Development of the method of static bend angle determining of friction welded samples made from steel VKS-180-ID

Samorukov M.L.
Samorukov M.L. Development of the method of static bend angle determining of friction welded samples made from steel VKS-180-ID // Proceedings of VIAM. 2013. No. 6. URL: https://www.viam-works.ru/en/journal/2013/6/5
Abstract

The article is about the results of determining of static bending angle of welded samples made by continuous drive friction welding. The drawing of the test sample is shown. Тhe methodology of determining of static bending angle is developed.