High-temperature coatings for fibers substratum

Solntsev St.S., Rosenenkova V.A., Mironova N.A., Solovyova G.A.
Solntsev St.S., Rosenenkova V.A., Mironova N.A., Solovyova G.A. High-temperature coatings for fibers substratum // Proceedings of VIAM. 2013. No. 10. URL: https://www.viam-works.ru/en/journal/2013/10/3
Abstract

Consideration high-temperature erosion and functional of coatings for heat-protection, heat-insulation and pack condense materials made of quarts, glass and metallic fibers, filamentary crystals and technology coatings.