Quality control of magnesium alloy casting and methods of restoration of cast products impermeability

Uridiya Z.P., Mukhina I.Y., Duyunova V.A., Kosarina E.I.
Uridiya Z.P., Mukhina I.Y., Duyunova V.A., Kosarina E.I. Quality control of magnesium alloy casting and methods of restoration of cast products impermeability // Proceedings of VIAM. 2014. No. 12. DOI: 10.18577/2307-6046-2014-0-12-4-4. URL: https://www.viam-works.ru/en/journal/2014/12/4
Abstract

Some of factors causing appearance of microporosity in magnesium alloy castings were researched. Many parts of different configuration and size with a variable degree of microporosity were studied. According to the analysis of data of ML5 alloy parts research, mechanical properties of castings in case of the steady production process depend, mainly, on the wall thickness of the tested part and on the microporosity degree. The degree of damage caused by microporosity is of a major significance. A scale of microporosity for castings made of ML5 and ML5c.p. magnesium alloys was created. The scale determines the relation between the microporosity image intensity when ML5 alloy casting is being x-rayed and mechanical properties of the casting (ultimate strength and elongation) in the damaged area. The new impregnation compounds Anakrol-90 and KP-GS55 for sealing of micropores and restoration of castings impermeability by vacuum-pressure method were suggested.

