High-temperature coatings оn basis of sol-gel technology

Solntsev St.S., Rosenenkova V.A., Mironova N.A., Solovyova G.A.
Solntsev St.S., Rosenenkova V.A., Mironova N.A., Solovyova G.A. High-temperature coatings оn basis of sol-gel technology // Proceedings of VIAM. 2014. No. 1. DOI: 10.18577/2307-6046-2014-0-1-3-3. URL: https://www.viam-works.ru/en/journal/2014/1/3
Abstract

Consideration high-temperature erosion and functional of coatings for heat- protec-tion, heat-insulation, pack condense materials and technology coatings. Demonstration results testings and effectiveness of sol-gel technology repairs, marking and other func-tional coatings.

Reference list
  1. Kablov E.N. Strategicheskie napravleniya razvitiya materialov i tehnologiy ih pererabotki na period do 2030 goda [Strategic directions of the development of materials and technologies of their processing for the period until 2030] //Aviatsionnye materialy i tehnologii. 2012. №S. S. 7–17.
  2. Ospennikova O.G. Strategiya razvitiya zharoprochnyh splavov i staley spetsial'nogo naznacheniya, zaschitnyh i teplozaschitnyh pokrytiy [Development strategy of heat-resistant alloys and special-purpose steels, protective and thermal-protective coatings] //Aviatsionnye materialy i tehnologii. 2012. №S. S. 19–36.
  3. Solntsev St.S., Rozenenkova V.A., Mironova N.A. Vysokotemperaturnye steklokeramicheskie pokrytiya i kompozitsionnye materialy [High-temperature glass-ceramic coatings and composite materials] //Aviatsionnye materialy i tehnologii. 2012. №S. S. 359–368.
  4. Rozenenkova V.A., Solntsev St.S., Mironova N.A. Steklokeramicheskie elektroizolyatsionnye pokrytiya dlya tolstoplenochnyh energonasyschennyh sistem [Glass-ceramic insulating coatings for thick-film energy-intensive systems] //Steklo i keramika. 2013. №7. S. 27–29.
  5. Jones R.W. Sol-gel preparation of ceramics and glasses [Sol-gel preparation of ceramics and glasses] //Metals and Materials. 1988. December. P. 748–751.
  6. Livage J. Sol-gel processing of metal oxides [Sol-gel processing of metal oxides] //Chemica Scripta. 1988. V. 28. P. 9–13.
  7. Sumio Sakka. Sol-gel glasses and their future applications [Sol-gel glasses and their future applications] //Trans. of the Indian Ceramic Society. 1987. V. 46. №l. P. 1–11.
  8. Solntsev St.S. High-Temperature CompositeMaterials and Coatings on the Basis of Glass and Ceramics for Aerospase Technics [High-Temperature Composite Materials and Coatings on the Basis of Glass and Ceramics for Aerospace Techniques] //Russian Journal of General Chemistry. 2001. V. 81. №5. P. 992–1000.
  9. Rozenenkova V.A., Solntsev St.S., Mironova N.A., Gavrilov S.V. Keramicheskie pokrytiya dlya gradientnyh vysokotemperaturnyh teplozaschitnyh materialov [Ceramic coatings for thermal-protective high-temperature gradient materials] //Steklo i keramika. 2013. №1. S. 29–33.
  10. Solntsev St.S., Rozenenkova V.A., Mironova N.A., Solov'eva G.A. Vysokotemperaturnye pokrytiya dlya voloknistyh teploizolyatsionnyh materialov [High-temperature coatings for fibrous heat-insulating materials] //Steklo i keramika. 2013. №5. S. 27–31.
  11. Schetanov B.V., Ivahnenko Yu.A., Babashov V.G. Teplozaschitnye materialy [Thermal-protective materials] //Rossiyskiy Himicheskiy zhurnal. 2010. T. LIV. №1. S. 12–19.
  12. Solntsev St.S. Vysokotemperaturnye kompozitsionnye materialy i pokrytiya na osnove stekla i keramiki [High-temperature composite materials and glass- and ceramic-based coatings] /V sb.: Aviatsionnye materialy. Izbrannye trudy «VIAM» 1932–2007. Yubileynyj nauch.-tehnich. sb. M.: VIAM. 2007. S. 90–99.
  13. Ivahnenko Yu.A., Babashov V.G., Zimichev A.M., Tinyakova E.V. Vysokotemperaturnye teploizolyatsionnye i teplozaschitnye materialy na osnove volokon tugoplavkih soedineniy [High-temperature heat-insulating and thermal-protective materials based on refractory compound fibers] //Aviatsionnye materialy i tehnologii. 2012. №S. S. 380–385.
  14. Solntsev Ct.C. Zaschitnye tehnologicheskie pokrytiya i tugoplavkie email [Protective processing coatings and refractory enamels]. M.: Mashinostroenie. 1984. 255 s.
  15. Solntsev St.S. Zaschitnye pokrytiya metallov pri nagreve [Protective coatings for metals at heating]: Spravochnoe posob. 2-e izd. M.: Librokom. 2009. 248 s.
  16. Solntsev S.S. Rozenenkova V.A. Mironova N.A. Gavrilov S.G. Teplozaschitnyj material na osnove keramicheskih armiruyuschih napolniteley [Thermal-protective material based on ceramic reinforcing fillers] //Steklo i keramika. 2012. №4. S. 22–25.
  17. Solntsev St.S., Rozenenkova V.A., Mironova N.A., Gavrilov S.V. Zaschitnye tehnologicheskie pokrytiya dlya termicheskoy obrabotki vysokoprochnyh staley tipa VKS [Protective coatings for thermal processing of VKS-type high-strength steels] //Steklo i keramika. 2011. №10. S. 28–30.
  18. Kondrashov E.K., Kozlova A.A., Malova N.E. Issledovanie kinetiki otverzhdeniya ftorpoliuretanovyh emaley alifaticheskimi poliizotsianatami razlichnyh tipov [Kinetics study of fluoropolyurethane enamels curing by aliphatic polyisocyanates of various types] //Aviatsionnye materialy i tehnologii. 2013. №1. S. 48‒49.
  19. Nefedov N.I., Semenova L.V. Tendentsii razvitiya v oblasti konformnyh pokrytiy dlya vlagozaschity i elektroizolyatsii plat pechatnogo montazha i elementov radioelektronnoy apparatury [Trends in the development of conformal coatings for moisture protection and electrical insulation of printed-circuit boards and radio equipment components] //Aviatsionnye materialy i tehnologii. 2013. №1. S. 50‒52.