Ni–B chemical coating's structure and properties investigation

Vinogradov S.S., Nikiforov A.A., S.V. Balakhonov, Leshchev K.A.
Vinogradov S.S., Nikiforov A.A., S.V. Balakhonov, Leshchev K.A. Ni–B chemical coating's structure and properties investigation // Proceedings of VIAM. 2014. No. 12. DOI: 10.18577/2307-6046-2014-0-12-7-7. URL: https://www.viam-works.ru/en/journal/2014/12/7
Abstract

The microstructure and the phase composition of Ni–B chemical coating have been investigated. The amorphous precipitate is shown to be crystallized during heating, and the layered-columnar structure disappears; microhardness increases and reaches the maximum value of chrome coating’s microhardness. The porosity not changed at 300°C, and thereafter slightly increases at 350‒400°C.

Reference list
  1. Kablov E.N. Strategicheskie napravlenija razvitija materialov i tehnologij ih pererabotki na period do 2030 goda [Strategic directions of development of materials and technologies to process them for the period up to 2030] //Aviacionnye materialy i tehnologii. 2012. №S. S. 7–17.
  2. Kablov E.N. Materialy dlja izdelija «Buran» – innovacionnye reshenija formirovanija shestogo tehnologicheskogo uklada [Materials for the product "Buran" - innovative solutions forming the sixth technological order] //Aviacionnye materialy i tehnologii. 2013. №S1. S. 3–9.
  3. Elagina O.Ju. Tehnologicheskie metody povyshenija iznosostojkosti detalej mashin [Technological methods to improve the wear resistance of machine parts]: Ucheb. posobie. M.: Logos. 2009. 488 s.
  4. Garkunov D.N. Povyshenie iznosostojkosti detalej samoletov [Wear resistance aircraft parts]. M.: Oborongiz. 1960. 142 s.
  5. Tonysheva O.A., Voznesenskaja N.M., Shal'kevich A.B., Petrakov A.F. Issledovanie vlijanija vysokotemperaturnoj termomehanicheskoj obrabotki na strukturu, tehnologicheskie, mehanicheskie i korrozionnye svojstva vysokoprochnoj korrozionnostojkoj stali perehodnogo klassa s povyshennym soderzhaniem azota [Investigation of the effect of high-temperature thermomechanical treatment on the structure, process, mechanical and corrosion properties of high-strength stainless steel transition class with a high content of nitrogen] //Aviacionnye materialy i tehnologii. 2012. №3. S. 31–36.
  6. Tonysheva O.A., Voznesenskaja N.M., Eliseev Je.A., Shal'kevich A.B. Novaja vysokoprochnaja jekonomnolegirovannaja azotsoderzhashhaja stal' povyshennoj nadezhnosti [New high sparingly nitrogen-containing steel of high reliability] //Aviacionnye materialy i tehnologii. 2012. №S. S. 84–88.
  7. Gromov V.I., Kurpjakova N.A., Sedov O.V., Korobova E.N. Vakuumnaja i ionno-plazmennaja himiko-termicheskaja obrabotka otvetstvennyh detalej gazoturbinnyh dvigatelej [Vacuum and ion-plasma chemical-thermal processing of critical parts of gas turbine engines] //Aviacionnye materialy i tehnologii. 2012. №S. S. 147–156.
  8. Ovsepjan S.V., Lukina E.A., Filonova E.V., Mazalov I.S. Formirovanie uprochnjajushhej fazy v processe vysokotemperaturnogo azotirovanija svarivaemogo zharoprochnogo deformiruemogo splava na osnove sistemy Ni‒Co‒Cr [Formation of the reinforcing phase in the high-temperature nitriding process weldable superalloy based wrought alloy of Ni–Co–Cr] //Aviacionnye materialy i tehnologii. 2013. №1. S. 3–8.
  9. Rjabov D.K., Kolobnev N.I., Samohvalov S.V., Mahsidov V.V. Vlijanie predvaritel'nogo estestvennogo starenija na svojstva splava 1913 v iskusstvenno sostarennom sostojanii [Effect of prior natural aging on the properties of the alloy 1913 in the artificially aged condition] //Aviacionnye materialy i tehnologii. 2013. №2. S. 8–11.
