Development trends in the field of fuel resistant paintwork coatings for protection of integral fuel tanks of aircrafts (review)
UDC
629.7.023.222
DOI
10.18577/2307-6046-2014-0-11-8-8
Article PDF (Russian)
(404.58 KB)
How to cite
Kuznetsova V.A., Kuznecov G.V. Development trends in the field of fuel resistant paintwork coatings for protection of integral fuel tanks of aircrafts (review) // Proceedings of VIAM. 2014. No. 11. DOI: 10.18577/2307-6046-2014-0-11-8-8. URL: https://www.viam-works.ru/en/journal/2014/11/8
Abstract
Development trends in the field of fuel resistant coatings which carry out a function of corrosion protection of inner surface of integral fuel tanks made from aluminum alloys, and also polymeric composite materials were considered. Analysis of scientific and technical documentation and security documents of world leading countries on the problem of development of fuel resistant coatings was carried out.
Reference list
- Kablov E.N. Strategicheskie napravlenija razvitija materialov i tehnologij ih pererabotki na period do 2030 goda [Strategic directions of development of materials and technologies to process them for the period up to 2030] //Aviacionnye materialy i tehnologii. 2012. №S. S. 7–17.
- Chebotarevskij V.V., Kondrashov Je.K. Tehnologija lakokrasochnyh pokrytij v mashinostroenii [Coatings technology in mechanical engineering]. M. Mashinostroenie. 1978. 295 s.
- Gol'dberg M.M., A.V. Korjukin, Je.K. Kondrashov. Pokrytija dlja polimernyh materialov [Coatings for polymeric materials]. M. Himija. 1980. 287 s.
- Jakovlev A.D. Himija i tehnologija lakokrasochnyh pokrytij [Chemistry and technology of coatings]. L. Himija. 1981. 252 s.
- Kondrashov Je.K., Kuznecova V.A., Semenova L.V., Lebedeva T.A., Malova N.E. Razvitie aviacionnyh lakokrasochnyh materialov [Development of aircraft paints and varnishes] //Vse materialy. Jenciklopedicheskij spravochnik. 2012. №5. S. 49–54.
- Semenova L.V., Malova N.E., Kuznecova V.A., Pozhoga A.A. Lakokrasochnye materialy i pokrytija [Coating materials and coating] //Aviacionnye materialy i tehnologii. 2012. №S. S. 315–327.
- 7 Kablov E.N. Sovremennye materialy – osnova innovacionnoj modernizacii Rossii [Modern materials – the basis of innovative modernization of Russia] //Metally Evrazii. 2012. №3. S. 10–15.
- Kablov E.N., Kondrashov S.V., Jurkov G.Ju. Perspektivy ispol'zovanija uglerodsoderzhashhih nanochastic v svjazujushhih dlja polimernyh kompozicionnyh materialov [Prospects for the use of carbonaceous nanoparticles in polymeric binders for composite materials] //Rossijskie nanotehnologii. 2013. T. 8. №3–4. S. 28–46.
- Chursova L.V., Kim M.A., Panina N.N., Shvecov E.P. Nanomodificirovannoe jepoksidnoe svjazujushhee dlja stroitel'noj industrii [Aircraft Materials and Technologies] //Aviacionnye materialy i tehnologii. 2013. №1. S. 40–47.
- Chertkov Ja.V., Spirkin V.G. Primenenie reaktivnyh topliv v aviacii [Application of jet fuels in aviation]. M.: Transport. 1974. 160 s.
- Rozenfel'd I.L., Rubinshtejn F.I. Antikorrozionnye gruntovki i ingibirovannye lakokrasochnye pokrytija [Anti-rust primer and inhibited coatings]. M.: Himija.
- 196 s.
- Vorob'ev G.Ja. Himicheskaja stojkost' polimernyh materialov [Chemical resistance of polymeric materials]. M.: Himija. 1981. 296 s.
- Zuev Ju.S. Razrushenie polimera pod dejstviem agressivnyh sred [Degradation of the polymer under the influence of aggressive media]. 2-e izd. M.: Himija. 1972. 232 s.
- Moiseev Ju.V., Zajkov G.E. Himicheskaja stojkost' polimerov v agressivnyh sredah [Chemical resistance of polymers in aggressive environments]. M.: Himija. 1979. 288 s.
- Sosnina S.A., Kuleshova I.D. Regulirovanie vzaimodejstvija komponentov v napolnennyh lakokrasochnyh kompozicijah [Regulation of interaction of the components in the paint-filled compositions] //Lakokrasochnye materialy i ih primenenie. 2011. №1.
- S. 60–62.
