Spheroplastic with adjustable viscosity for filling sections of honeycomb structures

Kovalenko A.V., Sidelnikov N.K., Sokolov I.I., Tundaykin K.O.
Kovalenko A.V., Sidelnikov N.K., Sokolov I.I., Tundaykin K.O. Spheroplastic with adjustable viscosity for filling sections of honeycomb structures // Proceedings of VIAM. 2019. No. 11. DOI: 10.18577/2307-6046-2019-0-11-37-43. URL: https://www.viam-works.ru/en/journal/2019/11/4
Keywords
spheroplastic, polymer fill, PCM, honeycomb fill, adjustable viscosity, honeycomb structures.
Abstract

Studies have been conducted to obtain a filler-spheroplastic with adjustable viscosity for filling areas of multilayer honeycomb structures based on an epoxy oligomer, compatible with the chemical nature and processing modes of cladding materials made of polymer composite materials. The rheological characteristics of polymer bases spheroplastic depending on the content of the modifying additives – toluylendiisocyanate. The influence of the content and characteristics of dispersed fillers on the rheological and physico-mechanical properties of spheroplastic was established. It is shown that the developed materials correspond.

Reference list
  1. Kablov E.N. Kompozity: segodnya i zavtra [Composites: today and tomorrow] // Metally Evrazii. 2015. №1. S. 36–39.
  2. Kablov E.N. Iz chego sdelat budushcheye? Materialy novogo pokoleniya, tekhnologii ikh sozdaniya i pererabotki – osnova innovatsiy [What to make the future of? Materials of a new generation, technologies for their creation and processing – the basis of innovation] // Krylya Rodiny. 2016. №5. S. 8–18.
  3. Kablov E.N. Innovacionnye razrabotki FGUP «VIAM» GNC RF po realizacii «Strategicheskih napravlenij razvitiya materialov i tehnologij ih pererabotki na period do 2030 goda» [Innovative developments of FSUE «VIAM» SSC of RF on realization of «Strategic directions of the development of materials and technologies of their processing for the period until 2030»] // Aviacionnye materialy i tehnologii. 2015. №1 (34). S. 3–33. DOI: 10.18577/2071-9140-2015-0-1-3-33.
  4. Kablov E.N. Materialy – osnova lyubogo dela [Materials are the basis of any business] // Delovaya slava Rossii. 2013. №2. S. 4–9.
  5. Kostyukov V.I. Primeneniye konstruktsionnykh plastmass v proizvodstve letatelnykh apparatov [The use of structural plastics in the manufacture of aircraft]. M.: Mashinostroyeniye, 1971. S. 192–196.
  6. Zakharov A.G., Anoshkin A.N., Kop'v V.F. Issledovaniye novykh vidov zapolniteley iz polimernykh kompozitsionnykh materialov dlya mnogosloynykh zvukopogloshchayushchikh konstruktsiy [The study of new types of aggregates made of polymer composite materials for multilayer sound-absorbing structures] // Vestnik Permskogo natsionalnogo issledovatelskogo politekhnicheskogo universiteta. Ser.: Aerokosmicheskaya tekhnika. 2017. №51. S. 95–103.
  7. Kostyukov V.I. Stekloplastiki na osnove kapillyarnykh steklyannykh volokon i mikrosfer [Fiberglass based on capillary glass fibers and microspheres] // Aviatsionnyye materialy na rubezhe XX–XXI vekov. M.: VIAM, 1994. S. 197–203.
  8. Pavlyuk B.Ph. Osnovnye napravleniya v oblasti razrabotki polimernyh funktsionalnyh materialov [The main directions in the field of development of polymeric functional materials] // Aviacionnye materialy i tehnologii. 2017. №S. S. 388–392. DOI: 10.18577/2071-9140-2017-0-S-388-392.
  9. Petrova A.P., Mukhametov R.R., Shishimirov M.V., Pavlyuk B.Ph., Starostina I.V. Metody ispytaniy i issledovaniy termoreaktivnykh svyazuyushchikh dlya polimernykh kompozitsionnykh materialov (obzor) [Test methods and researches thermosetting binding for polymeric composite materials (review)] // Trudy VIAM: elektron. nauch.-tekhnich. zhurnal. 2018. №12 (72). St. 07. Available at: http://viam-works.ru (accessed: March 25, 2019). DOI: 10.18577/2307-6046-2018-0-12-62-70.
  10. Sokolov I.I. Sferoplastiki na osnove termoreaktivnykh svyazuyushchikh dlya izdeliy aviatsionnoy tekhniki: dis. …kand. tekhn. nauk [Spheroplastics based on thermosetting binders for aircraft products: thesis, Cand. Sc. (Tech.)]. M., 2013. 127 s.
  11. Kirillov V.N., Vapirov Yu.M., Drozd E.A. Issledovanie atmosfernoj stojkosti polimernyh kompozicionnyh materialov v usloviyah atmosfery teplogo vlazhnogo i umerenno teplogo klimata [Research of atmospheric firmness of polymeric composite materials in the conditions of the atmosphere of warm wet and moderately warm climate] // Aviacionnye materialy i tehnologii. 2012. №4. S. 31–38.
  12. Sokolov I.I., Minakov V.T. Sferoplastiki aviatsionnogo naznacheniya na osnove epoksidnykh kleyev i dispersnykh napolniteley [Spheroplastics for aviation purposes based on epoxy adhesives and dispersed fillers] // Klei. Germetiki. Tekhnologii. 2012. №5. S. 22–26.
  13. Sokolov I.I., Kogan D.I., Raskutin A.E., Babin A.N., Filatov A.A., Morozov B.B. Mnogosloynyye konstruktsii so sferoplastikom dlya izdeliy aviatsionnoy tekhniki [Multilayer structures with spheroplastics for aircraft products] // Konstruktsii iz kompozitsionnykh materialov. 2014. №1 (133). S. 37–42.
  14. Berlin A.A., Shutov F.A. Uprochnennyye gazonapolnennyye plastmassy. Sintaktnye penoplasty [Hardened gas-filled plastics. Syntactic foams]. M.: Khimiya, 1980. S. 158–215.
  15. Panin V.F., Gladkikh Yu.A. Konstruktsii s zapolnitelem: spravochnik [Constructions with a placeholder: reference]. M.: Mashinostroyeniye, 1991. 272 s.
  16. Kutsevich K.E., Tyumeneva T.Yu., Petrova A.P. Vliyaniye napolniteley na svoystva kleyevykh prepregov i PKM na ikh osnove [Influence of fillers on properties of adhesive prepregs and PCM on their basis] // Aviacionnye materialy i tehnologii. 2017. №4 (49). S. 51–55. DOI: 10.18577/2071-9140-2017-0-4-51-55.
  17. Simonov-Emelyanov I.D., Trofimov A.N., Sokolov V.I., Zarubina A.Yu., Sinegayeva S.I., Trofimov D.A. Obobshchennyye parametry struktury i reologicheskiye svoystva dispersno-napolnennykh epoksidnykh oligomerov s inaktivnym rastvoritelem [Generalized structural parameters and rheological properties of dispersively-filled epoxy oligomers with an inactive solvent] // Klei. Germetiki. Tekhnologii. 2018. №5. S. 11–17.
  18. Petrova A.P., Malysheva G.V. Klei, kleyevyye svyazuyushchiye i kleyevyye prepregi / pod red. E.N. Kablova. [Glues, adhesive binders and adhesive prepregs / ed. E.N. Kablov] M.: VIAM, 2017. 472 s.