  10. Azarovskij E.N., Mubojadzhjan S.A. Modificirovanie poverhnosti detalej iz konstrukcionnyh stalej v vakuumno-dugovoj plazme titana [Surface modification of parts made of structural steel in the vacuum arc plasma titanium] //Aviacionnye materialy i tehnologii. 2013. №3. S. 20–25.
  11. Rjabov D.K., Kolobnev N.I. Izmenenie mehanicheskih svojstv splava 1913 pri dvuhstu-penchatom iskusstvennom starenii [Changes in mechanical properties of the alloy 1913 in the two-stage artificial aging] //Aviacionnye materialy i tehnologii. 2013. №4. S. 3–7.
  12. Solncev St.S. Jerozionnostojkie vlagozashhitnye termoregulirujushhie pokrytija mnogorazovoj teplozashhity orbital'nogo korablja «Buran» [Erosion-resistant waterproof thermal control coating reusable thermal protection orbiter "Buran"] //Aviacionnye materialy i tehnologii. 2013. №S1. S. 94–124.
  13. Ivanov E.V. Sozdanie iznosostojkih i antifrikcionnyh materialov i pokrytij dlja kosmicheskogo korablja «Buran» [Creating a wear-resistant and anti-friction materials and coatings for spacecraft "Buran"] //Aviacionnye materialy i tehnologii. 2013. №S1. S. 142–151.
  14. Azarovskij E.N., Mubojadzhjan S.A. Modificirovanie poverhnosti detalej iz kon-strukcionnyh stalej v vakuumno-dugovoj plazme titana [Surface modification of parts made of structural steel in the vacuum arc plasma titanium]. Chast' II //Aviacionnye materialy i tehnologii. 2014. №1. S. 3–11.
  15. Razuvaev E.I., Kapitanenko D.V. Vlijanie termomehanicheskoj obrabotki na strukturu i svojstva austenitnyh stalej [Effect of thermomechanical treatment on the structure and properties of austenitic steels] //Trudy VIAM. 2013. №5. St. 01 (viam-works.ru).
  16. Rozenenkova V.A., Solncev St.S., Mironova N.A. Tonkoplenochnye pokrytija dlja uplot-nitel'nyh istiraemyh materialov na osnove diskretnyh volokon dlja protochnogo trakta GTD [Thin film coatings for sealing abrasive materials on the basis of discrete fibers to the flow path GTD] //Trudy VIAM. 2013. №5. St. 04 (viam-works.ru).
  17. Markova E.S., Jakusheva N.A., Pokrovskaja N.G., Shal'kevich A.B. Tehnologicheskie osobennosti proizvodstva martensitostarejushhej stali VKS-180 [Technological features of production martensite-aging steel VKS-180] //Trudy VIAM. 2013. №7. St. 01 (viam-works.ru).
  18. Kablov E.N., Lomberg B.S., Ospennikova O.G. Sozdanie sovremennyh zharoprochnyh materialov i tehnologij ih proizvodstva dlja aviacionnogo dvigatelestroenija [The creation of modern high-temperature materials and production technologies for aviation engine] //Kryl'ja Rodiny. 2012. №3–4. S. 34–38.
  19. Bakradze M.M., Ovsepjan S.V., Shugaev S.A., Letnikov M.N. Vlijanie rezhimov zakalki na strukturu i svojstva shtampovok diskov iz zharoprochnogo nikelevogo splava JeK151-ID [Effect of tempering on the structure and properties of the disk forgings of heat-resistant nickel alloy EK151-ID] //Trudy VIAM. 2013. №9. St. 01 (viam-works.ru).
  20. Baldaev L.H. Renovacija i uprochnenie detalej mashin metodami gazotermicheskogo napylenija [Renovation and strengthening of machine parts methods of thermal spraying]. M.: Izd-vo KHT. 2004. 134 s.
  21. Petrov G.L., Burov N.G. Tehnologija i oborudovanie gazoplamennoj obrabotki metallov [Technology and equipment flame treatment of metals]. M.: Mashinostroenie. 1969. 288 s.
