Development and researching of thermostable sol-gel coatings in Y2O3–AL2O3–SIO2 system for SiC-based materials
Lebedeva Yu.E., Grachshencov D.V., Popovich N.V., Orlova L.A., Chaynikova A.S. Development and researching of thermostable sol-gel coatings in Y2O3–AL2O3–SIO2 system for SiC-based materials // Proceedings of VIAM. 2013. No. 12. URL: https://www.viam-works.ru/en/journal/2013/12/3
Abstract
In the course of the work with purpose of the obtaining by sol-gel method protective high-temperature coatings of Y2O3–Al2O3–SiO2 system technique of the preparation film-formation solution was perfected, influence of the components ratio in initial solution on physic-chemical characteristics of solutions, gels and sintered materials was studied, phase formations were studied. Application capability of this coatings to protective SiC materials at high temperature was investigated.
Reference list
- Kablov E.N. Strategicheskie napravleniya razvitiya materialov i tehnologiy ih pererabotki na period do 2030 goda [Strategic directions of the development of materials and technologies of their processing for the period until 2030] //Aviatsionnye materialy i tehnologii. 2012. №S. S. 7–17.
- Kablov E.N., Graschenkov D.V., Isaeva N.V., Solntsev S.S. Perspektivnye vysokotemperaturnye keramicheskie kompozitsionnye materialy [Advanced high-temperature ceramic composite materials] //Rossiyskiy himicheskiy zhurnal. 2010. T. LIV. №1. S. 20–24.
- Simonenko E.P., Simonenko N.P., Sevast'yanov V.G., Graschenkov D.V., Kuznetsov N.T., Kablov E.N. Funktsional'no gradientnyj kompozitsionnyj material SiC/(ZrO2–HfO2–Y2O3), poluchennyj s primeneniem zol'-gel' metoda [Functionally gradient com-posite material SiC/(ZrO2–HfO2–Y2O3) produced by sol-gel method] //Kompozity i nanostruktury. 2011. №4. S. 52–64.
- Graschenkov D.V., Chursova L.V. Strategiya razvitiya kompozitsionnyh i funktsional'nyh materialov [Development strategy of composite and functional materials] //Aviatsionnye materialy i tehnologii. 2012. №S. S. 231–242.
- Solntsev S.S., Rozenenkova V.A., Mironova N.A. Vysokotemperaturnye steklokeram-icheskie pokrytiya i kompozitsionnye materialy [High-Temperature Glass-Ceramic Coat-ings and Composite Materials] //Aviatsionnye materialy i tehnologii. 2012. №S. 359–368.
- Graschenkov D.V., Solntsev S.St., Schegoleva N.E., Naumova A.S., Gaponov B.N. Steklokeramicheskiy kompozitsionnyj material [Glass-Ceramic Composite Material] //Aviatsionnye materialy i tehnologii. 2012. №S. S. 368–372.
- Krenkel W., Berndt F. C/C–SiC composites for space applications and advanced friction systems //Materials Science and Engineering A. 2005. V. 412. №1–2. Р. 177–181.
- Westwood M.E., Hayes F.H., Day R.J., Taylor R. Oxidation Protection of Ceramic Composites with Carbon Fibre Reinforsment //J. Mater. Sci. 1996. V. 31. P. 1389–1397.
- Jacobson N.S. Corrosion of silicon-based ceramics in combustion environments //J. Eur. Ceram. Soc. 1993. V. 76. Р. 3–28.
- Huang J.-F., Li H.-J., Zeng X.-R. Influence of preparation technology on the microstructure and anti-oxidation property of SiC–Al2O3-mullite multi-coatings for carbon/carbon composites //Applied Surfase Science. 2006. V. 252. Р. 4244–4249.
- Cabet C. Review: Oxidation of SiC/SiC Composites in Low Oxidizing and High Tem-perature Environment /Materials Issues for Generation IV Systems. 2008. R. 351–366.
- Mironov V.V., Kochetkov Yu.M., Vvedenskiy V.S. i dr. Eksperimental'nye issledovaniya rabotosposobnosti tonkostennyh neohlazhdaemyh sopel ZhRD iz uglerodnyh kompozitsionnyh materialov [Experimental studies of operability of thin-walled un-cooled composite nozzles of LRE made of carbon composite materials] //Aviakosmicheskaya tehnika i tehnologiya. 2001. №3. S. 55–61.
- Toropov I.A. i dr. Diagrammy sostoyaniya silikatnyh system [Phase diagrams of silicate systems: Handbook]: Spravochnik. M.-L.: Nauka. 1965. 258 s.
- Harrysson R., Vomacka P Glass formation in the system Y2O3–Al2O3–SiO2 under conditions of laser melting //J. of the European Ceramic Society. 1994. №14. P. 377–380.
- Toropov I.A., Bondar' I.A., Lazarev A.N., Smolin Yu.I. Silikaty redkozemel'nyh elementov i ih analogi [Silicates of rare-earth elements and their analogues]. L.: Nauka. 1971. 230 s.
- www.mincryst.ru
- Shima J.B., Yoshikawa A., Nikl M., Soloviev N., Pejchal J., Yoon D.H., Fukuda T. Growth and characterization of Yb3+-doped YAlO3 fiber single crystals grown by the modified micro-pulling-down method //Journal of Crystal Growth. 2003. №256. Р. 298–304.
- Liang Wu, Guanghua Liu, Jiangtao Li, Bin He, Zengchao Yang, Yixiang Chen Dependence of glass-forming ability on starting compositions in Y2O3–Al2O3–SiO2 system //Ceramics – Silikáty. 2011. V. 55. №3. P. 228–231.
