Technology of receiving samples for certification of the heat resisting alloys melted with application of waste of foundry production of plants of branch

Belicov A.V., Gerasimov V. V., Visik E.M.
Belicov A.V., Gerasimov V. V., Visik E.M. Technology of receiving samples for certification of the heat resisting alloys melted with application of waste of foundry production of plants of branch // Proceedings of VIAM. 2013. No. 6. URL: https://www.viam-works.ru/en/journal/2013/6/2
Abstract

The article is devoted to the description of the certification process of the mechanical properties of the material semifinished-products manufactured in VIAM with the use of foundry waste plants of the industry. Asked for producing monocrystalline billets for samples for determination of mechanical properties of technical conditions on alloy use полупромышленную installation of directional solidification In 1790, which gives a great economic effect in the case of small-tonnage production and supply of alloys on the requests of the enterprises of the industry.