UVNK-type vacuum units for casting of superalloys (review)
UDC
621.74:669.018.44
DOI
10.18577/2307-6046-2014-0-12-2-2
Article PDF (Russian)
(817.86 KB)
How to cite
Belicov A.V., Sinichkina T.S., Visik E.M. UVNK-type vacuum units for casting of superalloys (review) // Proceedings of VIAM. 2014. No. 12. DOI: 10.18577/2307-6046-2014-0-12-2-2. URL: https://www.viam-works.ru/en/journal/2014/12/2
Abstract
Experimental and industrial UVNK-type units of various sizes purposed for casting of heat-resistant alloys not only at VIAM, but also in industrial production are described in the paper. The units listed in the article cover all requirements of large-scale and short-run production providing an opportunity to manufacture cast products of higher quality.
Reference list
- Kablov E.N. Strategicheskie napravlenija razvitija materialov i tehnologij ih pererabotki na period do 2030 goda [Strategic directions of development of materials and technologies to process them for the period up to 2030] //Aviacionnye materialy i tehnologii. 2012. №S. S. 7–17.
- Kablov E.N., Petrushin N.V., Svetlov I.L., Demonis I.M. Nikelevye litejnye zharoprochnye splavy novogo pokolenija [Casting nickel superalloys new generation] //Aviacionnye materialy i tehnologii. 2012. №S. S. 36−52.
- Kablov E.N., Svetlov I.L., Petrushin N.V. Nikelevye zharoprochnye splavy dlja lit'ja lopatok s napravlennoj i monokristallicheskoj strukturoj (Chast' I) [Nickel superalloys for casting blades with directional and single-crystal structure] //Materialovedenie. 1997. №4. S. 32–39.
- Kablov E.N., Svetlov I.L., Petrushin N.V. Nikelevye zharoprochnye splavy dlja lit'ja lopatok s napravlennoj i monokristallicheskoj strukturoj (Chast' II) [Nickel superalloys for casting blades with directional and single-crystal structure] //Materialovedenie. 1997. №5. S. 14–16.
- Belikov A.V., Visik E.M., Gerasimov V.V. Modernizacija oborudovanija dlja napravlennoj kristallizacii – jeffektivnyj put' sovershenstvovanija tehnologii monokristalliche-skogo lit'ja [Modernization of equipment for directional solidification - an effective way of improving the technology of single crystal casting] //Litejnoe proizvodstvo. 2014. №4. S. 34–36.
- Gerasimov V.V., Koljadov E.V., Visik E.M. O napravlennoj kristallizacii krupnogabaritnyh otlivok na ustanovke UVNK-15 [About the directional solidification of large castings for installation UVNK-15] //Litejnoe proizvodstvo. 2013. №3. S. 21–24.
- Belikov A.V., Gerasimov V.V., Visik E.M. Tehnologija poluchenija obrazcov dlja attestacii zharoprochnyh splavov, vyplavlennyh s primeneniem othodov litejnogo proizvodstva zavodov otrasli [The technology of obtaining samples for certification superalloys melted using foundry waste branch factories] //Trudy VIAM. 2013. №6. St. 02 (viam-works.ru).
- Gerasimov V.V., Koljadov E.V. Tehnicheskie harakteristiki i tehnologicheskie vozmozhnosti ustanovok UVNK-9A i VIP-NK dlja poluchenija monokristallicheskih otlivok iz zharoprochnyh splavov [Specifications and technological capabilities installations UVNK-9A and VIP-NK to produce single crystal castings of superalloys] //Litejshhik Rossii. 2012. №11. S. 33–37.
- Kablov E.N., Gerasimov V.V., Visik E.M., Demonis I.M. Rol' napravlennoj kristallizacii v resursosberegajushhej tehnologii proizvodstva detalej GTD [The role of directional solidification in the resource-saving technology of production of gas-turbine] //Trudy VIAM. 2013. №3. St. 01 (viam-works.ru).
- Gerasimov V.V., Visik E.M., Koljadov E.V. Ob osvoenii tehnologii poluchenija krupnogabaritnyh lityh lopatok s monokristallicheskoj strukturoj [About the development of technology for production of large cast blades with single-crystal structure] //Litejnoe proizvodstvo. 2014. №3. S. 29–32.
- Gorjunov A.V., Rigin V.E. Sovremennaja tehnologija poluchenija litejnyh zharoprochnyh nikelevyh splavov [Modern technology of production of heat-resistant nickel alloys casting] //Aviacionnye materialy i tehnologii. 2014. №2. S. 3–7.
- Koljadov E.V., Gerasimov V.V., Visik E.M. Poluchenie krupnogabaritnyh zagotovok diskov turbiny GTD napravlennoj kristallizaciej [Getting large workpieces drives turbines GTE directional solidification] //Litejnoe proizvodstvo. 2013. №10. S. 28–32.
- Bazyleva O.A., Arginbaeva Je.G., Turenko E.Ju. Zharoprochnye litejnye intermetallidnye splavy [Heat-resistant casting intermetallic alloys] //Aviacionnye materialy i tehnologii. 2012. №S. S. 57−60.
- Tolorajja V.N., Ostrouhova G.A., Demonis I.M. Formirovanie monokristallicheskoj struktury lityh krupnogabaritnyh turbinnyh lopatok GTD i GTU na ustanovkah vysokogradientnoj napravlennoj kristallizacii [Formation of a single-crystal structure of large cast turbine blades and turbine engine gas turbine installations on high-gradient directional solidification] //MiTOM. 2011. №1. S. 25–33.
- Gerasimov V.V., Visik E.M. Tehnologicheskie aspekty lit'ja detalej gorjachego trakta GTD iz intermetallidnyh nikelevyh splavov tipa VKNA s monokristallicheskoj strukturoj [Technological aspects of the casting of turbine engine hot section of the intermetallic nickel alloys such VKNA with single-crystal structure] //Litejshhik Rossii. 2012. №2. S. 19–23.
- Kablov E.N., Ospennikova O.G., Sidorov V.V., Rigin V.E., Kablov D.E. Osobennosti tehnologii vyplavki i razlivki sovremennyh litejnyh vysokozharoprochnyh nikelevyh splavov [Features of technology of smelting and casting foundry modern nickel-base superalloys] //Vestnik MGTU im. N.Je. Baumana. Ser. «Mashinostroenie». 2011. №SP2. S. 68–79.
- Koljadov E.V., Gerasimov V.V., Visik E.M. O poluchenii obrazcov dlja jekspress-analiza himsostava zharoprochnyh splavov [On receipt of the samples for the rapid analysis of chemical composition of high-temperature alloys] //Metallurgija. 2012. №3. S. 27–28.
- Kablov E.N., Bondarenko Ju.A., Kablov D.E. Osobennosti struktury i zharoprochnyh svojstv monokristallov 001> vysokorenievogo nikelevogo zharoprochnogo splava, poluchennogo v uslovijah vysokogradientnoj napravlennoj kristallizacii [Structure and properties of single crystals of high-temperature 001> high-rhenium nickel superalloy obtained under high-gradient directional solidification] //Aviacionnye materialy i tehnologii. 2011. №4. S. 25–31.
- Kablov E.N., Petrushin N.V., Bronfin M.B., Alekseev A.A. Osobennosti monokristallicheskih zharoprochnyh nikelevyh splavov, legirovannyh reniem [Features single-crystal high-temperature nickel alloys doped with rhenium] //Metally. 2006. №5. S. 47–57.