Modern equipment for turbine blades production designed with a glance of high-gradient directional crystallization process
UDC
629.7.03-226.2
DOI
10.18577/2307-6046-2014-0-12-3-3
Article PDF (Russian)
(644.26 KB)
How to cite
Echin A.B., Bondarenko Yu.A. Modern equipment for turbine blades production designed with a glance of high-gradient directional crystallization process // Proceedings of VIAM. 2014. No. 12. DOI: 10.18577/2307-6046-2014-0-12-3-3. URL: https://www.viam-works.ru/en/journal/2014/12/3
Abstract
An influence of the high-gradient directional crystallization on the structural features (interdendritic distance and porosity) of the superalloys is presented in the paper. The industrial-scale high-gradient unit of UVNS-6 type and some benefits of its use are shown as well. Studies of some test specimens manufactured on UVNS-6 unit completed with measurement of the interdendritic distance were carried out. The temperature gradient was estimated by experimental method.
Reference list
- Kablov E.N., Gerasimov V.V., Visik E.M., Demonis I.M. Rol' napravlennoj kristallizacii v resursosberegajushhej tehnologii proizvodstva detalej GTD [The role of directional solidification in the resource-saving technology of production of gas-turbine] //Trudy VIAM. 2013. №3. St. 01 (viam-works.ru).
- Belikov A.V., Gerasimov V.V., Visik E.M. Tehnologija poluchenija obrazcov dlja attestacii zharoprochnyh splavov, vyplavlennyh s primeneniem othodov litejnogo proizvodstva zavodov otrasli [The technology of obtaining samples for certification superalloys melted using foundry waste branch factories] //Trudy VIAM. 2013. №6. St. 02 (viam-works.ru).
- Litye lopatki gazoturbinnyh dvigatelej: splavy, tehnologii, pokrytija [Alloy blades of gas turbine engines: alloys, technology, coatings] /Pod obshh. red. E.N. Kablova. 2-e izd. M.: Nauka. 2006. 632 s.
- Bondarenko Ju.A., Echin A.B., Surova V.A., Narskij A.R. O napravlennoj kristallizacii zharoprochnyh splavov s ispol'zovaniem ohladitelja [About the directional solidification of superalloys using cooler] //Litejnoe proizvodstvo. 2011. №5. S. 36–39.
- Gerasimov V.V., Visik E.M., Koljadov E.V. O napravlennoj kristallizacii krupnogabaritnyh otlivok na ustanovke UVNK-15 [About the directional solidification of large cast-ings for installation UVNK-15] //Litejnoe proizvodstvo. 2013. №3. S. 21–23.
- Kablov E.N., Bondarenko Ju.A., Echin A.B., Surova V.A. Razvitie processa napravlennoj kristallizacii lopatok GTD iz zharoprochnyh splavov s monokristallicheskoj i kompozicionnoj strukturoj [The development process of directional solidification of the gas turbine engine blades superalloys with a single-crystal structure and composition] //Aviacionnye materialy i tehnologii. 2012. №1. S. 3–8.
- Bondarenko Ju.A., Bazyleva O.A., Echin A.B. i dr. Vysokogradientnaja napravlennaja kristallizacija detalej iz splava VKNA-1V [High-gradient directional solidification of an alloy parts VKNA-1B] //Litejnoe proizvodstvo. 2012. №6. S. 12–16.
- Bondarenko Ju.A., Echin A.B., Surova V.A., Narskij A.R. Vlijanie temperaturnogo gradienta na fronte rosta na strukturu zharoprochnogo splava pri napravlennoj kristallizacii [The influence of the temperature gradient at the growth front on the structure of superalloy with directional solidification] //Litejshhik Rossii. 2014. №5. S. 24–27.
- Kablov E.N., Bondarenko Ju.A., Kablov D.E. Osobennosti struktury i zharoprochnyh svojstv monokristallov 001> vysokorenievogo nikelevogo zharoprochnogo splava, poluchennogo v uslovijah vysokogradientnoj napravlennoj kristallizacii [Structure and properties of single crystals of high-temperature 001> high-rhenium nickel superalloy obtained under high-gradient directional solidification] //Aviacionnye materialy i tehnologii. 2011. №4. S. 25–31.
