnitel'nom materiale na osnove nikelja [Determination of silicon carbide and aluminum nitride in the sealing material based on nickel] //Trudy VIAM. 2014. №5. St. 03 (viam-works.ru).
  20. Myshljaeva L.V., Krasnoshhekov V.V. Analiticheskaja himija kremnija [Analytical chem-istry of silicon]. M.: Nauka. 1972. 212 s.
  21. Nikolaeva D.N. Soedinenija molibdovanadofosfornyh geteropolikislot s osnovnymi krasiteljami v fotometricheskih opredelenijah fosfora [Heteropoly compounds molybdenum-vanadium-phosphoric acids with basic dyes in photometric determination of phosphorus] //Talanta. 1973. V. 20. №8. P. 749–754.