Low-cost alloyed titanium alloys for metal-polymer laminates

Nochovnaya N.A., Panin P.V., Alexeev E.B., Bokov K.A.
Nochovnaya N.A., Panin P.V., Alexeev E.B., Bokov K.A. Low-cost alloyed titanium alloys for metal-polymer laminates // Proceedings of VIAM. 2014. No. 11. DOI: 10.18577/2307-6046-2014-0-11-2-2. URL: https://www.viam-works.ru/en/journal/2014/11/2
Abstract

Two pilot low-cost alloyed near-α-(Ti–Fe–Zr–O–N) and α+β (Ti–Al–V–Fe)-alloys have been developed specially for titanium-polymer laminates, which allow a 20 percent weight reduction in comparison to that of bulk aluminum-based alloys constructions. The new alloys are doped with REM and possess increased mechanical and service properties.

Reference list
  1. Kablov E.N. Strategicheskie napravlenija razvitija materialov i tehnologij ih pererabotki na period do 2030 goda [Strategic directions of development of materials and technologies to process them for the period up to 2030] //Aviacionnye materialy i tehnologii. 2012. №S. S. 7–17.
  2. Tarasov Ju.M., Antipov V.V. Novye materialy VIAM – dlja perspektivnoj aviacionnoj tehniki proizvodstva OAO «OAK» [New materials VIAM - for promising aviation equipment produced by JSC «UAC»] //Aviacionnye materialy i tehnologii. 2012. №2. S. 5–6.
  3. Kablov E.N., Antipov V.V., Senatorova O.G. Sloistye aljumostekloplastiki SIAL-1441 i sotrudnichestvo s Airbus i TU DELFT [Layered aluminum-fiberglass Sial-1441 and cooperation with Airbus and TU DELFT] //Cvetnye metally. 2013. №9(849). S. 50–53.
  4. Antipov V.V., Senatorova O.G., Lukina N.F. i dr. Sloistye metallopolimernye kompozicionnye materialy [Layered metal-composite materials] //Aviacionnye materialy i tehnologii. 2012. №S. S. 226–230.
  5. Lukina N.F., Dement'eva L.A., Anihovskaja L.I. Kleevye prepregi dlja sloistyh alju-mostekloplastikov klassa SIAL [Adhesive prepregs layered aluminum-fiberglass class SIAL] //Trudy VIAM. 2014. №1. St. 05 (viam-works.ru).
  6. Krasnov E.I., Shtejnberg A.S., Shavnev A.A., Berezovskij V.V. Issledovanie sloistogo metal-licheskogo kompozicionnogo materiala sistemy Ti–TiAl3 [Study layered metal composite material of Ti–TiAl3] //Aviacionnye materialy i tehnologii. 2013. №3. S. 16–19.
  7. Boyer R.R., Williams J.C. Developments in research and applications in the titanium industry in the USA //Proc. of 12th World Conf. on Titanium. 2011. V. I. P. 10–19.
  8. Il'in A.A., Kolachev B.A., Pol'kin I.S. Titanovye splavy. Sostav, struktura, svojstva [Titanium alloys. The composition, structure and properties]: Spravochnik. M.: VILS–MATI. 2009. 520 s.
  9. Horev A.I., Belov S.P., Glazunov S.G. Metallovedenie titana i ego splavov [Physical metallurgy of titanium and its alloys]. M.: Metallurgija. 1992. 352 s.
  10. Niinomi M. Recent trends in titanium research and development in Japan //Proc. 12th World Conf. on Titanium. 2011. V. I. P. 30–37.
  11. Kablov E.N., Ospennikova O.G., Vershkov A.V. Redkie metally i redkozemel'nye jelementy – materialy sovremennyh i budushhih vysokih tehnologij [Rare metals and rare-earth elements - materials for current and future high-tech] //Trudy VIAM. 2013. №2. St. 01 (viam-works.ru).
  12. Splav na osnove titana i izdelie, vypolnennoe iz nego [Titanium-base alloy and article made therefrom]: pat. 2222627 Ros. Federacija; opubl. 27.01.2004.
  13. Titanium-aluminum-vanadium alloys and products made therefrom: pat. 5980655 US; publ. 09.11.1999.
  14. Splav na osnove titana i sposob termicheskoj obrabotki krupnogabaritnyh polufabrikatov iz jetogo splava [Titanium-base alloy and method for thermal processing of large-polufab-finished products of the alloy]: pat. 2169204 Ros. Federacija; opubl. 20.06.2001.
  15. Splav na osnove titana [Titanium-base alloy]: pat. 2169782 Ros. Federacija; opubl. 06.05.2006.
  16. Titanium-based alloy: pat. EP 1882752; publ. 03.06.2009.
  17. Titanium-based alloy: pat. US 6632396; publ. 14.10.2003.
  18. High strength Ti alloy and its production method: pat. JP 2004010963; publ. 15.02.2004.
  19. Yashiki T. Development of a high temperature oxidation-resistant titanium alloy for exhaust systems of motorcycles and automobiles //Proc. 11th World Conf. on Titanium. 2007. V. II. P. 1387–1390.
  20. Otsuka H. et al. Formability of newly developed high-performance titanium alloys for automotive exhaust systems //Proc. 11th World Conf. on Titanium. 2007. V. I. P. 251–254.
  21. Titanium alloy part and method of manufacturing same: pat. EP 2508643; publ. 10.10.2012.
  22. Titanium alloy with improved properties: app. US 2012/0107132; publ. 03.05.2012.
  23. Conrad H. Effect of interstitial solutes on the strength and ductility of titanium //Progress in Mat. Sci. 1981. V. 26(2–4). P. 123–403.
  24. Zhu J. et al. Influence of boron addition on microstructure and mechanical properties of dental cast titanium alloys //Mat. Sci. & Eng.: A. 2003. V. 339(1–2). P. 53–62.
  25. Ando T. et al. Precipitation of fine beta-phase in high nitrogen titanium alloy //Proc. 11th World Conf. on Titanium. 2007. V. I. P. 447–450.
  26. Koike M. et al. Evaluation of cast Ti–Fe–O–N alloys for dental applications //Mat. Sci. & Eng.: C. 2005. V. 25(3). P. 349–356.