Oil-gasoline-proof sealant with special properties on the base of polysulphide oligomer

Smirnov D.N., Zaytseva E.I., Еliseev O.A.
Smirnov D.N., Zaytseva E.I., Еliseev O.A. Oil-gasoline-proof sealant with special properties on the base of polysulphide oligomer // Proceedings of VIAM. 2014. No. 11. DOI: 10.18577/2307-6046-2014-0-11-7-7. URL: https://www.viam-works.ru/en/journal/2014/11/7
Abstract

Influence of different fillers and modifying additives on physical-mechanical, pro-cessing and adhesive properties was investigated. It was shown that an introduction of modifying additives of different chemical nature leads to changing of properties, in par-ticular swelling in water of oil-gazoline-proof sealant on a base of polysulphide oligomer.

Reference list
  1. Kablov E.N. Strategicheskie napravlenija razvitija materialov i tehnologij ih pererabotki na period do 2030 goda [Strategic directions of development of materials and technologies for their reprocessing for the period up to 2030] //Aviacionnye materialy i tehnologii. 2012. №S. S. 7–17.
  2. Germetizirujushhaja kompozicija [A sealant composition]: pat. 2436818 Ros. Federacija; opubl. 01.07.2010.
  3. Eliseev O.A., Krasnov L.L., Zajceva E.I., Savenkova A.V. Razrabotka i modificirovanie jelastomernyh materialov dlja primenenija vo vseklimaticheskih uslovijah [Development and modification of elastomeric materials for use in all-climatic conditions] //Aviacionnye materialy i tehnologii. 2012. №S. S. 309–314.
  4. Minkin V.S., Hakimullin Ju.N., Deberdeev T.R., Berlin Al. Al. Vlijanie ionov Fe (III) v sostave MnO2 na kinetiku vulkanizacii zhidkih tiokolov [Effect of ions Fe (III) in the composition MnO2 vulcanization kinetics liquid thiokols] //Klei. Germetiki. Tehnologii. 2009. №4. S. 28–30.
  5. Zajceva E.I., Chursova L.V. Issledovanie mikrobiologicheskoj stojkosti polisul'fidnogo germetika s novymi antisepticheskimi dobavkami [Study of microbiological resistance polysulfide sealant with new antiseptic additives] //Klei. Germetiki. Tehnologii. 2012. №1. S. 16–20.
  6. Zajceva E.I., Donskoj A.A. Sealants Based on Polysulfide Elastomers //Polymer Science. Ser. S. 2008. V. 1. P. 15–25.
  7. Zajceva E.I., Donskoj A.A. Germetiki na osnove polisul'fidnyh jelastomerov [Sealants based on polysulfide elastomers] //Klei. Germetiki. Tehnologii. 2008. №6–7. S. 15–25.
  8. Zajceva E.I., Donskoj A.A. Novye polisul'fidnye germetiki dlja aviacionnoj promyshlennosti [New polysulfide sealants for the aviation industry] //Klei. Germetiki. Tehnologii. 2009. №3. S. 18–23.
  9. Zajceva E.I., Donskoj A.A. Novye polisul'fidnye germetiki dlja aviacionnoj pro-myshlennosti [New polysulfide sealants for the aviation industry] /V sb. Trudov «Har'kovskaja nanotehnologicheskaja associacija–2008». 2008. S. 191–200.
  10. Petrova A.P., Donskoj A.A. Klejashhie materialy, germetiki [Adhesives, Sealants]: Spravochnik. SPb.: NPO «Professional». 2008. S. 503–567.
  11. Edward M. Petrie Handbook of Adhesives and Sealants. New York. 2000. P. 14–23.
  12. Sidney H. Goodman Epoxy Resins. New York. 2002. Р. 19–28.
  13. Minkin V.S., Suhanov P.P., Averko-Antonovich L.A., Dzhanbekova L.R. Stroenie i vulkanizacija polisul'fidnyh oligomerov [Structure and curing polysulfide oligomers] //Kauchuk i rezina. 1994. №1. S. 14–19.