- Kuznecova V.A., Deev I.S., Kondrashov Je.K., Kuznecov G.V. Vlijanie otverditelej na mikrostrukturu i svojstva modificirovannogo jepoksidnogo svjazujushhego dlja toplivostojkogo pokrytija [Effect of curing agents for the microstructure and properties of the modified epoxy coating binder fuel resistant cover] //Vse materialy. Jenciklopedicheskij spravochnik. 2012. №11. S. 38–41.
- Kuznecova V.A., Kondrashov Je.K., Semenova L.V., Kuznecov G.V. O vlijanii formy chastic oksida cinka na jekspluatacionnye svojstva polimernyh pokrytij [On the influence of the form of zinc oxide particles on the performance of the polymer coatings] //Materialovedenie. 2012. №12. S. 12–14.
- Kondrashov Je.K., Kuznecova V.A., Semenova L.V., Lebedeva T.A. Osnovnye napravlenija povyshenija jekspluatacionnyh svojstv, tehnologicheskih i jekologicheskih harakteristik lakokrasochnyh pokrytij dlja aviacionnoj tehniki [The main directions of improving the performance properties, technological and environmental performance coatings for aircraft equipment] //Rossijskij himicheskij zhurnal. 2010. T. LIV. №1.
- S. 96–102.
- Semenova L.V., Rodina N.D., Nefedov N.I. Vlijanie sherohovatosti sistem lakokrasochnyh pokrytij na jekspluatacionnye svojstva samoletov [The effect of roughness of coatings systems for performance of the aircraft] //Aviacionnye materialy i tehnologii. 2013. №2. S. 37–40.
- Kalendova A., Kalendova P. Issledovanie antikorrozionnyh pigmentov na osnove modificirovannyh fosfatov [Investigation of anticorrosive pigments based on modified phosphate] //Lakokrasochnye materialy i ih primenenie. 2004. №4. S. 11–14.
- Guseva R.I. Ispol'zovanie lakokrasochnyh sistem pri pokraske detalej iz polimernyh kompozicionnyh materialov [The use of paint systems for painting parts of polymeric composite materials] //Uchenye zapiski. 2010. №111-1 (3). S. 101–107.
- Fabuljak F.G. Molekuljarnaja podvizhnost' polimerov v poverhnostnyh slojah [The molecular mobility in the polymer surface layers]. Kiev: Naukova dumka. 1983. 144 s.
- Kuznecova V.A., Deev I.A., Kuznecov G.V., Kondrashov Je.K. Vlijanie napolnitelja na ustalostnuju prochnost' i mikrostrukturu svobodnyh polimernyh plenok pri cikli-cheskom rastjazhenii [Effect of filler on the fatigue strength and microstructure of the polymer films available under cyclic tension] //Zavodskaja laboratorija. 2014. T. 80. №5. S. 35–39.
- Kondrashov Je.K., Kozlova A.A., Malova N.E. Issledovanie kinetiki otverzhdenija ftorpoliuretanovyh jemalej alifaticheskimi poliizocianatami razlichnyh tipov [Study of curing kinetics ftorpoliuretanovyh enamels aliphatic polyisocyanates different types] //Aviacionnye materialy i tehnologii. 2013. №1. S. 48–49.
- Muhametov R.R., Ahmadieva K.R., Chursova L.V., Kogan D.I. Novye polimernye svjazujushhie dlja perspektivnyh metodov izgotovlenija konstrukcionnyh voloknistyh PKM [New polymeric binders for the promising methods for the manufacture of structural fibrous PCM] //Aviacionnye materialy i tehnologii. 2011. №2. S. 38–42.
- Langer E., Kuczynska H., Kaminska-Tarnawska E., Lukashuk J. Self-stratifying coatings containing barrier and active anticorrosive pigments //Progress in Organic Coatings. 2011. V. 71. №2. P. 162–166.
- Fang Wang, Junjun Liu, Yuefei Li, Ruibin Fan, Yanni Li. Complex Barrier Layer of Triazinedithoil Prepared by Electrodeposition and Initiated Polymerization on aluminum Alloy towards Corrosion Protection //Internatioal Journal of Elektrochemiсal Science. 2012. №7. P. 3672–3680.
- Zheludkevich M.L., Tedim J., Ferreira M.G.S. «Smart» coating for active corrosion protection based on multifunctional micro and nanocontainers //Electrochimica Acta. 2012. V. 82. P. 314–323.
- Carneiro J., Tedim J., Fernandes S.C.M., Freire S.C.R., Silvestre A.J.D., Gandini A., Ferreira M.G.S., Zheludkevich M.L. Chitosan-based self-healing protective coatings doped with cerium nitrate for corrosion protection of aluminum alloy 2024 //Progress in Organic Coatings. 2012. V. 75. №1–2. P. 8–13.
- Chromate free waterborne epoxy corrosion resistant primer: pat. 50773312 US;
- pabl. 2002.
- Method of forming a multi-layer coating on automobile bodies without a primer bake: pat. 2007190312 US; pabl. 2007.