Abstract

The most important problems at casting of magnesium alloys were considered: сrea-tion of new compositions and technology of antiburning-on additive materials (AAM) production with improved properties and study of the mechanism of protection of mag-nesium alloys from oxidation in the process of casting into sand-clay mixtures (SCM)

Reference list
  1. Kornysheva I.S., Volkova E.F., Goncharenko E.S., Muhina I.Ju. Perspektivy magnievyh i litejnyh aljuminievyh splavov [Prospects of magnesium and cast aluminum alloys] //Aviacionnye materialy i tehnologii. 2012. №S. S. 212–222.
  2. Karimova S.A., Pavlovskaja T.G. Razrabotka sposobov zashhity ot korrozii konstrukcij, rabotajushhih v uslovijah kosmosa [Development of methods of corrosion protection structures operating in the space environment] //Trudy VIAM. 2013. №4. St. 02 (viam-works.ru).
  3. Goncharenko E.S., Trapeznikov A.V., Ogorodov D.V. Litejnye aljuminievye splavy (k 100-letiju so dnja rozhdenija M.B. Al'tmana) [Casting aluminum alloys (on the 100-th anniversary of M.B. Altman)] //Trudy VIAM. 2014. №4. St. 02 (viam-works.ru).
  4. Dujunova V.A. Metody zashhity magnievyh splavov v otechestvennom litejnom proizvodstve s 1930-h gg. do nastojashhego vremeni [Methods of protection of magnesium alloys in the domestic foundry industry since the 1930's. far] //Litejshhik Rossii. 2010. №10. S. 35–37.
  5. Dujunova V.A. Magnievye splavy: nauchnye issledovanija Central'nogo ajerogidrodinamicheskogo instituta i Vsesojuznogo instituta aviacionnyh materialov. 1930–1935 gg. [Magnesium alloys: research Central hydrodynamic Institute and All-Union Institute of Aviation Materials. 1930–1935] //Istorija nauki i tehniki. 2012. №10. S. 27–35.
  6. Kablov E.N. Osnovnye itogi i napravlenija razvitija materialov dlja perspektivnoj aviacionnoj tehniki [Main Results and directions of development of promising materials for aeronautical engineering] /V sb. 75 let. Aviacionnye materialy. Izbrannye trudy «VIAM» 1932–2007: Jubilejnyj nauch.-tehnich. sb. M.: VIAM. 2007. S. 20–26.
  7. Kablov E.N. Strategicheskie napravlenija razvitija materialov i tehnologij ih perera-botki na period do 2030 goda [Strategic directions of development of materials and technologies to process them for the period up to 2030] //Aviacionnye materialy i tehnologii. 2012. №S. S. 7–17.
  8. Kablov E.N., Ospennikova O.G., Vershkov A.V. Redkie metally i redkozemel'nye jelementy – materialy sovremennyh i budushhih vysokih tehnologij [Rare metals and rare-earth elements – materials for current and future high-tech] //Trudy VIAM. 2013. №2. St. 01 (viam-works.ru).
  9. Kablov E.N. VIAM: prodolzhenie puti [VIAM: continuation of the path] //Nauka v Rossii. 2012. №3. S. 36–44.
  10. Kablov E.N. Sovremennye materialy – osnova innovacionnoj modernizacii Rossii [Modern materials - the basis of innovative modernization of Russia] //Metally Evrazii. 2012. №3. S. 10–15.
  11. Kablov E.N. Himija v aviacionnom materialovedenii [Chemicals in aviation materials] //Rossijskij himicheskij zhurnal. 2010. T. LIV. №1. S. 3–4.
  12. Kozlov I.A., Karimova S.A. Korrozija magnievyh splavov i sovremennye metody ih zashhity [Corrosion of magnesium alloys, and modern methods of protection] //Aviacionnye materialy i tehnologii. 2014. №2. S. 15–20.
  13. Korchagina V.A. Radi kachestva magnievyh otlivok [For the sake of the quality of magnesium castings] //Inzhenernaja gazeta. 2006. №33–34. S. 5.
  14. Kablov E.N., Muhina I.Ju., Korchagina V.A. Prisadochnye materialy dlja formovochnyh smesej pri lit'e magnievyh splavov [Filler materials for molding compounds during casting of magnesium alloys] //Litejnoe proizvodstvo. 2007. №5. S. 15–18.
  15. Dujunova V.A., Muhina I.Ju., Uridija Z.P. Novye protivoprigarnye prisadochnye materialy dlja litejnyh form magnievyh otlivok [New antipenetration filler materials for molds magnesium castings] //Litejnoe proizvodstvo. 2009. №9. S. 18–21.
  16. Antjufeeva N.V., Aleksashin V.M., Zhelezina G.F., Stoljankov Ju.V. Metodicheskie podhody termoanaliticheskih issledovanij dlja ocenki svojstv prepregov i ugleplastikov [Methodological approaches thermoanalytical studies to evaluate the properties of the prepreg and carbon fiber reinforced plastics] //Vse materialy. Jenciklopedicheskij spravochnik. 2012. №4. S. 18–27.
  17. Muhina I.Ju., Dujunova V.A., Uridija Z.P. Perspektivnye litejnye magnievye splavy [Prospective casting magnesium alloys] //Litejnoe proizvodstvo. 2013. №5. S. 2–5.
  18. Dujunova V.A., Goncharenko N.S., Muhina I.Ju., Uridija Z.P., Volkova E.F. Nauchnoe nasledie akademika I.N. Fridljandera. Sovremennye issledovanija magnievyh i litejnyh aljuminievyh splavov v VIAM [Scientific Heritage of Academician I.N. Friedlander. Modern studies of magnesium and cast aluminum alloys in VIAM] //Cvetnye metally. 2013. №9. S. 71–78.
  19. Frolov A.V., Muhina I.Ju., Dujunova V.A., Uridija Z.P. Vlijanie tehnologicheskih
  20. parametrov plavki na strukturu i svojstva novyh magnievyh splavov [Effect of process parameters on the structure and melting properties of the novel magnesium alloys] //Metallurgija mashinostroenija. 2014. №2. S. 26–29.
  21. Dujunova V.A., Uridija Z.P. Issledovanie vosplamenjaemosti litejnyh magnievyh splavov sistemy Mg–Zn–Zr [Investigation of the flammability of the casting of magnesium alloys Mg–Zn–Zr] //Litejshhik Rossii. 2012. №11. S. 21–23.
  22. Dujunova V.A., Kozlov I.A. Holodnotverdejushhie formovochnye smesi: perspektivy ispol'zovanija pri lit'e magnievyh splavov [Cold-molding materials: prospects for the use in the casting of magnesium alloys] //Vse materialy. Jenciklopedicheskij spravochnik. 2011. №1. S. 41–43.
  23. Antipov V.V., Vahromov R.O., Dujunova V.A., Nochovnaja N.A. Materialy s vysokoj udel'noj prochnost'ju na osnove aljuminija, magnija, titana i tehnologii ih pererabotki [Materials with a high specific strength of the aluminum, magnesium, titanium, and processing technologies] //Boepripasy i spechimija. 2013. №3. S. 51–55.
  24. Kablov E.N. Aviakosmicheskoe materialovedenie [Aerospace Materials] //Vse materialy. Jenciklopedicheskij spravochnik. 2008. №3. S. 2–14.