The preparation and use of the polimer film coated with a transparent conductive oxide doped indium

Kislyakov P.P., Khokhlov Y.A., Krynin A.G., Kondrashov S.V.
Kislyakov P.P., Khokhlov Y.A., Krynin A.G., Kondrashov S.V. The preparation and use of the polimer film coated with a transparent conductive oxide doped indium // Proceedings of VIAM. 2013. No. 11. URL: https://www.viam-works.ru/en/journal/2013/11/6
Keywords
ITO
Abstract

Studied the possibility stabilizing the reactive magnetron discharge when applying ITO coating by maintaining optimum oxygen partial pressure and maintain the ratio of the intensities of the emission of excited atoms of indium and oxygen. The possibility of application the films as the transparent heating element and comprising an optically active material glazing.

Reference list
  1. Dobrowolski J. A., Ho F. C., Menagh D., Simpson R., and Waldorf A. Transparent conducting indium tin oxide films formed on low or medium temperature substrates by ion-assisted deposition //Applied Optics. 1987. V. 26, Issue 24. P. 5204–5210.
  2. Bazhin A.I., Trotsan A.N., Chertopalov S.V., Stipanenko A.A., Stupak V.A. Vliyanie rezhima magnetronnogo raspyleniya i sostava reaktsionnogo gaza na strukturu i svoystva plenok ITO [An effect of the magnetron sputtering conditions and composition of the reaction gas on the structure and properties of ITO films] //FIP PSE. 2012. T. 10. V. 10. № 4. S. 342–349.
  3. Zaytseva E.A., Zakirova R.M., Krylov P.N., Lebedev K.S., Fedotova I.V. Vliyanie ionnoy obrabotki v protsesse VCh magnetronnogo raspyleniya na tolschinu i pokazatel' prelomleniya ITO plenok [Effect of ion-beam processing in the process of high-frequency magnetron sputtering on the thickness and refractive index of ITO films] //Vestnik udmurtskogo universiteta. 2012. Vyp. 2. Fizika. Himiya. S. 26–30.
  4. Hohlov Yu.A., Krynin A.G., Bogatov V.A., Kislyakov P.P. Opticheskie konstanty tonkih plenok oksida indiya, legirovannogo olovom, osazhdennyh na polietilen-tereftalatnuyu plenku metodom reaktivnogo magnetronnogo raspyleniya (blizhnyaya in-frakrasnaya oblast' spektra) [Optical Constants of Thin Indium Oxide Films, Alloyed by Tin and Deposited onto Polyethylene Terephthalate Film by the Reactive Magnetron Sputtering Method (Infrared Short-Range Region of Spectrum)] //Aviatsionnye materi-aly i tehnologii. 2013. №1. S. 24–28.
  5. Martin P.J., Netterfield R.P., McKenzie D.R. Properties of indium tin oxide films prepared by ion-assisted deposition Original Research Article //Thin Solid Films. 1986. V. 137. №2. P. 207–214.
  6. Sposob naneseniya pokrytiya dlya zaschity ot vysokotemperaturnogo okisleniya poverhnosti vnutrenney polosti ohlazhdaemyh lopatok turbin iz bezuglerodistyh zharoprochnyh splavov na osnove nikelya [Method of coating deposition for protection against high-temperature oxidation of the surface of inner cavity of cooled turbine blades made of carbon-free high-temperature nickel-based alloys]: pat. 2471887 Ros. Federatsiya; opubl. 17.10.2011.
  7. Metody issledovaniya plazmy. Spektroskopiya, lazery, zondy [Methods of plasma studies. Spectroscopy, lasers, probes] /Pod red. V. Lohte-Hol'tgrevena. M.: Mir. 1971. 552 s.
  8. Grishin S.D., Mamonov V.I., Marahtanov M.K., Ponkratov A.B., Hohlov Yu.A. K voprosu ob opredelenii elektronnoy temperatury zamagnichennoy plazmy nizkoy kontsentratsii spektral'nymi metodami s pomosch'yu opornyh zondovyh izmereniy [On the determination of the electron temperature of magnetized low-concentration plasma by spectral methods using the reference probe measurements] //Teplofizika vysokih temperatur. 1986. T. 24. №2. S. 398–400.