Ferromagnetic microwires α-Fe/(PrDy)(FeCo)B for micromanipulators and polymer composites
Koplak O.V., Kunitsyna E.I., Valeev R.A., Korolev D.V., Piskorsky V.P., Morgunov R.B. Ferromagnetic microwires α-Fe/(PrDy)(FeCo)B for micromanipulators and polymer composites // Proceedings of VIAM. 2019. No. 11. DOI: 10.18577/2307-6046-2019-0-11-60-67. URL: https://www.viam-works.ru/en/journal/2019/11/7
Keywords
magnetic microwire, pendant drop melt extraction, magnetic hysteresis, bistability, composites.
Abstract
Technology of manufacturing of the α-Fe microwires of 30 μm diameter covered with amorphous (PrDy)(FeCo)B phase with high magnetostriction is developed. The microwires satisfy to technical conditions in rectangular shape of their magnetic hysteresis and geometric parameters. Note that one of the technologies for manufacturing permanent rare-earth magnets includes the stage of preparation of the amorphous phase, which then crystallizes, forming crystallites with a given direction of the main axes of magnetization (magnetic texture). It is this stage that leads to the production of microwires with functional properties.
Reference list
- Varga R., Zhukov A., Zhukova V., Blanco J. M., Gonzalez J. Supersonic domain wall in magnetic microwires // Physical Review B. 2007. Vol. 76. P. 132406. DOI: 10.1103/PhysRevB.76.132406.
- Ivanov Yu.P., del Real R.P., Chubykalo-Fesenko O., Vázquez M. Magnetic reversal modes in cylindrical nanowires // Journal of Applied Physics. 2015. Vol. 115. P. 063909. DOI: 10.1088/0022-3727/46/48/485001/meta.
- Velazquez J., Vazquez M. An analysis of interacting bistable magnetic microwires: from ordered to chaotic behaviours // Physica B: Condensed Matter. 2002. Vol. 320. P. 230–235.
- Peng H., Qin F., Phan M. Ferromagnetic microwire composites. From Sensors to Microwire applications. Series: Engineering Materials and Processes. Springer, 2016. P. 245. DOI: 10.1007/978-3-319-29276-2.
- Szary P., Luciu I., Duday D., Périgo E.A., Wirtz T., Choquet P., Michels A. Synthesis and magnetic properties of Ta/NdFeB-based composite microwires // Journal of Applied Physics. 2015. Vol. 117. P. 17D134. DOI: 10.1063/1.4917058.
- Yamamoto K., Irie T., Takeuchi M. Influence of Cooling Rate on Constituent Phases and Distribution of Elements in (Nd,Dy)–Fe–B Magnet Alloys // Journal of Japan Society of Powder and Powder Metallurgy. 2016. Vol. 63. P. 630. DOI: 10.2497/jjspm.63.630.
- Algarabel P.A., Del Moral A., Ibarra M.R., Marquina C. High field magnetostriction and magnetic thermal expansion of RE2Fe14B hard intermetallics // Journal of Magnetism and Magnetic Materials. 1992. Vol. 114. P. 161.
- Kablov E.N., Ospennikova O.G., Piskorskij V.P., Valeev R.A. i dr. Fazovyj sostav spechennyh materialov sistemy Nd–Dy–Fe–Co–B [Phase composition of Nd–Dy–Fe–Co–B sintered materials] // Aviacionnye materialy i tehnologii. 2014. №S5. S. 95–100. DOI: 10.18577/2071-9140-2014-0-s5-95-100.
- Kablov E.N., Ospennikova O.G., Piskorskij V.P., Rezchikova I.I., Valeev R.A., Davydova E.A. Fazovyj sostav spechennyh materialov sistemy Pr–Dy–Fe–Co–B [Phase composition of the Pr–Dy–Fe–Co–B sintered materials] // Aviacionnye materialy i tehnologii. 2015. №S2 (39). S. 5–10. DOI: 10.18577/2071-9140-2015-0-S2-5-10.
- Kablov E.N., Ospennikova O.G., Cherednichenko I.V., Rezchikova I.I., Valeev R.A., Piskorskij V.P. Vliyanie soderzhaniya medi na fazovyj sostav i magnitnye svojstva termostabilnyh spechennyh magnitov sistem Nd–Dy–Fe–Co–B i Pr–Dy–Fe–Co–B [Influence of Cu content to phase structure and magnetic properties of thermostable sintered magnets of Nd–Dy–Fe–Co–B and Pr–Dy–Fe–Co–B systems] // Aviacionnye materialy i tehnologii. 2015. №S2 (39). S. 11–19. DOI: 10.18577/2071-9140-2015-0-S2-11-19.
- Morgunov R.B., Koplak O.V., Talantsev A.D., Korolev D.V., Piskorskij V.P., Valeev R.A. Fenomenologiya petel magnitnogo gisterezisa v mnogoslojhykh mikroprovodakh α-Fe/DyPrFeCoB [The phenomenology of the magnetic hysteresis loops in multilayer microwires α-Fe/DyPrFeCoB] // Trudy VIAM: elektron. nauch.-tehnich. zhurn. 2019. №7 (79). St. 08. Available at: http://www.viam-works.ru (accessed: September 23, 2019). DOI: 10.18577/2307-6046-2019-0-7-67-75.
- Severino A.M., Gómez-Polo C., Marín P., Vázquez M. Influence of the sample length on the switching process of magnetostrictive amorphous wire // Journal of Magnetism and Magnetic Materials. 1992. Vol. 103. P. 117. DOI: 10.1016/0304-8853(92)90244-I.
- Zhukov V., Zhukova A., Blancoc J.M., Cobeno A.F., Vazquez M., Gonzalez J. Magnetostriction of Co-Fe-Based Amorphous Soft Magnetic Microwires // Journal of Magnetism and Magnetic Materials. 2003. Vol. 151. P. 258–259. DOI: 10.1007/978-3-319-48220-0_29.
- Gudoshnikov S.A., Grebenshchikov Yu.B., Ljubimov B.Ya. et al. Ground state magnetization distribution and characteristic width of head to head domain wall in Fe-rich amorphous microwire // Physica Status Solidi A. 2009. Vol. 206. No. 4. P. 613.
- Ye J., del Real R.P., Infante G., Vazquez M. Local magnetization profile and geometry magnetization effects in microwires as determined by magneto-optical Kerr effect // Journal of Applied Physics. 2013. Vol. 113. P. 043904. DOI: 10.1063/1.4776730.
- Varga R., Klein P., Jimenez A., Vazquez M. Study of the single domain-wall structure in glass-coated microwires // Physica Status Solidi A. 2015. Vol. 213. Issue 2. P. 356–362.
- Sampaio L.C., Sinnecker E., Cernicchiaro G. et al. Magnetic microwires as macrospins in a long-range dipole-dipole interaction // Physical Review B. 2000. Vol. 61. P. 8976.
- Korolev D.V., Rezchikova I.I., Piskorskij V.P., Valeev R.A., Morgunov R.B. Metod goryachej deformatsii dlya izgotovleniya postoyannykh magnitov sistemy RZM–Fe–B s ispolzovaniem ustanovok iskrovogo plazmennogo spekaniya (obzor) [The method of hot deformation for the manufacture of the permanent magnets of REM–Fe–B by the spark plasma sintering (review)] // Aviacionnye materialy i tehnologii. 2017. №4 (49). S. 11–18. DOI: 10.18577/2071-9140-2017-0-4-11-18.