Determination of silicon content in aluminium alloys by ICP-AES method in combination with microwave pre-treatment

Zagvozdkina T.N., Karachevtsev F.N., Dvoretskov R.M., Yakimova M.S.
Zagvozdkina T.N., Karachevtsev F.N., Dvoretskov R.M., Yakimova M.S. Determination of silicon content in aluminium alloys by ICP-AES method in combination with microwave pre-treatment // Proceedings of VIAM. 2014. No. 12. DOI: 10.18577/2307-6046-2014-0-12-10-10. URL: https://www.viam-works.ru/en/journal/2014/12/10
Abstract

Silicon is present in aluminum alloys in a wide range of concentrations – from a few hundredths of a percent in heat treatable alloys up to dozens of percent in casting alloys. Existing techniques for determination of silicon content in aluminum alloys are of low accuracy. To solve this problem, a method of silicon mass fraction measurement in aluminum-based alloys by atomic emission spectrometry with inductively coupled plasma (ICP-AES) in combination with microwave preparation of samples has been developed and certified. Mixture compositions for dissolving and microwave-induced decomposition parameters were selected. Limits of relative measurement error for Si mass fraction from 0,001 to 18% do not exceed 5% (±δ, at P=0,95).

Reference list
  1. . Kablov E.N., Antipov V.V., Senatorova O.G. Novyj klass sloistyh aljumostekloplastikov na osnove aljuminijlitievogo splava 1441 s ponizhennoj plotnost'ju [A new class of layered aluminum-fiberglass based aluminum-lithium 1441 alloy with low density] //Vestnik MGTU im. N.Je. Baumana. 2011. №SP2. C. 174–183.
  2. Kablov E.N. Strategicheskie napravlenija razvitija materialov i tehnologij ih pererabotki na period do 2030 goda [Strategic directions of development of materials and technologies to process them for the period up to 2030] //Aviacionnye materialy i tehnologii. 2012. №S. S. 7–17.
  3. Kablov E.N., Ospennikova O.G., Vershkov A.V. Redkie metally i redkozemel'nye jelementy – materialy sovremennyh i budushhih vysokih tehnologij [Rare metals and rare earth elements - materials of current and future high-tech] //Trudy VIAM. 2013. №2. St. 01 (viam-works.ru).
  4. Klochkov G.G., Grushko O.E., Popov V.I. i dr. Struktura, tehnologicheskie svojstva i sva-rivaemost' listov iz splava V-1341 sistemy Al–Mg–Si [Structure, processing properties and weldability of the alloy sheets B 1341 system Al-Mg-Si] //Aviacionnye materialy i tehnologii. 2011. №1. S. 3–8.
  5. Klochkova Ju.Ju., Grushko O.E., Lancova L.P. i dr. Osvoenie v promyshlennom proizvodstve polufabrikatov iz perspektivnogo aljuminijlitievogo splava V-1469 [The development of industrial production of semi-finished prospective aluminum-lithium alloy B-1469] //Aviacionnye materialy i tehnologii. 2011. №1. S. 8–12.
  6. Rjabov D.K., Kolobnev N.I., Samohvalov S.V., Mahsidov V.V. Vlijanie predvaritel'nogo estestvennogo starenija na svojstva splava 1913 v iskusstvenno sostarennom sostojanii [Effect of prior natural aging on the properties of the alloy 1913 in the artificially aged condition] //Aviacionnye materialy i tehnologii. 2013. №2. S. 8–11.
  7. Mahsidov V.V., Kolobnev N.I., Karimova S.A., Sbitneva S.V. Vzaimosvjaz' struktury i korrozionnoj stojkosti v splave 1370 sistemy Al–Mg–Si–Cu–Zn [Interconnection structure and corrosion resistance of the alloy system 1370 Al-Mg-Si-Cu-Zn] //Aviacionnye materialy i tehnologii. 2012. №1. S. 8–13.
  8. Matejko I.V., Shevchenko M.A., Kotova N.V., Sudavcova V.S. Termodinamicheskie svojstva splavov sistemy Al–Si [Thermodynamic properties of alloys of the Al-Si] //Zhurnal fizicheskoj himii. 2011. T. 85. №2. S. 212–218.
  9. Prohorov A.Ju., Belov N.A., Alabin A.N. Osobennosti tehnologii plavki i lit'ja slitkov provodnikovyh aljuminievo-cirkonievyh splavov v promyshlennyh uslovijah [Technology features melting and casting ingots conductor aluminum-zirconium alloys in an industrial environment] //Litejshhik Rossii. 2010. №4. S. 30–34.
  10. Brodova I.G., Chikova O.A., Vitjushin M.A. i dr. Osobennosti struktury diffuzionnyh sloev, obrazujushhihsja pri rastekanii rasplavov Al–Si po stali St3 [Features of the structure of the diffusion layers formed in the melt flow for Al-Si steel St3] //Fizika metallov i metallovedenie. 2010. T. 109. №6. S. 665–670.
  11. GOST 11739.7–99. Splavy aljuminievye litejnye i deformiruemye. Metody opredelenija kremnija [Aluminum casting alloys and wrought. Methods for determination of silicon].
  12. Pupyshev A.A., Danilova D.A. Ispol'zovanie atomno-jemissionnoj spektrometrii s induktivno-svjazannoj plazmoj dlja analiza materialov i produktov chernoj metallurgii [Using atomic emission spectrometry with inductively coupled plasma for analysis of materials and products of ferrous metallurgy] //Analitika i kontrol'. 2007. №2–3. T. 11. S. 131–181.
  13. Tormysheva E.A., Smirnova E.V., Ermolaeva T.N. Mikrovolnovaja probopodgotovka naplavochnyh materialov dlja analiza metodom atomno-jemissionnoj spektroskopii s induktivno-svjazannoj plazmoj [Microwave Sample Preparation surfacing materials for analysis by atomic emission spectroscopy with inductively coupled plasma] //Zavodskaja laboratorija. Diagnostika materialov. 2010. T. 76. №10. S. 10–13.
  14. Lidin R.A., Molochko V.A., Andreeva L.L. Himicheskie svojstva neorganicheskih veshhestv [The chemical properties of inorganic substances]. M.: Himija. 2000. 480 s.