  14. Muhutdinov M.A., Hakimullin Ju.N., Gubajdulin L.Ju., Liakumovich A.G. Modificirovannye tiokolovye germetiki s uluchshennymi adgezionnymi svojstvami [Modified Thiokol sealants with improved adhesion properties] //Kauchuk i rezina. 1998. №3. S. 6–8.
  15. Nizkovjazkaja silikonovaja kompozicija [Low-viscosity silicone composition]: pat. 2356117 Ros. Federacija; opubl. 20.06.2007.
  16. Mendeleeva G.A., Porfil'eva R.T., Gerasimov V.V., Efimova V.A. Tehnologii i svojstva polisul'fidnogo materiala, modificirovannogo organometallofosfatnymi soedinenijami [Technology and material properties of the polysulfide, modified organometallic-phosphate compounds] //Vestnik kazanskogo tehnologicheskogo universiteta. 2009. №3. S. 18–22.
  17. Kurbangoleeva A.R., Petlina I.A., Hakimullin Ju.N. Vlijanie napolnitelej na svojstva tiokolovyh germetikov [Effect of fillers on the properties of Thiokol sealants] //Vestnik kazanskogo tehnologicheskogo universiteta. 2011. №18. S. 86–89.
  18. Kablov E.N. Aviakosmicheskoe materialovedenie [Aerospace Materials] //Vse materialy. Jenciklopedicheskij spravochnik. 2008. №3. S. 2–14.
  19. Sostav dlja zashhitnogo pokrytija [Ingredients for the protective coating]: pat. 2334158 Ros. Federacija; opubl. 19.12.2006.
  20. Savenkova A.V., Chursova L.V., Eliseev O.A., Shragin D.I., Kopylov V.Ja., Glazov P.A. Vosstanovlenie tehnologii izgotovlenija teplomorozostojkih germetikov na osnove kremnijorganicheskih kauchukov, sintezirovannyh po novym promyshlennym tehnologijam [Restoring production technology teplomorozostoykih sealants based on silicone rubber, synthesized by the new technologies industrial] //Aviacionnye materialy i tehnologii. 2012. №4. S. 25–31.
  21. Chursova L.V., Kim M.A., Panina N.N., Shvecov E.P. Nanomodificirovannoe jepoksidnoe svjazujushhee dlja stroitel'noj industrii [Nanomodified epoxy binder for the construction industry] //Aviacionnye materialy i tehnologii. 2013. №1. S. 40–47.
  22. Novakov I.A., Nistratov A.V., Frolova V.I. i dr. Issledovanie struktury i svojstv materialov na osnove kompozicij polisul'fidnyj oligomer–polimerizacionnosposobnoe soedinenie [Investigation of the structure and properties of materials based on compositions polysulfide oligomer-polymerizable compound] //Plasticheskie massy. 2011. №1. S. 3–8.
  23. Novakov I.A., Nistratov A.V., Frolova V.I. i dr. Osobennosti poluchenija materialov na osnove kompozicij polisul'fidnyj oligomer–polimerizacionnosposobnoe soedinenie, otverzhdaemyh v prisutstvii oksida marganca [Peculiarities of materials based on the compositions of the polysulfide oligomer-polymerizable compound is cured in the presence of manganese oxide] //Klei. Germetiki. Tehnologii. 2011. №10. S. 6–12.
  24. Zajceva E.I., Chursova L.V., Smirnov D.N. Perspektivy snizhenija plotnosti polisul'fidnyh germetikov [Prospects for reducing the density of polysulfide sealants] //Klei. Germetiki. Tehnologii. 2012. №5. S. 10–14.
  25. Karimova S.A., Pavlovskaja T.G. Razrabotka sposobov zashhity ot korrozii konstrukcij, rabotajushhih v uslovijah kosmosa [Development of methods of corrosion protection structures operating in the space environment] //Trudy VIAM. 2013. №4. St. 02 (viam-works.ru).