Transparent interfrence coating for functional glass materials

Krynin A.G., Khokhlov Y.A., Bogatov V.A., Kislyakov P.P.
Krynin A.G., Khokhlov Y.A., Bogatov V.A., Kislyakov P.P. Transparent interfrence coating for functional glass materials // Proceedings of VIAM. 2013. No. 11. URL: https://www.viam-works.ru/en/journal/2013/11/5
Abstract

The results of studies of the functional properties of the transparent heat-radioprotective aircraft glazing material on the basis of organic glass with optical interference coating, and the results of environmental tests of experimental models of heat-radioprotective glazing are done.

Reference list
  1. Boeing B 747 Cockpit Windows. www.sierracin.com.
  2. Bogatov V.A., Zaharov S.S., Kislyakov P.P., Krynin A.G., Hohlov Yu.A. Vliyanie rezhimov magnetronnogo napyleniya na optiko-fizicheskie svoystva mednyh nanopokrytiy [Effect of magnetron sputtering conditions on the optical and physical properties of copper nano-coatings] //Nanomaterialy i nanotehnologii. 2011. №4. S. 45–53.
  3. Hohlov Yu.A., Krynin A.G., Bogatov V.A., Kislyakov P.P. Opticheskie konstanty tonkih plenok oksida indiya, legirovannogo olovom, osazhdennyh na polietilen-tereftalatnuyu plenku metodom reaktivnogo magnetronnogo raspyleniya (blizhnyaya in-frakrasnaya oblast' spektra) [Optical Constants of Thin Films of Indium Oxide Alloyed with Tin and Deposited onto Polyethylene Terephthalate Film by the Reactive Magnetron Sputtering Method (Infrared Short-Range Region of Spectrum)] //Aviatsionnye materialy i tehnologii. 2013. №1. S. 24–28.
  4. Rodriguez J., Gomez M., Ederth J., Niklasson G.A., Granqvist C.G. Thickness dependence of the optical properties of sputter deposited Ti oxide films //Thon Solid Films. 2010. V. 365. Р. 119–125.
  5. Zaharov A.N., Kovsharov N.F., Oskomov K.V., Rabotkin S.V., Solov'ev A.A., Sochugov N.S. Svoystva nizkoemissionnyh pokrytiy na osnove Ag i Su, nanesennyh na polimernuyu plenku metodom magnetronnogo raspyleniya [Properties of Ag and Cu-based low-emission coatings deposited on a polymer film by the magnetron sputtering method] //Perspektivnye materialy. 2012. №2. S. 62–70.
  6. Putilin E.S. Opticheskie pokrytiya: Ucheb. posob. [Optical coatings: Study guide] SPb.: GUITMO. 2005. 230 s.
  7. Berning P.H. Teoriya i metody rascheta opticheskih svoystv tonkih plenok [Theory and computational methods of optical properties of thin films] //Fizika tonkih plenok. T. 1 /Pod red. G. Hassa. M.: Mir. 1967. S. 91–151.
  8. Krylova T.N. Interferentsionnye pokrytiya [Interference coatings]. L.: Mashinostroenie. 1973. S. 30–34.
  9. Danilin B.S., Syrchin V.K. Magnetronnye raspylitel'nye sistemy [Magnetron sputtering systems]. M.: Radio i svyaz'. 1982. 73 s.
  10. Hohlov Yu.A. Tehnologiya opticheskih pokrytiy [Technology of optical coatings]. M.: MGTU im. Baumana. 2004. 81 s.
  11. Solov'ev A.A., Zaharov A.N., Rabotkin S.V., Oskomov K.V., Sochugov N.S. Harakteristiki plazmy nesbalansirovannoy magnetronnoy raspylitel'noy sistemy i ih vliyanie na parametry pokrytiy ZnO:Ga [Plasma characteristics of an unbalanced magnetron sputtering system and their effect on parameters of ZnO:Ga coatings] //Fizika i ximiya obrabotki materialov. 2009. №2. S. 58–65.
  12. Hohlov Yu.A., Bogatov V.A., Berezin N.M. Stabilizatsiya reaktivnogo magnetronnogo osazhdeniya magnitnym polem [Stabilization of reactive magnetron sputtering by a magnetic field] //Fizika i himiya obrabotki materialov. 2012. №5. S. 46–50.
  13. Jager S., Szyszka B., Szczyrbowski J., Brauer G. Surface and Coating Technology. 2008. Р. 1304–1314.
  14. Brauer G., Szyszka B., Vergo M., Bandorf R. Magnetron sputtering – Milestones of 30 years //Vacuum. 2010. №84. Р. 1354–1359.
  15. Graschenkov D.V., Chursova L.V. Strategiya razvitiya kompozitsionnyh i funktsional'nyh materialov [Development strategy of composite and functional materials] //Aviatsionnye materialy i tehnologii. 2012. №S. S. 231–241.
  16. Kablov E.N. Strategicheskie napravleniya razvitiya materialov i tehnologiy ih pere-rabotki na period do 2030 goda [Strategical Areas of Developing Materials and Their Processing Technologies for the Period up to 2030] //Aviatsionnye materialy i tehnologii. 2012. №S. S. 7–17.
  17. Grishin S.D., Mamonov V.I., Marahtanov M.K., Hohlov Yu.A. Opredelenie energii ionov v plazme razryada s azimutal'nym dreyfom elektronov [Determination of ions energy in a plasma discharge with the azimuthal electron drift] //Fizika i himiya obrabotki materialov. 1986. №2. S. 131–132.
  18. Nizkoemissionnoe pokrytie, nanesennoe na prozrachnuyu podlozhku [Low-emission coating deposited on a transparent substrate]: pat. 2190692 Ros. Federatsiya; opubl. 10.10.2002.
  19. Bogatov V.A., Kondrashov S.V., Hohlov Yu.A. Mnogofunktsional'nye opticheskie pokrytiya i materialy [Multifunctional Optical Coatings and Materials] //Aviatsionnye materialy i tehnologii. 2012. №S. S. 343–348.
  20. Bogatov V.A., Kondrashov S.V., Hohlov Yu.A. Poluchenie gradientnogo pokrytiya oksinitrida alyuminiya metodom reaktivnogo magnetronnogo raspyleniya [Deposition of gradient aluminium oxynitride coating by the reactive magnetron sputtering method] //Aviatsionnye materialy i tehnologii. 2010. №3. S. 19–21.