On the question of carbon fiber reinforced plastics (CFRP) test specimen flaws

Stolyankov Yu.V., Iskhodzhanova I.V., Antyufeeva N.V.
Stolyankov Yu.V., Iskhodzhanova I.V., Antyufeeva N.V. On the question of carbon fiber reinforced plastics (CFRP) test specimen flaws // Proceedings of VIAM. 2014. No. 10. DOI: 10.18577/2307-6046-2014-0-10-10-10. URL: https://www.viam-works.ru/en/journal/2014/10/10
Abstract

For strength characteristics and properties evaluation test of composite polymer ma-terials (PCM), i.e. CFRP on the basis of glue epoxy resin and carbon fillers, it is neces-sary to make test specimen first. As a rule test specimen make from CFRP plates pro-duced by means of some molding technique. Cutting tool machining is the most wide-spread method among various existing methods of test specimen production. When studying the cutting technology influence on specimen surface quality some flaws have been reviled in the form of cleavage in addition to cracks and other flaws, which are re-sponsible for test specimen surface quality, and, therefore, the CFRP characteristics. Test specimen flaws have been described with their quantitative estimation. Flaws quantitative estimation technique has been worked out by means of computerized quantitative optical metallographic analysis method.

Reference list
  1. Kablov E.N. Strategicheskie napravlenija razvitija materialov i tehnologij ih pererabotki na period do 2030 goda [Strategic directions of development of materials and technologies to process them for the period up to 2030] //Aviacionnye materialy i tehnologii. 2012. №S. S. 7–17.
  2. Kablov E.N. Materialy i himicheskie tehnologii dlja aviacionnoj tehniki [Materials and chemical technologies for aircraft equipment] //Vestnik Rossijskoj akademii nauk. 2012. T. 82. №6. S. 520–530.
  3. Kablov E.N. Aviacionnoe materialovedenie: itogi i perspektivy [Aeronautical materials: results and prospects] //Vestnik Rossijskoj akademii nauk. 2002. T. 72. №1. S. 3–12.
  4. Perepjolkin K.E. Armirujushhie volokna i voloknistye polimernye kompozity [Reinforcing fibers or fibrous polymer composites]. SPb: Nauchnye osnovy i tehnologii. 2009.
  5. S. 171–185.
  6. Dushin M.I., Hrul'kov A.V., Muhametov R.R., Chursova L.V. Osobennosti izgotovlenija izdelij iz PKM metodom propitki pod davleniem [Features the manufacture of PCM by pressure impregnation] //Aviacionnye materialy i tehnologii. 2012. №1. S. 18–26.
  7. Hrul'kov A.V., Dushin M.I., Popov Ju.O., Kogan D.I. Issledovanija i razrabotka avtoklavnyh i bezavtoklavnyh tehnologij formovanija PKM [Research and development and autoclave molding technology bezavtoklavnogo PCM] //Aviacionnye materialy i tehnologii. 2012. №S. S. 292–301.
  8. Grigor'ev M.M., Kogan D.I., Tverdaja O.N., Panina N.N. Osobennosti izgotovlenija PKM metodom RFI [Peculiarities of PCM by RFI] //Trudy VIAM. 2013. №4. St. 03 (viam-works.ru).
  9. Muhametov R.R., Ahmadieva K.R., Chursova L.V., Kogan D.I. Novye polimernye svjazujushhie dlja perspektivnyh metodov izgotovlenija konstrukcionnyh voloknistyh PKM [New polymeric binders for the promising methods for the manufacture of structural fibrous PCM] //Aviacionnye materialy i tehnologii. 2011. №2. S. 38–42.
  10. Muhametov R.R., Ahmadieva K.R., Kim M.A., Babin A.N. Rasplavnye svjazujushhie dlja perspektivnyh metodov izgotovlenija PKM novogo pokolenija [Melt binders for advanced methods of manufacturing a new generation of PCM] //Aviacionnye materialy i tehnologii. 2012. №S. S. 260–265.
