The research opportunity to improve service properties of compressor gte blades ion modified surface method

Muboyadzhyan S.A., Lutsenko A.N., Aleksandrov D.A., Gorlov D.S.
Muboyadzhyan S.A., Lutsenko A.N., Aleksandrov D.A., Gorlov D.S. The research opportunity to improve service properties of compressor gte blades ion modified surface method // Proceedings of VIAM. 2013. No. 1. URL: https://www.viam-works.ru/en/journal/2013/1/2
Abstract

In this article will have been discussed effect ion modified of surface to improve service properties steel and titanium compressor’s blades. Have been showed theoretical foundation physical principles manage ion modification surface processing. Have been detected main regularities of properties modify surface from conductive material and technological process options. The results of the research phase and chemical composition, metallography, heat re-sistance and corrosion resistance, mechanical properties of steel and titanium alloys after ion modified.