A behavioral model of the fibrous material during bending tests

Butakov V.V., Basargin O.V., Babashov V.G., Ivakhnenko Yu.A.
Butakov V.V., Basargin O.V., Babashov V.G., Ivakhnenko Yu.A. A behavioral model of the fibrous material during bending tests // Proceedings of VIAM. 2014. No. 12. DOI: 10.18577/2307-6046-2014-0-12-6-6. URL: https://www.viam-works.ru/en/journal/2014/12/6
Abstract

The paper considers the behavior features of a flexible fibrous material during the bending test. A behavioral model of the flexible fibrous material during bending tests is suggested. This model shows the relationship between ability of the material to withstand bending stress and its ability to the elastic compression and tension. The article describes the correlation between the minimum bend radius and elasticity module at compressive and tension. Proposals on ways to enhance flexibility of the fibrous material are given.

Reference list
  1. Hejg Dzh.R., Linch Dzh.F. i dr. Ogneupory dlja kosmosa [Refractories for space]. M. Metallurgija. 1967. 268 s.
  2. Mnogorazovyj orbital'nyj korabl' «Buran» [Reusable orbital ship "Buran"] /Pod red. Ju.P. Semenova, G.E. Lozino-Lozinskogo. M.: Mashinostroenie. 1995. 448 s.
  3. Kablov E.N. Strategicheskie napravlenija razvitija materialov i tehnologij ih pererabotki na period do 2030 goda [Strategic directions of development of materials and technologies to process them for the period up to 2030] //Aviacionnye materialy i tehnologii. 2012. №S. S. 7‒17.
  4. Kablov E.N. Materialy dlja izdelija «Buran» – innovacionnye reshenija formirovanija shestogo tehnologicheskogo uklada [Materials for the product "Buran" - innovative solutions forming the sixth technological order] //Aviacionnye materialy i tehnologii. 2013. №S1. S. 3–9.
  5. Kablov E.N., Shhetanov B.V., Ivahnenko Ju.A., Balinova Ju.A. Perspektivnye armirujushhie vysokotemperaturnye volokna dlja metallicheskih i keramicheskih kompozicionnyh materialov [Prospective reinforcing fibers for high temperature ceramic composites and metal materials] //Trudy VIAM. 2013. №2. St. 05 (viam-works.ru).
  6. Kablov E.N., Grashhenkov D.V., Isaeva N.V. i dr. Perspektivnye vysokotemperaturnye keramicheskie kompozicionnye materialy [Promising high-temperature ceramic composite materials] //Rossijskij himicheskij zhurnal. 2010. T. LIV. №1. S. 20–24.
  7. Grashhenkov D.V., Balinova Ju.A., Tinjakova E.V. Keramicheskie volokna oksida aljuminija i materialy na ih osnove [Ceramic alumina fibers and materials based on them] //Steklo i keramika. 2012. №4. S. 32‒36.
  8. Kablov E.N., Ivahnenko Ju.A., Balinova Ju.A., Semenova E.V. Volokna dioksida cirkonija dlja novogo pokolenija materialov aviacii i kosmosa [Zirconium fibers for a new generation of materials Air and Space] /V sb. materialov XXV jubilejnoj Mezhdunarodnoj konf. i vystavki «Kompozicionnye materialy v promyshlennosti». Jalta: Mir kompozitov. 2005. S. 320‒323.
  9. Shhetanov B.V., Balinova Ju.A., Ljuljukina G.Ju., Solov'eva E.P. Struktura i svojstva nepreryvnyh polikristallicheskih volokon α-Al2O3 [Structure and properties of continuous fibers of polycrystalline α-Al2O3] //Aviacionnye materialy i tehnologii. 2012. №1. S. 13‒17.
  10. Kablov E.N., Shhetanov B.V. Metody poluchenija monokristallicheskih volokon oksida aljuminija dlja kompozicionnyh materialov [Methods of obtaining single-crystal aluminum oxide fibers for composite materials] /V sb. materialov XXIX ezhegodnoj Mezhdunarodnoj konf. i seminara «Kompozicionnye materialy v promyshlennosti». Jalta. 2009. S. 150‒155.
  11. Milejko S.T., Serebrjakov A.V., Kijko V.M. i dr. Monokristallicheskie volokna mullita, poluchaemye metodom vnutrennej kristallizacii [Monocrystalline mullite fiber, obtained by internal crystallization] //Kompozity i nanostruktury. 2009. №2. S. 47‒60.
  12. Shhetanov B.V., Kupcov R.S., Svistunov V.I. Metody poluchenija monokristallicheskih volokon oksida aljuminija dlja sozdanija kompozicionnyh materialov i vysokotemperaturnoj volokonnoj optiki [Methods for obtaining polycrystalline alumina fibers to create a high-temperature composite materials and fiber optics] //Trudy VIAM. 2013. №4. St. 01 (viam-works.ru).
  13. Balinova Ju.A. Nepreryvnye polikristallicheskie volokna oksida aljuminija dlja kompozicionnyh materialov [Continuous polycrystalline alumina fibers for composite materials]: Avtoref. dis. k.t.n. M. 2012. 20 s.
  14. Sposob poluchenija neorganicheskogo voloknistogo materiala [A method of producing an inorganic fiber material]: pat. 2213074 Ros. Federacija; opubl. 27.09.2003.
  15. Proizvodstvo formovannogo produkta na osnove volokna oksida aljuminija [Production of a molded product based on alumina fibers]: pat. 5319949 Japonija; opubl. 03.12.1993.
  16. Janssen R. Reaction Formed Alumina-Alumina FRCMC /Rolf Janssen /In: 7-th International Conference on High Temperature Ceramic Matrix Composites (HT-CMC 7). Bayreuth. 2010. С. 398‒414.
  17. Zhang Y., Ding Y., Gao J. Mullite fibres prepared by sol–gel method using polyvinyl butyral //J. of the European Ceramic Society. 2009. V. 29. №6. Р. 1101‒1107.
  18. Tinjakova E.V., Grashhenkov D.V. Teploizoljacionnyj material na osnove mullito-korundovyh i kvarcevyh volokon [Thermal insulation material on the basis of mullite-corundum and quartz fibers] //Aviacionnye materialy i tehnologii. 2012. №3. S. 43‒46.
  19. Ivahnenko Ju.A., Babashov V.G., Zimichev A.M., Tinjakova E.V. Vysokotemperaturnye teploizoljacionnye i teplozashhitnye materialy na osnove volokon tugoplavkih soedinenij [High-temperature insulating and heat-proof materials for fiber-based refractory compounds] //Aviacionnye materialy i tehnologii. 2012. №S. S. 380‒385.
  20. Zhdanov G.S. Fizika tverdogo tela [Solid State Physics]. M.: Izd-vo MGU im. M.V. Lomonosova. 1961. 504 s.
  21. Posac'kij S.L. Opir materialiv [Resistance of materials]. L'vov: Izd-vo L'vovskogo un-ta. 1963. 360 s.