Investigation of the influence of the reinforcement scheme on the combustibility characteristics of carbon fiber reinforced polymer material

Barbotko S.L., Volnyj O.S., Marachovskiy P.C.
Barbotko S.L., Volnyj O.S., Marachovskiy P.C. Investigation of the influence of the reinforcement scheme on the combustibility characteristics of carbon fiber reinforced polymer material // Proceedings of VIAM. 2019. No. 10. DOI: 10.18577/2307-6046-2019-0-10-103-110. URL: https://www.viam-works.ru/en/journal/2019/10/10
Keywords
polymeric composite material, carbon reinforced polymeric material, fire safety, flammability, scheme of laying, reinforcement structure.
Abstract

The influence of the structure of carbon fiber reinforced plastic VKU-25/SYT49S based on the binder VSE-1212 and high-strength carbon harness SYT49S on the flammability characteristics determined in accordance with the requirements of aviation regulations. The significant effect of the scheme of reinforcement on the value of the residual duration of combustion and the length of the burn-out. It is established that in the entire range of the studied material thicknesses (from 1 to 4 mm) the samples of unidirectional material with the orientation of the carbon filler [0] have significantly worse fire safety values compared to the samples with the orientation [90] or with an equally strong material (quasi-isotropic laying).

Reference list
  1. Destefany J. Hole in Four … or More // Cutting Tool Engineering. January 2011. P. 34–40.
  2. Gründer M. Immer mehr Kunststoffe // Flug Revue. 2009. Juni. P. 93–95.
  3. Lyon R.E. Nongalogen Fire-Resistant Plastics for Aircraft Interiors // Technical Report DOT/FAA/AR TN08/5. 2008. 33 p.
  4. Gründer M. Kunststoff oder Metall? // Flug Revue. 2011. September. P. 74–77.
  5. Raskutin A.E. Rossiiskie polimernye kompozitsionnye materialy novogo pokoleniia, ikh osvoenie i vnedrenie v perspektivnykh razrabatyvaemykh konstruktsiiakh [Russian polymer composite materials of new generation, their exploitation and implementation in advanced developed constructions] // Aviacionnye materialy i tehnologii. 2017. №S. S. 349–367. DOI: 10.18577/2071-9140-2017-0-S-349-367.
  6. Kutsevich K.E., Dementeva L.A., Lukina N.F., Tyumeneva T.Yu. Kleyevyye prepregi – perspektivnyye materialy dlya detaley i agregatov iz PKM [Adhesive prepregs as promising materials for parts and assemblies from polymeric composite materials] // Aviacionnye materialy i tehnologii. 2017. №S. S. 379–387. DOI: 10.18577/2071-9140-2017-0-S-379-387.
  7. Kondrashov S.V., Shashkeev K.A., Petrova G.N., Mekalina I.V. Polimernye kompozicionnye materialy konstrukcionnogo naznacheniya s funkcionalnymi svojstvami [Constructional polymer composites with functional properties] // Aviacionnye materialy i tehnologii. 2017. №S. S. 405–419. DOI: 10.18577/2071-9140-2017-0-S-405-419.
  8. Giordano G. Plastics in Defense & Safety // Plastics Engineering. 2011. October. P. 28–31.
  9. Decadal Survey of Civil Aeronautics: Foundation for the Future / Steering Committee for the Decadal Survey of Civil Aeronautics, National Research Council of the National Academies. Washington, D.C.: The National Academies Press, 2006. 212 p.
  10. Sarkos G. Evolution of FAA Fire Safety R&D Over the Years: report of the Fifth Triennial Fire & Cabin Safety Research Conference (Atlantic City, Oct. 29 – Nov. 01, 2007). 2007. 56 p. Available at: http://www.fire.tc.faa.gov (accessed: September 30, 2019).