- Del' Pino K.H.S. Termicheskoe razlozhenie i nekotorye fiziko-himicheskie svoystva kristallogidratov nitrata ittriya [Thermal decomposition and some physical-chemical properties of yttrium nitrate crystalline hydrates]: Avtoref. dis. k.h.n. M.: RHTU im. Mendeleeva. 1981. 16 s.
- Yahong Zhang, Navrotsky A. Thermochemistry of Glasses in the Y2O3–Al2O3–SiO2 System //J. Am. Ceram. Soc. 2003. V. 86. №10. P. 1727–1732.
- Shen Xiaoyi, Zhai Yuchun Preparation and optical properties of Y2O3/SiO2 powder //Rare metals. 2011. V. 30. №1. Р. 33–38.
- MacLaren I., Richter G. The structure and possible origins of stacking faults in gamma-yttrium disilicate //Philosophical Magazine. 2009. V. 89. №2. P. 169–181.
- Ya-Qin Wang, Jian-Feng Huang, Li-Yun Cao,1 and Xie-Rong Zeng Direct Preparation of Y2SiO5 Nanocrystallites by a Microwave Hydrothermal Process //ISRN Nanotech-nology. 2011. V. 1. P. 1–5.
- Ziqi Sun, Meishuan Li, Yanchun Zhou Thermal properties of single-phase Y2SiO5 //Journal of the European Ceramic Society. 2009. №29. P. 551–557.
- Zarzyki J. Past and Present of Sol-Gel Science and Technology //J. of Sol-Gel Science and Technology. 1997. №8. Р. 17–22.
- Mackenzie J.D. Sol-Gel Research-Achievements Since 1981 and Prospects for the Fu-ture //J. of Sol-Gel Science and Technology. 2003. №26. Р. 23–27.
- Andrianov N.T. Zol'-gel' metod v tehnologii oksidnyh materialov [The sol-gel method in the oxide materials technology] //Steklo i keramika. 2003. №10. S. 17–22.
- Atkinson A., Segal D.L. Some Recent Developments in Aqueous Sol-Gel Processing //J. of Sol-Gel Science and Technology. 1998. №13. Р. 133–139.
- Simonenko E.P., Ignatov N.A., Simonenko N.P., Ezhov Yu.S., Sevast'yanov V.G., Kuznetsov N.T. Sintez vysokodispersnyh sverhtugoplavkih karbidov tantala-tsirkoniya Ta4ZrC5 i tantala-gafniya Ta4HfC5 cherez zol'-gel' tehniku [Synthesis of fine-grained ultra-refractory carbides of tantalum-zirconium Ta4ZrC5 and tantalum-hafnium Ta4HfC5 by the sol-gel techniques] //Zhurnal neorganicheskoy himii. 2011. №56 (11). S. 1763–1769.
- Sevast'yanov V.G., Simonenko E.P., Simonenko N.P., Kuznetsov N.T. Sintez vysokodispersnogo tugoplavkogo oksida tsirkoniya–gafniya–ittriya s ispol'zovaniem zol'-gel' tehniki [Synthesis of fine-grained refractory oxide of zirconium-hafnium-yttrium by the sol-gel techniques] //Zhurnal neorganicheskoy himii. 2012. №57 (3). S. 355–361.
- Lebedeva Yu.E., Popovich N.V., Orlova L.A. Zaschitnye vysokotemperaturnye pokrytiya dlya kompozitsionnyh materialov na osnove SiC [High-temperature protective coatings for SiC-based composite materials] //Trudy VIAM. 2013. №2 (elektronnyj zhurnal).
- Uvarova N.E., Orlova L.A., Lebedeva Yu.E., Graschenkov D.V. Primenenie metoda elektronnogo paramagnitnogo rezonansa dlya izucheniya strukturnyh izmeneniy v protsesse geleobrazovaniya pri poluchenii keramiki i steklokeramiki zol'-gel' metodom [Usage of electron paramagnetic resonance for studying the structural changes during the gel formation process when producing ceramics and glass ceramic by the sol-gel method] //Aviatsionnye materialy i tehnologii. 2011. №3. S. 26–30.
- Aparacio M., Duran A. Yttrium silicate Coatings for Oxidation Protection of Carbon-silicon Carbide Composites [Yttrium silicate Coatings for Oxidation Protection of Carbon-silicon Carbide Composites] //J. Amer. Ceram. Soc. 2000. V. 83. №6. P. 1351–1355.
- Kolitsch U., Seifert H.J., Ludwig T., Aldinger F Phase equilibria and crystal chemistry in the Y2O3–Al2O3–SiO2 system [Phase equilibria and crystal chemistry in the Y2O3–Аl2О3–SiO2 system] //J. of Materials Research. 1999. V. 14. №2. Р. 447–455.
- Sarkisov P.D., Orlova L.A., Popovich N.V., Anan'eva Yu.E. Protsessy strukturoobrazovaniya pri poluchenii ittriysilikatnyh materialov zol'-gel' metodom [Structure formation processes in the course of production of yttrium silicate materials by the sol-gel method] //Steklo i keramika. 2007. №1. S. 3–6.
- Ziqi Sun, Meishuan Li, Yanchun Zhou Kinetics and Mechanism of Hot Corrosion of γ-Y2Si2O7 in Thin-Film Na2SO4 Molten Salt [Kinetics and mechanism of hot corrosion of γ-Y2Si2O7 in thin-film Na2SO4 molten salt] //J. Am. Ceram. Soc. 2008. V. 91. №7. P. 2236–2242.