Multi-layer protective and decorative material for decorating details in the cabin of aircraft and helicopters

Nesterova T.A., Barbotko S.L., Nikolaeva M.F., Gerter J.A.
Nesterova T.A., Barbotko S.L., Nikolaeva M.F., Gerter J.A. Multi-layer protective and decorative material for decorating details in the cabin of aircraft and helicopters // Proceedings of VIAM. 2013. No. 8. URL: https://www.viam-works.ru/en/journal/2013/8/4
Abstract

Developed a multi-layer protective and decorative material mark «poliplex» which is a one-way fiberglass protective and decorative coating of rubber-based copolymers of ftoroplast. The physical, physico - mechanical properties of the material, fireproof  properties of the material, and also as a part of covering and three-layered sandwich structures are studied. Material meets the requirements of domestic and foreign aviation regulations AP-25, FAR 25 and CS-25 on fireproof properties (flammability, smoke generation and heat dissipation). Material multi-layer protective and decorative mark «poliplex» is recommended for the decoration of walls, ceilings, storage compartments and other parts made of glass-, organic plastics and three-layered sandwich panels in the cabin of aircraft and helicopters, as well as a repair option. Material «polyplex» can be opera