  11. Sarkos G. Aircraft fire Safety R&D: Past, Present & Future: report of the 6th Triennial Fire & Cabin Safety Research Conference. (Atlantic City, Oct. 25–28, 2010). 2010. 26 p. Available at: http://www.fire.tc.faa.gov (accessed: September 30, 2019).
  12. Barbotko S.L. Pozharobezopasnost polimernykh materialov aviatsionnogo naznacheniya i konstruktivnykh elementov na ikh osnove: avtoref. dis. … d-ra tekhn. nauk [Fire safety of polymer materials for aviation purposes and structural elements based on them: thesis, Dr. Sc. (Tech.)]. M.: VIAM, 2019. 47 s.
  13. Terebnev V.V., Artem'yev N.S., Grachev V.A. Transport: nazemnyy, morskoy, rechnoy, vozdushnyy, metro. Protivopozharnaya zashchita i tusheniye pozharov [Transport: land, sea, river, air, metro. Fire protection and extinguishing fires]. M.: Pozhnauka, 2007. Kn. 6. 383 s.
  14. Dzhafarov M.A., Lozovoy N.F., Lutsenko V.I., Fedorov V.K. Obespecheniye pozharnoy bezopasnosti na aerodromakh grazhdanskoy aviatsii [Ensuring fire safety at aerodromes of civil aviation]. M.: Transport, 1987. 263 s.
  15. Webster H. Fuselage Burnthrough from Large Exterior Fuel Fires // Technical Report DOT/FAA/CT-90-10. 1994. 114 p.
  16. Predvaritelny otchet po rezultatam rassledovaniya aviatsionnogo proisshestviya samoleta RRJ-95B RA-89098 / Mezhgosudarstvennyy aviatsionnyy komitet. Komissiya po rassledovaniyu aviatsionnykh proisshestviy [Preliminary report on the results of the investigation of the accident RRJ-95B RA-89098 / Interstate Aviation Committee. Accident Investigation Commission]. Available at: http://www.mak-iac.org (accessed: June 20, 2019).
  17. Marker T.R. Shot Takes and Current Projects // International Aircraft Materials Fire Test Forum Meeting (Cologne, Germany. June 18, 2019). Available at: http://www.fire.tc.faa.gov (accessed: September 13, 2019).
  18. Marker T.R. Full-Scale Test Evaluation of Aircraft Fuel Fire Burnthrough Resistance Improvements // Technical Report DOT/FAA/AR-98/52. US. 1999. 41 p.
  19. Marker T.R., Speitel L.C. Evaluating the Decomposition Products Generated Inside an Intact Fuselage During a Simulated Postcrash Fuel Fire: Report DOT/FAA/AR-09/58. U.S. Department of Transportation FAA, 2011. 86 p.
  20. Barbotko S.L., Volnyy O.S., Kiriyenko O.A., Shurkova E.N. Postroyeniye matematicheskoy modeli i raschet temperatur obraztsov pri ispytaniyakh na ognestoykost [Creation of the mathematical model and calculation of sample temperatures at tests on fire resistance] // Trudy VIAM: elektron. nauch.-tekhnich. zhurn. 2017. №7 (55). St. 12. Available at: http://www.viam-works.ru (accessed: May 01, 2019). DOI: 10.18577/2307-6046-2017-0-7-12-12.
  21. Barbotko S.L., Volny O.S., Veshkin E.A., Goncharov V.A. Otsenka ognestoykosti materialov i konstruktivnykh elementov dlya aviatsionnoy tekhniki [Assessment of fire resistance of materials and structural elements for aircraft] // Aviatsionnaya promyshlennost. 2018. №2. S. 63–67.
  22. Barbotko S.L., Volnyy O.S., Kiriyenko O.A., Shurkova E.N. Otsenka pozharobezopasnosti polimernykh materialov aviatsionnogo naznacheniya: analiz sostoyaniya, metody ispytaniy, perspektivy razvitiya, metodicheskiye osobennosti / pod obshch. red. E.N. Kablova [Fire safety assessment of aviation polymer materials: state analysis, test methods, development prospects, methodological features / gen. ed. E.N. Kablov]. M.: VIAM, 2018. 424 s.
