Study of influence of different protective coatings on characteristics of fire safety of fuselage thermal acoustic insulation

Kirienko O.A., Shurkova E.N., Volnyj O.S., Barbotko S.L.
Kirienko O.A., Shurkova E.N., Volnyj O.S., Barbotko S.L. Study of influence of different protective coatings on characteristics of fire safety of fuselage thermal acoustic insulation // Proceedings of VIAM. 2014. No. 10. DOI: 10.18577/2307-6046-2014-0-10-7-7. URL: https://www.viam-works.ru/en/journal/2014/10/7
Keywords
thermal acoustic insulation, fire safety
Abstract

Samples of perspective material of thermal acoustic isolation were manufactured. The sound heat-insulating material contained the following layers:heat - sound - insulating layer on a base of basalt and silica fibers; a layer of non-woven material, based on aramid fibers; protective coating on a base of fiberglass or heat-resistant polymer film (polyimide film PMA, fluoropolymer film F-4MD, material STF-26, material on a base of fiberglass with fluoroplast F-42 impregnation, polyethersulfone film). Investigation on characterization of fire safety (duration of residual independent burning, length of burn-through) of thermal acoustic insulation material of fuselage with different protective coatings according to the requirements of aviation regulations AP-25, p. 25.856(a) Appendix F, Part VI. Tests were performed in a chamber with a heat radiation panel under an influence on the material both a heat radiation flow of variable intensity and a burner flame. Both separate specimens of pro

