Crack growth resistance of aviation materials in fatigue testing

Erasov V.S., Nuzhny G.A., Grinevich A.V., Terekhin A.L.
Erasov V.S., Nuzhny G.A., Grinevich A.V., Terekhin A.L. Crack growth resistance of aviation materials in fatigue testing // Proceedings of VIAM. 2013. No. 10. URL: https://www.viam-works.ru/en/journal/2013/10/6
Abstract

In this paper was proposed a solution of problem determination moment of formation main fatigue crack by the use of resonance test machine. Method of determination cycle number that main crack is form and methods of prediction residual life were offer. Experimental data about determination moment of formation main fatigue crack in aluminum alloys was show.