  23. Rehn S. Vertical Bunsen Burner Testing of 3D-Printed Material // International Aircraft Materials Fire Test Forum Meeting (Cologne, Germany. June 18, 2019). Available at: http://www.fire.tc.faa.gov (accessed: September 13, 2019).
  24. Green M. CHM014M – Flame Retardant Chemicals: Technologies and Global Markets. BCC Research, 2015. 164 p.
  25. Polymer Green Flame Retardants / ed. C.D. Papaspyrides, P. Kiliaris. Elsevier, 2014. 943 p.
  26. Lyon R.E., Gandhi S., Crowley S. Fire Properties of Heat-Resistant Polymers: Report DOT/FAA/TC-TN18/32. U.S. Department of Transportation FAA, 2019. 33 p.
  27. Barbotko S.L., Volnyj O.S., Postnov V.I., Shurkova E.N. Issledovaniye vliyaniya struktury armirovaniya na kharakteristiki pozharnoy opasnosti stekloplastika [Investigation of the effect of reinforcement structures on fire hazard characteristics of the fiberglass] // Trudy VIAM: elektron. nauch.-tekhnich. zhurn. 2019. №4 (76). St. 12. Available at: http://www.viam-works.ru (accessed: June 18, 2019). DOI: 10.18577/2307-6046-2019-0-4-108-120.
  28. Kablov E.N. Innovacionnye razrabotki FGUP «VIAM» GNC RF po realizacii «Strategicheskih napravlenij razvitiya materialov i tehnologij ih pererabotki na period do 2030 goda» [Innovative developments of FSUE «VIAM» SSC of RF on realization of «Strategic directions of the development of materials and technologies of their processing for the period until 2030»] // Aviacionnye materialy i tehnologii. 2015. №1 (34). S. 3–33. DOI: 10.18577/2071-9140-2015-0-1-3-33.
  29. Kablov E.N. Na perekrestke nauki, obrazovaniya i promyshlennosti [At the crossroads of science, education and industry] // Ekspert. 2015. №15 (941). S. 49–53.
  30. Kablov E.N. Iz chego sdelat' budushcheye? Materialy novogo pokoleniya, tekhnologii ikh sozdaniya i pererabotki – osnova innovatsiy [What to make the future of? Materials of a new generation, technologies for their creation and processing - the basis of innovation] // Krylya Rodiny. 2016. №5. S. 8–18.
  31. Platonov A.A., Dushin M.I. Konstrukcionnyj ugleplastik VKU-25 na osnove odnonapravlennogo preprega [Carbon composites VKU-25 based on unidirectional prepregs] // Trudy VIAM: elektron. nauch.-tehnich. zhurn. 2015. №11. St. 06. Available at: http://www.viam-works.ru (accessed: August 19, 2019). DOI: 10.18577/2307-6046-2015-0-11-6-6.
  32. Normy letnoy godnosti samoletov transportnoy kategorii: AP-25 [Airworthiness standards for transport category aircraft: AP-25]: utv. Postanovleniyem 35-y sessii Soveta po aviatsii i ispolzovaniyu vozdushnogo prostranstva 23.10.2015. 5-e izd. s popravkami 1–8. M.: Aviaizdat, 2015. 290 s.
  33. Horner A. Aircraft Materials Fire Test Handbook: Report DOT/FAA/AR-00/12. U.S. Department of Transportation, Federal Aviation Administration, 2012. 235 p.
  34. Certification Specifications and Acceptable Means of Compliance for Large Aeroplanes. CS-25. Amendment 15. July 21, 2014. 921 p.
  35. Federal Regulations. Part 25 – Airworthiness Standards: Transport Category Airplanes. Available at: http://www.ecfr.gov (accessed: June 21, 2019 ).