Reference list
  1. Dzhafarov M.A., Lozovoj N.F., Lucenko V.I., Fedorov V.K. Obespechenie pozharnoj bezopasnosti na ajerodromah grazhdanskoj aviacii [Fire safety on the ground of Civil Aviation]. M.: Transport. 1987. 3 s.
  2. Terebnjov V.V., Artem'ev N.S., Grachev V.A. Transport: nazemnyj, morskoj, rechnoj, vozdushnyj, metro. Protivopozharnaja zashhita i tushenie pozharov [Transportation: land, sea, river, air, underground. Fire protection and fire fighting]. Kn. 6. M.: Pozhnauka. 2007. 211 s.
  3. Barbot'ko S.L., Shurkova E.N. O pozharnoj bezopasnosti materialov, ispol'zuemyh dlja izgotovlenija vneshnego kontura samoletov [On the fire safety of the materials used for the manufacture of the outer contour of aircraft] //Pozharovzryvobezopasnost'. 2011. T. 20. №10. S. 19–24.
  4. Barbot'ko S.L., Nagaev A.S. K voprosu ob obespechenii pozharnoj bezopasnosti vneshnego kontura samoletov [On the issue of fire safety outer contour aircraft] /V sb. dokl. VIII nauch. konf. po gidroaviacii «Gidroaviasalon–2010». Ch. II. M.: CAGI. 2010. S. 107–110.
  5. Barbot'ko S.L., Shurkova E.N., Vol'nyj O.S., Skryljov N.S. Ocenka pozharnoj bezopasnosti polimernyh kompozicionnyh materialov dlja vneshnego kontura aviacionnoj tehniki [Assessment of fire safety of polymeric composite materials for the outer loop of aeronautical engineering] //Aviacionnye materialy i tehnologii. 2013. №1. S. 56–59.
  6. Barbot'ko S.L. Pozharobezopasnost' aviacionnyh materialov [Flammability of aircraft materials] //Aviacionnye materialy i tehnologii. 2012. №S. S. 431–439.
  7. Barbot'ko S.L., Kirillov V.N., Shurkova E.N. Ocenka pozharnoj bezopasnosti polimernyh kompozicionnyh materialov aviacionnogo naznachenija [Assessment of fire safety of polymeric composite materials for aircraft industry] //Aviacionnye materialy i tehnologii. 2012. №3. S. 56–63.
  8. Sytyj Ju.V., Sagomonova V.A., Kisljakova V.I., Bol'shakov V.A. Vibropogloshhajushhie materialy na osnove termojelastoplastov [Vibration-absorbing materials based on thermoplastic elastomers] //Trudy VIAM. 2013. №3. St. 06 (viam-works.ru).
  9. Nesterova T.A., Barbot'ko S.L., Nikolaeva M.F., Gerter Ju.A. Mnogoslojnyj zashhitno-dekorativnyj material dlja dekorirovanija detalej v salonah samoletov i vertoletov [Multi-layer protective decorative material for decorating details in the cabin of aircraft and helicopters] //Trudy VIAM. 2013. №8. St. 4 (viam-works.ru).
  10. Obzor rynka teploizoljacionnyh materialov na osnove bazal'tovogo volokna v Rossii [Market Overview of thermal insulating materials, based on basalt fiber in Russia / Report LLC «InfoMine»] /Otchet OOO «Infomajn» (demo-versija). 2007. 145 s.
  11. Ohlopkova A.A., Vasil'ev S.V., Gogoleva O.V. Razrabotka polimernyh kompozitov na osnove politetraftorjetilena i bazal'tovogo volokna [Development of polymer composites based on polytetrafluoroethylene and basalt fiber] //Neftegazovoe delo. 2011. №6. S. 404–411 (jelektronnyj nauchnyj zhurnal).
  12. Kablov E.N. Aviakosmicheskoe materialovedenie [Aerospace materials] //Vse materialy. Jenciklopedicheskij spravochnik. 2008. №3. S. 2–14.
  13. Istorija aviacionnogo materialovedenija. VIAM – 80 let: gody i ljudi [Strategic directions of development of materials and technologies to process them] /Pod obshh. red. E.N. Kablova. M.: VIAM. 2012. S. 505–509.
  14. Kablov E.N. Strategicheskie napravlenija razvitija materialov i tehnologij ih pererabotki na period do 2030 goda [Strategic directions of development of materials and technologies to process them for the period up to 2030] //Aviacionnye materialy i tehnologii. 2012. №S. S. 7–17.
  15. Kablov E.N. Himija v aviacionnom materialovedenii [Chemicals in aviation materials] //Rossijskij himicheskij zhurnal. 2010. T. LIV. №1. S. 3–4.
  16. Kablov E.N. Materialy i himicheskie tehnologii dlja aviacionnoj tehniki [Materials and chemical technologies for aircraft equipment] //Vestnik Rossijskoj akademii nauk. 2012. T. 82. №6. S. 520–530.
  17. Gavril'eva A.A., Vinokurov G.G., Kychkin A.K., Oreshko S.M. Tehnologicheskie harakteristiki formovanija bazal'tovyh nepreryvnyh volokon pri fil'ernom sposobe ih poluchenija [Technological characteristics of the molding of basalt continuous fibers spun at their reception] //Izvestija Samarskogo NC RAN. 2013. T. 15. №4(2). S. 448–450.
  18. Hodakova N.N., Uglova T.K., Firsov V.V., Tatarinceva O.S. Mineral'noe syr'e Kavkaza dlja proizvodstva bazal'tovyh volokon [Minerals of the Caucasus for the production of basalt fibers] //Polzunovskij vestnik. Prikladnaja himija i smezhnye oblasti. 2013. №1. S. 138–142.
  19. Issledovanie rynka armirujushhih izdelij i materialov iz nepreryvnogo bazal'tovogo volokna v Rossii [Market research reinforcing materials and products of continuous basalt fiber in Russia] /Otchet agentstva «Megaresearch» (demo-versija). 2011. 142 s.
  20. Stepanova E.V. Struktura i svojstva bazal'toplastikov, armirovannyh bazal'tovymi nitjami raznyh proizvoditelej, i modifikacija ih fizicheskimi i himicheskimi metodami [Structure and properties of basalt fiber reinforced basalt yarns of different manufacturers, and the modification of their physical and chemical methods]: Avtoref. dis. k.t.n. Saratov. 2006. 20 s.
  21. Tatarinceva O.S. Izoljacionnye materialy iz bazal'tovyh volokon, poluchennyh indukcionnym sposobom [Insulating materials made of basalt fibers obtained inductively]: Avtoref. dis. d.t.n. Bijsk. 2006. 42 s.
  22. Aviacionnye pravila. Gl. 25. Normy letnoj godnosti samoletov transportnoj kategorii [Aviation Regulations. Chap. 25 Standards of Airworthiness transport category airplanes]. 3-e izd. OAO Aviaizdat. 2009. 274 s.
  23. Efimov V.A., Shvedkova A.K., Koren'kova T.G., Kirillov V.N. Issledovanie polimernyh konstrukcionnyh materialov pri vozdejstvii klimaticheskih faktorov i nagruzok v laboratornyh i naturnyh uslovijah [Investigation of polymeric structural materials under the influence of climatic factors and stress in laboratory and field conditions] //Trudy VIAM. 2013. №1. St. 05 (viam-works.ru).
  24. Skryljov N.S., Vol'nyj O.S., Postnov V.I., Barbot'ko S.L. Issledovanie vlijanija teplovyh faktorov klimata na izmenenie harakteristik pozharobezopasnosti polimernyh kompozicionnyh materialov [Investigation of the influence of thermal factors of climate change on fire characteristics of polymer composite materials] //Trudy VIAM. 2013. №9. St. 05 (viam-works.ru).