Quantum chemical calculation of intermolecular interaction methylsilane molecules during the pyrolysis process
Sidorov D.V., Shavnev A.A., Solodkin P.V., Kirilin A.D. Quantum chemical calculation of intermolecular interaction methylsilane molecules during the pyrolysis process // Proceedings of VIAM. 2019. No. 11. DOI: 10.18577/2307-6046-2019-0-11-44-52. URL: https://www.viam-works.ru/en/journal/2019/11/5
Keywords
methylsilane, quantum chemical calculation, molecular structure, thermodynamic parameter.
Abstract
The article describes theoretical investigation for produce more favorable chemical structure from two molecules methylsilane during the pyrolysis process. In this investigation, we used quantum chemical calculation by second order Moller–Plesset perturbation theory with 6-311+G (d) basis set. It was used for chemical structure geometry optimization, computation thermodynamic data and estimate intermolecular interaction energies of chemical reactions. The calculated results showed that reaction with produce methyl(sililmethyl)silane are more favorable in case of the intermolecular interaction.
Reference list
- Kablov E.N. Innovacionnye razrabotki FGUP «VIAM» GNC RF po realizacii «Strategicheskih napravlenij razvitiya materialov i tehnologij ih pererabotki na period do 2030 goda» [Innovative developments of FSUE «VIAM» SSC of RF on realization of «Strategic directions of the development of materials and technologies of their processing for the period until 2030»] // Aviacionnye materialy i tehnologii. 2015. №1 (34). S. 3–33. DOI: 10.18577/2071-9140-2015-0-1-3-33.
- Kablov E.N. Materialy novogo pokoleniya – osnova innovatsiy, tekhnologicheskogo liderstva i natsionalnoy bezopasnosti Rossii [Materials of a new generation – the basis of innovation, technological leadership and national security of Russia] // Intellekt i tekhnologii. 2016. №2 (14). S. 16–21.
- Grashchenkov D.V. Strategiya razvitiya nemetallicheskih materialov, metallicheskih kompozicionnyh materialov i teplozashhity [Strategy of development of non-metallic materials, metal composite materials and heat-shielding] // Aviacionnye materialy i tehnologii. 2017. №S. S. 264–271. DOI: 10.18577/2071-9140-2017-0-S-264-271.
- Kablov E.N. VIAM: materialy novogo pokoleniya dlya PD-14 [VIAM: new generation materials for PD-14] // Krylya Rodiny. 2019. №7–8. S. 54–58.
- Sidorov D.V., Serpova V.M., Shavnev A.A. Vzaimodeystviye titanovykh splavov i volokon karbida kremniya v metallicheskikh kompozitsionnykh materialakh sistemy Ti–SiCf [Interaction of titanium alloys and silicon carbide fibers in metal composite materials of the Ti – SiCf system] // Khimicheskaya tekhnologiya. 2018. T. 19. №8. S. 339–344.
- Sidorov D.V., Serpova V.M., Shavnev A.A. Sposoby izgotovleniya i oblasti primeneniya vysokoprochnykh voloknistykh kompozitsionnykh materialov, armirovannykh kernovym voloknom karbida kremniya [Methods of manufacture and scope of high-strength fibrous composite materials reinforced with silicon carbide core fiber] // Vse materialy. Entsiklopedicheskiy spravochnik. 2018. №3. S. 15–22.
- Evdokimov S.A., Shchegoleva N.E., Sorokin O.Yu. Keramicheskiye materialy v aviatsionnom dvigatelestroyenii (obzor) [Ceramic materials in aviation engineering (review)] // Trudy VIAM: elektron. nauch.-tehnich. zhurn. 2018. №12 (72). St. 06. Available at: http://www.viam-works.ru (accessed: September 05, 2019). DOI: 10.18577/2307-6046-2018-0-12-54-61.
- Johnson D.W., Evans A.G., Goettler R.W. Ceramic Fibers and Coatings: Advanced Materials for the Twenty-First Century. Committee on advanced fibers for high-temperature ceramic composites. Washington DC: Nat. Acad. Press, 1998. 112 p.
- Sidorov D.V., Storozhenko P.A., Shutova O.G., Kozhevnikov B.E. Polucheniye alkilsilanov vysokoy chistoty [Obtaining high purity alkylsilanes] // Khimicheskaya tekhnologiya. 2006. №7. S. 22–24.
- Ohshita Y. Reactants in SiC chemical vapor deposition using CH3SiH3 as a source gas [Reactants in SiC chemical vapor deposition using CH3SiH3 as a source gas] // Journal of Crystal Growth. 1995. Vol. 147. P. 111–116.
- Minkin V.I., Simkin B.Ya., Minyayev R.M. Teoriya stroyeniya molekul [Theory of the structure of molecules]. Rostov n/D: Feniks, 1997. 560 s.
- Gordon M., Truong T. Potential primary pyrolysis processes of methylsilane // Chemical Physics Letters. 1987. Vol. 142. P. 110–114.
- Truong T., Gordon M., Pople J. Thermal decomposition pathways of ethane // Chemical Physics Letters. 1986. Vol. 130. P. 245–249.
- Gordon M., Truong T., Bonderson E. Potential Primary Pyrolysis Processes for Disilane // Journal of the American Chemical Society. 1986. Vol. 108. P. 1421–1427.
- Becerra R., Carpenter I., Gordon M. Gas phase kinetic and quantum chemical studies of the reaction of silylene with the methylsilanes. Absolute rate constants, temperature dependences, RRKM modeling and potential energy surfaces // Physical Chemistry Chemical Physics. 2007. Vol. 9. P. 2121–2129.
- Gano R., Gordon M., Boatz J. Ab initio study of some methylene and silylene insertion reactions // Journal of the American Chemical Society. 1991. Vol. 113. P. 6711–6718.
- Abyzov A.M., Smirnov E.P. Kinetika khimicheskogo osazhdeniya karbida kremniya iz gazovoy fazy metilsilana [Kinetics of the chemical deposition of silicon carbide from the gas phase of methylsilane] // Neorganicheskiye materialy. 2000. T. 36. №9. S. 1059–1066.
- Lakhin A.V. Protsessy polucheniya kompozitsionnykh materialov i pokrytiy na osnove karbida kremniya khimicheskim gazofaznym osazhdeniyem iz metilsilana pri otnositelno nizkikh temperaturakh i davleniyakh: avtoref. dis. … kand. tekhn. nauk [Processes for producing composite materials and coatings based on silicon carbide by chemical vapor deposition from methylsilane at relatively low temperatures and pressures: thesis Cand. Sc. (Tech.)]. M., 2006. 25 s.
- Prokofev V.A., Sorokin O.Yu., Vaganova M.L., Lebedeva Yu.E. Vysokotemperaturnyy material s gradiyentnoy strukturoy, poluchennyy metodom zhidkofaznoy infiltratsii rasplava [High-temperature functionally graded material fabricated via reactive alloy infiltration] // Trudy VIAM: elektron. nauch.-tehnich. zhurn. 2018. №11 (71). St. 06. URL: http://www.viam-works.ru. (accessed: October 01, 2019). DOI: 10.18577/2307-6046-2018-0-11-45-53.
- Gaussian-09: revision A.02 / Frisch M.J., Trucks G.W., Schlegel H.B. et al. Wallingford, CT: Gaussian Inc., 2009.