- Bondarenko Ju.A., Kablov E.N. Napravlennaja kristallizacija zharoprochnyh splavov s povyshennym temperaturnym gradientom [Directional solidification of superalloys with a high temperature gradient] //MiTOM. 2002. №7. S. 20–23.
- Bondarenko Ju.A., Echin A.B., Surova V.A., Narskij A.R. Vlijanie uslovij napravlennoj kristallizacii na strukturu detalej tipa lopatki GTD [Effect of directional solidification conditions on the structure of parts such as blades of GTE] //Litejnoe proizvodstvo. 2012. №7. S. 14–16.
- Kablov E.N., Petrushin N.V., Sidorov V.V., Demonis I.M. Razrabotka monokristallicheskih vysokorenievyh zharoprochnyh nikelevyh splavov metodom komp'juternogo konstruirovanija [Development of single-crystal high-rhenium high-temperature nickel alloys by computer-aided design] /V kn.: Litejnye zharoprochnye splavy. Jeffekt S.T. Kishkina: nauch.-tehn. sb. M.: Nauka. 2006. S. 79–97.
- Echin A.B., Bondarenko Ju.A. Promyshlennaja vysokogradientnaja ustanovka napravlennoj kristallizacii UVNS-6 [Industrial high-gradient directional solidification installation UVNS-6] //Metallurgija mashinostroenija. 2013. №3. S. 32–34.
- Echin A.B., Bondarenko Ju.A. Novaja promyshlennaja vysokogradientnaja ustanovka napravlennoj kristallizacii UVNS-6, ee harakteristiki i preimushhestva [The new indus-trial plant high-gradient directional solidification UVNS-6, its features and benefits] //Novosti materialovedenija. Nauka i tehnika. 2014. №2 (materialsnews.ru).
- Echin A.B., Bondarenko Ju.A. Novaja promyshlennaja vysokogradientnaja ustanovka UVNS-6 dlja poluchenija lopatok i drugih detalej GTD iz litejnyh zharoprochnyh i intermetallidnyh splavov s monokristallicheskoj strukturoj [The new industrial plant UVNS high-gradient-6 for blades and other GTE parts of the casting heat-resistant and intermetallic alloys with the single-crystal structure] //Aviacionnye materialy i tehnologii. 2014 (v pechati).
- Shalin R.E., Svetlov I.L., Kachanov E.B. i dr. Monokristally nikelevyh zharoprochnyh splavov [Single crystals of nickel superalloys]. M.: Mashinostroenie. 1997. 336 s.
- Petrushin N.V., Bronfin M.B., Kablov E.N. i dr. Osobennosti strukturno-fazovyh prevrashhenij pri termicheskoj obrabotke monokristallov vysokorenievyh zharoprochnyh nikelevyh splavov [Features of structural and phase transformations during the heat treat-ment of single crystals of high-rhenium high-temperature nickel alloys] /V kn.: Litejnye zharoprochnye splavy. Jeffekt S.T. Kishkina: nauch.-tehn. sb. M.: Nauka. 2006. S. 142–154.
- Kablov E.N., Bondarenko Ju.A., Echin A.B., Surova V.A., Kablov D.E. Razvitie processa napravlennoj kristallizacii lopatok GTD iz zharoprochnyh i intermetallidnyh splavov s monokristallicheskoj strukturoj [The development process of directional solidification of high-temperature gas turbine engine blades and intermetallic alloys with a single-crystal structure] //Vestnik MGTU im. N.Je. Baumana. Ser. «Mashinostroenie». 2011. №SP2. S. 20–25.
- Kablov E.N. Strategicheskie napravlenija razvitija materialov i tehnologij ih pererabotki na period do 2030 goda [Strategic directions of development of materials and technologies to process them for the period up to 2030] //Aviacionnye materialy i tehnologii. 2012. №S. S. 7–17.