  22. Mazalov I.S., Filonova E.V., Lomberg B.S. Formirovanie struktury pri deformacii i termicheskoj obrabotke zagotovok detalej iz nikelevogo vysokoprochnogo svarivaemogo splava VZh172 [Structure formation during the deformation and heat treatment blanks welded high-strength nickel alloy VZH172] //Trudy VIAM. 2013. №12. St. 01 (viam-works.ru).
  23. Kablov E.N., Mubojadzhjan S.A. Ionnoe travlenie i modificirovanie poverhnosti otvetstvennyh detalej mashin v vakuumno-dugovoj plazme [Ion etching and surface modification of critical parts in machines vacuum arc plasma] //Vestnik MGTU im. N.Je. Baumana. Ser. «Mashinostroenie». 2011. №SP2. S. 149–163.
  24. Erasov V.S., Kotova E.A. Jerozionnaja stojkost' aviacionnyh materialov k vozdejstviju tverdyh (pylevyh) chastic [Erosion resistance to the effects of aircraft materials solid (dust) particles] //Aviacionnye materialy i tehnologii. 2011. №3. S. 30–36.
  25. Kablov E.N., Starcev O.V., Krotov A.S., Kirillov V.N. Klimaticheskoe starenie kompozicionnyh materialov aviacionnogo naznachenija. III. Znachimye faktory starenija [Climatic aging of composite materials aviation applications. III. Significant factors of aging] //Deformacija i razrushenie materialov. 2011. №1. S. 34–40.
  26. Bogorad L.Ja. Hromirovanie [Chromium-plating]. L.: Mashinostroenie. 1984. 97 s.
  27. Solodkova L.N., Kudrjavcev V.N. Jelektroliticheskoe hromirovanie [Electrolytic chrome]. M.: Globus. 2007. 191 s.
  28. Beljaev P.P., Zil'berfarb M.I., Garetovskaja M.P. Metallicheskie pokrytija v himicheskom mashinostroenii [Metal coatings in chemical engineering]. Sb. II. M.: Mashgiz. 1951. 144 s.
  29. Borisov V.S., Kasparova E.V. Himicheskoe nikelirovanie [Chemical nickel plating]. Sb. 2. M.: MDNTP im. F.Je. Dzerzhinskogo. 1958.
  30. Vishenkov S.A., Kasparova E.V. Povyshenie iznosostojkosti i zashhita ot korrozii detalej iz chernyh i cvetnyh metallov himicheskim nikelirovaniem [Wear resistance and corrosion protection of ferrous and non-ferrous metal chemical nickel plating] //Bjulleten' obmena proizvodstvenno-tehnicheskim opytom. 1958. №6. 208 s.
  31. Gorbunova K.M., Nikiforova A.A. Fiziko-himicheskie osnovy processa himicheskogo nikelirovanija [Physico-chemical foundations of electroless nickel plating]. M.: AN SSSR. 1960. 448 s.
  32. Rjabchenkov A.V., Velemicina V.I. Himicheskoe nikelirovanie kak sredstvo zashhity perlitnyh stalej ot vysokotemperaturnoj gazovoj korrozii. Vnutrennie naprjazhenija nikel'-fosfornyh pokrytij i ih vlijanie na ustalostnuju prochnost' stali [Chemical nickel plating as a means of protection pearlite steels from high-temperature gas corrosion. Internal voltage nickel-phosphorus coatings and their influence on the fatigue strength of steel] /Trudy CNIITMASh. 1961. №22. 37 s.
  33. Vishenkov S.A., Kasparova E.V. Povyshenie nadezhnosti i dolgovechnosti detalej mashin himicheskim nikelirovaniem [Improving the reliability and durability of machine parts electroless nickel plating]. M.: Mashgiz. 1963. 208 s.
  34. Vansovskaja K.M. Metallicheskie pokrytija, nanesennye himicheskim sposobom [Metal coatings deposited by chemical means]. L.: Mashinostroenie. 1985. 103 s.
  35. Gal'vanicheskie pokrytija v mashinostroenii [Electroplating in mechanical engineering]: Spravochnik v 2-h t. T. 1. /Pod red. M.A. Shlugera. M.: Mashinostroenie. 1985. 248 s.
  36. GOST 9.303–84. Pokrytija metallicheskie i nemetallicheskie neorganicheskie. Obshhie trebovanija k vyboru [Metallic and non-metallic mineral. General requirements for the selection].