  11. Prepreg i izdelie, vypolnennoe iz nego [Prepreg and a product made therefrom]: pat. 2427594 Ros. Federacija; opubl. 21.12.2009.
  12. Aleksashin V.M., Antjufeeva N.V. Razvitie metodov termicheskogo analiza v issledovanii polimernyh kompozicionnyh materialov [Development of methods for thermal analysis in the polymer composite material] /V sb. 75 let. Aviacionnye materialy i tehnologii. Izbrannye trudy «VIAM» 1932–2007. M.: VIAM. 2007. S. 245–249.
  13. Antjufeeva N.V., Aleksashin V.M., Zhelezina G.F., Stoljankov Ju.V. Metodicheskie podhody termoanaliticheskih issledovanij dlja ocenki svojstv prepregov i ugleplastikov [Methodological approaches thermoanalytical studies to evaluate the properties of the prepreg and carbon fiber reinforced plastics] //Prilozhenie k zhurnalu «Vse materialy. Jenciklopedicheskij spravochnik». 2012. №4. S. 18–28.
  14. Gunjaev G.M., Kablov E.N., Aleksashin V.M. Modificirovanie konstrukcionnyh ugleplastikov uglerodnymi nanochasticami [Modification of structural carbon fiber reinforced plastics with carbon nanoparticles] //Rossijskij himicheskij zhurnal. 2010. T. 54. №1. S. 3–11.
  15. Kablov E.N., Kondrashov S.V., Jurkov G.Ju. Perspektivy ispol'zovanija uglerodsoderzhashhih nanochastic v svjazujushhih dlja polimernyh kompozicionnyh materialov [Prospects for the use of carbonaceous nanoparticles in polymeric binders for composite materials] //Rossijskie nanotehnologii. 2013. T. 8. №3–4. S. 24–42.
  16. Kirillov V.N., Starcev O.V., Efimov V.A. Klimaticheskaja stojkost' i povrezhdaemost' polimernyh kompozicionnyh materialov, problemy i puti reshenija [Weather resistance and a defect of polymeric composite materials, problems and solutions] //Aviacionnye materialy i tehnologii. 2012. №S. S. 412–423.
  17. Kirillov V.N., Efimov V.A., Shvedkova A.K., Nikolaev E.V. Issledovanie vlijanija klimaticheskih faktorov i mehanicheskogo nagruzhenija na strukturu i mehanicheskie svojstva PKM [Investigation of the influence of climatic factors and mechanical loading on the structure and mechanical properties of the PCM] //Aviacionnye materialy i tehnologii. 2011. №4. S. 41–45.
  18. Antjufeeva N.V., Stoljankov Ju.V., Ishodzhanova I.V. Issledovanie i ocenka svojstv polimernyh kompozicionnyh materialov po metodikam, garmonizirovannym s mezhdunarodnymi standartami [Research and evaluation of properties of polymeric composite materials according to the procedures harmonized with international standards] //Konstrukcii iz kompozicionnyh materialov. №3. 2013. S. 41–45.
  19. ASTM D5687М-95. 2002.
  20. ISO 20134. 2003.
  21. Portnoj K.I., Salibekov S.E., Svetlov I.L., Chubarov V.M. Struktura i svojstva kompozicionnyh materialov [Structure and properties of composite materials]. M. Mashinostroenie. 1979. 255 s.
  22. Chabina E.B., Alekseev A.A., Filonova E.V., Lukina E.A. Primenenie metodov analiticheskoj mikroskopii i rentgenostrukturnogo analiza dlja issledovanija strukturno-fazovogo sostojanija materialov [Application of the methods of analytical microscopy and X-ray analysis for the study of structural-phase state materials] //Trudy VIAM. 2013. №5. St. 06 (viam-works.ru).
  23. Baurova N.I. Mikrostrukturnye issledovanija poverhnostej razrushenija ugleplastika [Microstructural studies of the fracture surfaces of CFRP] //Vse materialy. Jenciklopedicheskij spravochnik. Kompozicionnye materialy. 2012. №8. S. 25–30.
  24. Cherepanov G.P. Mehanika razrushenija kompozicionnyh materialov [Fracture mechanics of composite materials]. M.: Nauka. 1983. S. 32–37.