Reference list
  1. Kornysheva I.S., Volkova E.F., Goncharenko E.S., Muhina I.Ju. Perspektivy primenenija magnievyh i litejnyh aljuminievyh splavov [Prospects for the use of magnesium and aluminum foundry alloys] //Aviacionnye materialy i tehnologii. 2012. №S. S. 212–222.
  2. Kablov E.N. Osnovnye itogi i napravlenija razvitija materialov dlja perspektivnoj aviacionnoj tehniki [The main results and directions of development of promising materials for aircraft equipment] /V sb. 75 let. Aviacionnye materialy. Izbrannye trudy «VIAM» 1932–2007: Jubilejnyj nauch.-tehnich. sb. M.: VIAM. 2007. S. 20–26.
  3. Kablov E.N. Strategicheskie napravlenija razvitija materialov i tehnologij ih pererabotki na period do 2030 goda [Strategic directions of development of materials and technologies to process them on the period up to 2030] //Aviacionnye materialy i tehnologii. 2012. №S. S. 7–17.
  4. Kablov E.N. VIAM: prodolzhenie puti [VIAM: continuation of the path] //Nauka v Rossii. 2012. №3. S. 36–44.
  5. Kablov E.N. Sovremennye materialy – osnova innovacionnoj modernizacii Rossii [Modern materials – the basis of innovative modernization of Russia] //Metally Evrazii. 2012. №3. S. 10–15.
  6. Kablov E.N. Himija v aviacionnom materialovedenii [Chemistry aviation materials] //Rossijskij himicheskij zhurnal. 2010. T. LIV. №1. S. 3–4.
  7. Kablov E.N. Aviakosmicheskoe materialovedenie [Aerospace Materials] //Vse materialy. Jenciklopedicheskij spravochnik. 2008. №3. S. 2–14.
  8. Korchagina V.A. Radi kachestva magnievyh otlivok [For the sake of the quality of magnesium castings] //Inzhenernaja gazeta. 2006. №33–34. S. 5.
  9. Sadkov V.V., Laponov Ju.L., Ageev A.P. i dr. Perspektivy i uslovija primenenija magnievyh splavov v samoletah OAO «Tupolev» [Prospects and conditions of use of magnesium alloys in aircraft JSC "Tupolev"] //Metallurgija mashinostroenija. 2007. №4. S. 19–23.
  10. Antipov V.V., Vahromov R.O., Dujunova V.A., Nochovnaja N.A. Materialy s vysokoj udel'noj prochnost'ju na osnove aljuminija, magnija, titana i tehnologii ih pererabotki [Materials with high specific resistance, based on aluminum, magnesium, titanium, and processing technologies] //Boepripasy i spechimija. 2013. №3. S. 51–55.
  11. Muhina I.Ju., Uridija Z.P. Magnij – osnova sverhlegkih materialov [Magnesium – the basis of ultra-light materials] //Metallurgija mashinostroenija. 2005. №6. S. 29–31.
  12. Dujunova V.A. Metody zashhity magnievyh splavov v otechestvennom litejnom proizvodstve s 1930-h gg. do nastojashhego vremeni [Methods of protection of magnesium alloys in the domestic foundry with the 1930s. up to date] //Litejshhik Rossii. 2010. №10. S. 35–37.
  13. Dujunova V.A., Muhina I.Ju., Uridija Z.P. Novye protivoprigarnye prisadochnye materialy dlja litejnyh form magnievyh otlivok [New antiscorching filler materials for molds magnesium castings] //Litejnoe proizvodstvo. 2009. №9. S. 18–21.
  14. Muhina I.Ju., Dujunova V.A., Uridija Z.P. Perspektivnye litejnye magnievye splavy [Prospective casting magnesium alloys] //Litejnoe proizvodstvo. 2013. №5. S. 2–5.
  15. Dujunova V.A., Goncharenko N.S., Muhina I.Ju. i dr. Nauchnoe nasledie akademika I.N. Fridljandera. Sovremennye issledovanija magnievyh i litej-nyh aljuminievyh splavov v VIAM [Scientific Heritage of Academician I.N. Friedlander. Modern studies of magnesium and cast aluminum alloys VIAM] //Cvetnye metally. 2013. №9. S. 71–78.
  16. Frolov A.V., Muhina I.Ju., Dujunova V.A., Uridija Z.P. Vlijanie tehnologicheskih parametrov plavki na strukturu i svojstva novyh magnievyh splavov [Effect of process parameters on the structure and melting properties of the novel magnesium alloys] //Metallurgija mashinostroenija. 2014. №2. S. 26–29.
  17. Muhina I.Ju. Litejnye splavy i tehprocessy pri proizvodstve magnievyh otlivok [Casting alloys and process technologies in the production of magnesium castings] //Litejnoe proizvodstvo. 2003. №4. S. 18–19.
  18. Goncharenko E.S., Trapeznikov A.V., Ogorodov D.V. Litejnye aljuminievye splavy (k 100-letiju so dnja rozhdenija M.B. Al'tmana) [Casting aluminum alloys (for 100-th anniversary of the birth MB Altman)] //Trudy VIAM. 2014. №4. St. 02 (viam-works.ru).
  19. Mel'nikov N.A. Ob obrazovanii gazovoj poristosti v otlivkah iz aljuminievyh i magnievyh splavov [On the Formation of gas porosity in the casting of aluminum and magnesium alloys] //Litejnoe proizvodstvo. 2006. №2. S. 4.
  20. Al'tman M.B. i dr. Magnievye splavy [Magnesium alloys]: Spravochnik. M.: Metallurgija. 1978. T. 2. S. 147.
  21. Uridija Z.P., Muhina I.Ju. Novye propityvajushhie materialy dlja germetizacii otlivok iz aljuminievyh i magnievyh splavov [New materials for impregnating the sealing castings from aluminum and magnesium alloys] //Vse materialy. Jenciklopedicheskij spravochnik. 2011. №8. S. 37–41.
  22. Uridija Z.P., Muhina I.Ju. O germetizacii otlivok iz aljuminievyh i magnievyh splavov [About sealing castings of aluminum and magnesium alloys] //Litejnoe proizvodstvo. 2012. №2. S. 14–16.
  23. Shishkareva L.M., Kuz'mina N.A. Obzor metodik opredelenija kachestva struktury monokristallicheskih otlivok zharoprochnyh splavov [Review of methods for determining the quality of the structure of single crystal castings of superalloys] //Trudy VIAM. 2014. №1. St. 06 (viam-works.ru).
  24. Postnov V.I., Burhan O.L., Rahmatullin A.Je., Kachura S.M. Nerazrushajushhie metody kontrolja soderzhanija svjazujushhih v prepregah i PKM (obzor) [Non-destructive testing binder content of the prepregs and RMB (review)] //Trudy VIAM. 2013. №12. St. 06 (viam-works.ru).
  25. Murashov V.V. Nerazrushajushhij kontrol' zagotovok i detalej iz uglerod-uglerodnogo kompozicionnogo materiala dlja mnogorazovogo kosmicheskogo korablja «Buran» [Non-destructive testing of blanks and components made of carbon-carbon composite material for the space shuttle "Buran"] //Trudy VIAM. 2013. №4. St. 05 (viam-works.ru).
  26. OST1 90427–94. Kachestvo produkcii. Nerazrushajushhij kontrol' lityh detalej i polufabrikatov aviacionnoj tehniki iz aljuminievyh i magnievyh splavov radiograficheskim metodom. Obshhie polozhenija [Quality products. Nondestructive testing of cast parts and semi-finished aeronautical engineering from aluminum and magnesium alloys by radiography. General provisions].
  27. PI 1.2.226–2008 Nerazrushajushhij kontrol' (NK) metallicheskih izdelij rentgenovskimi metodami [Non-destructive testing (NDT) of metal products X-ray methods].
  28. OST1 90121–90 Magnievye litejnye splavy. Rezhimy termicheskoj obrabotki [Magnesium casting alloys. Heat treatment].
  29. GOST 1497–84 Metally. Metody ispytanija na rastjazhenie [Metals. Test Methods Tensile].
  30. OST1 90248–77 Otlivki fasonnye iz magnievyh splavov. Obshhie tehnicheskie trebovanija [Casting shapes, of magnesium alloys. General specifications].
  31. Moskvichev A.N. Germetizacija por v lityh zagotovkah i izdelijah poroshkovoj metallurgii [Sealing of the pores in the cast billets and powder metallurgy products] //Klei. Germetiki. Tehnologii. 2005. №1. S. 12.
  32. Gurov A.A. Anajerobnye germetizirujushhie materialy «ANATERM» [Anaerobic sealants "Anaterm"] //Klei. Germetiki. Tehnologii. 2004. №5. S. 14.