Glass reinforced plastics on the basis of thermoplastic matrix

Beider E.Ya., Petrova G.N., Izotova T.F., Barbotko S.L.
Beider E.Ya., Petrova G.N., Izotova T.F., Barbotko S.L. Glass reinforced plastics on the basis of thermoplastic matrix // Proceedings of VIAM. 2013. No. 7. URL: https://www.viam-works.ru/en/journal/2013/7/3
Abstract

In the article the physical, mechanical and fire-resistant properties of glass reinforced plastics based on heat-resistant thermoplastic binders, made in RF, are given. It is shown, that materials have high strength properties and satisfied the standards of AP-25, FAR-25.853 for fire safety.