Thermoplastic binders. The present and the future

Tkachuk A.I., Grebeneva T.A., Chursova L.V., Panina N.N.
Tkachuk A.I., Grebeneva T.A., Chursova L.V., Panina N.N. Thermoplastic binders. The present and the future // Proceedings of VIAM. 2013. No. 11. URL: https://www.viam-works.ru/en/journal/2013/11/7
Abstract

Provides an overview of types of thermoplastic binder, the focus is on the most promising for the preparation of polymer composites are currently thermoplastic binder. The assessment of the advantages and disadvantages of both operational and technological characteristics super-engineering thermoplastics. Describe techniques for improving process performance super-engineering thermoplastics processing in polymeric composite materials.

Reference list
  1. Kablov E.N. Strategicheskie napravleniya razvitiya materialov i tehnologiy ih pererabotki na period do 2030 goda [Strategic directions of the development of materials and technologies of their processing for the period until 2030] //Aviatsionnye materialy i tehnologii. 2012. №S. S. 7–17.
  2. Graschenkov D.V., Chursova L.V. Strategiya razvitiya kompozitsionnyh i funktsional'nyh materialov [Development strategy of composite and functional materials] //Aviatsionnye materialy i tehnologii. 2012. №S. S. 231–242.
  3. Chursova L.V., Kim M.A., Panina N.N., Shvetsov E.P. Nanomodifitsirovannoe epoksidnoe svyazuyuschee dlya stroitel'noy industrii [Nanomodified Epoxy Binder for the Construction Industry] //Aviatsionnye materialy i tehnologii. 2013. №1. S. 40–47.
  4. Chursova L.V., Raskutin A.E., Gurevich Ya.M., Panina N.N. Svyazuyuschee holodnogo otverzhdeniya dlya stroitel'noy industrii [Cold-cured Binder for the Construction Industry] //Klei. Germetiki. Tehnologii. 2012. №5. S. 40–44.
  5. Petrova G.N., Perfilova D.N., Gryaznov V.I., Beyder E.Ya. Termoplastichnye elastomery dlya zameny rezin [Thermoplastic elastomer for the substitution of rubbers] //Aviatsionnye materialy i tehnologii. 2012. №S. S. 302–308.
  6. Petrova G.N., Beyder E.Ya. Konstruktsionnye materialy na osnove armirovannyh termoplastov [Structural materials based on reinforced thermoplastics] //Rossiyskiy himicheskiy zhurnal. 2010. T. LIV. №1. S. 34–40.
  7. Petrova G.N., Beyder E.Ya. Lit'evye termoplasticheskie materialy aviakosmicheskogo naznacheniya [Molding thermoplastic materials of aerospace application] //Rossiyskiy himicheskiy zhurnal. 2010. T. LIV. №1. S. 41–45.
  8. Petrova G.N., Rumyantseva T.V., Perfilova D.N., Beyder E.Ya., Gryaznov V.I. Termoelastoplasty – novyj klass polimernyh materialov [Thermoelastoplastics – a new class of polymer materials] //Aviatsionnye materialy i tehnologii. 2010. №4. S. 20–25.
  9. Biron M. 8 – Future Prospects for Thermoplastics and Thermoplastic Composites //Thermoplastics and Thermoplastic Composites (Second Edition). 2013. A volume in Plastics Design Library. P. 985–1025.
  10. Katsevman M.L. Polimernye kompozity i lokalizatsiya [Polymer composites and localization] //The Chemical Journal. 2013. №1–2. S. 66–69.
  11. Mihaylin Yu.A. Konstruktsionnye polimernye kompozitsionnye materialy [Structural polymer composite materials]. SPb.: NOT. 2008. 820 s.
  12. Kerber M.L., Vinogradov V.M. Polimernye kompozitsionnye materialy: struktura, svoystva, tehnologiya [Polymer composite materials: structure, properties, technology]. SPb.: Professiya. 2009. 560 s.
  13. Mett'yuz F., Rolings R. Kompozitsionnye materialy. Mehanika i tehnologiya [Composite materials. Mechanics and technology]: Per. s angl. M.: Tehnosfera. 2004. 408 s.
  14. Berlin Al.Al. Sovremennye polimernye kompozitsionnye materialy [Modern polymer composite materials] //Sorosovskiy obrazovatel'nyj zhurnal. 1995. №1. S. 57–65.
  15. Evraziyskiy himicheskiy rynok. Novye polimery: polifenilensul'fid [Eurasian Chemical Market. New polymers: polyphenylene sulfide] //Mezhdunarodnyj delovoy zhurnal. 2008. T. 39. №3. S. 14–21.
  16. Ebnesajjad S., Morgan R.A. 11 – Applications of Processing Aid Additives //Fluoropolymer Additives. 2012. A volume in Plastics Design Library. P. 193–209.
  17. Rungsima Homklina, Nattakarn Hongsriphan. Mechanical and Thermal Properties of PLA/PBS Co-continuous Blends Adding Nucleating Agent //Energy Procedia. 2013. V. 34. P. 871–879.
  18. Mukhopadhyay S., Fangueiro R. Physical Modification of Natural Fibers and Thermoplastic Films for Composites – A Review //Journal of Thermoplastic Composite Materials. 2009. V. 22. №2. P. 135–162.
  19. Tay G.S., Shannon-Ong S.H., Goh S.W., Rozman H.D. Thermoplastic–lignocellulose composites enhanced by chemically treated Alcell lignin as compatibilizer //Journal of Thermoplastic Composite Materials. 2013. V. 26. №6. P. 733–746.