Research of influence of technological modes of production of epoxy nanocomposites with carbon nanotubes on their heat resistance

Zagora A.G., Kondrashov S.V., Antyufeeva N.V., Pykhtin A.A.
Zagora A.G., Kondrashov S.V., Antyufeeva N.V., Pykhtin A.A. Research of influence of technological modes of production of epoxy nanocomposites with carbon nanotubes on their heat resistance // Proceedings of VIAM. 2019. No. 1. DOI: 10.18577/2307-6046-2019-0-1-64-73. URL: https://www.viam-works.ru/en/journal/2019/1/8
Keywords
epoxy oligomer, epoxynanocomposite, thermal analysis, three-roll mixer.
Abstract

In work the temperature and time mode of hardening of the studied epoxy compositions which provided its almost full course was chosen. Therefore, temperature change of vitrification as a result of the conducted researches is explained by exclusively modifying action of carbon nanotubes. It is shown that the three-roll mixer plays a key role in the technological modes of production of epoxynanocomposites. Non-functional multiwall carbon nanotubes (MWCNTs) with its help considerably increase heat resistance of epoxy compositions.

Reference list
  1. Kablov E.N. Rol khimii v sozdanii materialov novogo pokoleniya dlya slozhnykh tekhnicheskikh sistem [The role of chemistry in the creation of a new generation of materials for complex technical systems] // Tez. dokl. XX Mendeleyevskogo syezda po obshchey i prikladnoy khimii. UrO RAN, 2016. S. 25–26.
  2. Kablov E.N. Innovacionnye razrabotki FGUP «VIAM» GNC RF po realizacii «Strategicheskih napravlenij razvitiya materialov i tehnologij ih pererabotki na period do 2030 goda» [Innovative developments of FSUE «VIAM» SSC of RF on realization of «Strategic directions of the development of materials and technologies of their processing for the period until 2030»] // Aviacionnye materialy i tehnologii. 2015. №1 (34). S. 3–33. DOI: 10.18577/2071-9140-2015-0-1-3-33.
  3. Kablov E.N. Kompozity: segodnya i zavtra [Composites: today and tomorrow] // Metally Evrazii. 2015. №1. S. 36–39.
  4. Pavlyuk B.F. Osnovnye napravleniya v oblasti razrabotki polimernyh funktsionalnyh materialov [The main directions in the field of development of polymeric functional materials] // Aviatsionnye materialy i tekhnologii. 2017. №S. S. 388–392. DOI: 10.18577/2071-9140-2017-0-S-388-392.
  5. Mukhametov R.R., Petrova A.P. Svoystva epoksidnykh polimernykh svyazuyushchikh i ikh pererabotka v polimernyye kompozitsionnyye materialy [Properties of epoxy binders and their processing in polymers composition materials] // Novosti materialovedeniya. Nauka i tekhnika: elektron. nauch.-tekhnich. zhurn. 2018. №3–4. St. 06. Available at: http://materialsnews.ru (accessed: December 04, 2018).
  6. Timoshkov P.N., Kogan D.I. Sovremennye tehnologii proizvodstva polimernyh kompozicionnyh materialov novogo pokoleniya [Modern production technologies of polymeric composite materials of new generation] // Trudy VIAM: elektron. nauch.-tehnich. zhurn. 2013. №4. St. 07. Available at: http://www.viam-works.ru (accessed: December 04, 2018).
  7. Kablov E.N., Kondrashov S.V., Yurkov G.Yu. Perspektivy ispolzovaniya uglerodsoderzhashchikh nanochastits v svyazuyushchikh dlya polimernykh kompozitsionnykh materialov [Prospects for the use of carbon-containing nanoparticles in binders for polymer composite materials] // Rossiyskiye nanotekhnologii. 2013. T. 8. №3–4. S. 24–42.
  8. Simonov-Yemelyanov I.D., Pykhtin A.A., Smotrova S.A., Kovaleva A.N. Strukturoobrazovaniye i fiziko-mekhanicheskiye kharakteristiki epoksidnykh nanokompozitov [Structure formation and physico-mechanical characteristics of epoxy nanocomposites] // Vse materialy. Entsiklopedicheskiy spravochnik. 2017. №2. S. 2–7.
  9. Bolshakov V.A., Solodilov V.I., Korokhin R.A., Kondrashov S.V., Merkulova Yu.I., Dyachkova T.P. Issledovaniye treshchinostoykosti polimernykh kompozitsionnykh materialov, izgotovlennykh metodom infuzii s ispolzovaniyem razlichnykh kontsentratov na osnove modifitsirovannykh UNT [Research of crack resistance of polymeric composite materials fabricated by infusion using various concentrates on the basis of modified CNT] // Trudy VIAM: elektron. nauch.-tehnich. zhurn. 2017. №7 (55). St. 09. Available at: http://www.viam-works.ru (accessed: December 04, 2018). DOI: 10.18577/2307-6046-2017-0-7-9-9.
  10. Gunyayev G.M., Kablov E.N., Aleksashin V.M. Modifitsirovaniye konstruktsionnykh ugleplastikov uglerodnymi nanochastitsami [Modification of structural carbon plastics with carbon nanoparticles] // Rossiyskiy khimicheskiy zhurnal. 2010. T. LIV. №1. S. 3–11.
  11. Thakre P.R., Bisrat Y., Lagoudas D.C. Electrical and mechanical properties of carbon nanotube‐epoxy nanocomposites // Journal of Applied Polymer Science. 2010. Vol. 116. No. 1. P. 191–202.
  12. Zhou Y.X., Wu P.X., Cheng Z.-Y. et al. Improvement in electrical, thermal and mechanical properties of epoxy by filling carbon nanotube // Express Polymer Letters. 2008. Vol. 2. No. 1. P. 40–48.
  13. Hernag̀ndez-Peg̀rez A., Avileg̀s F., May-Pat A. Effective properties of multiwalled carbon nanotube/epoxy composites using two different tubes // Composites Science and Technology. 2008. Vol. 68. P. 1422–1431.
  14. Wang Sh., Liang R., Wang B., Zhang Ch. Covalent Addition of Diethyltoluenediamines Onto Carbon Nanotubes for Composite Application // Polymer Composites. 2009. Vol. 30 (8). DOI: 10.1002/pc.20654.
  15. Wang Sh., Liang Z., Liu T. et al. Effective amino-functionalization of carbon nanotubes for reinforcing epoxy polymer composites // Nanotechnology. 2006. Vol. 17. Р. 1551–1557.
  16. Shen J., Huang W., Wu L. et al. The reinforcement role of different amino-functionalized multi-walled carbon nanotubes in epoxy nanocomposites // Composites Science and Technology. 2007. Vol. 67. Р. 3041–3050.
  17. Allaoui A., Bounia N.El. How carbon nanotubes affect the cure kinetics and glass transition temperature of their epoxy composites?: a review // Express Polymer Letters. 2009. Vol. 3. No. 9. Р. 588–594.
  18. Marakhovskiy P.S., Kondrashov S.V., Akatenkov R.V., Aleksashin V.M., Anoshkin I.V., Mansurova I.A. O modifikatsii teplostoykikh epoksidnykh svyazuyushchikh uglerodnymi nanotrubkami // Vestnik MGTU im. N.E. Baumana. Ser.: Mashinostroyeniye. 2015. №2. S. 118–127.
  19. Ma P.-C., Naveed A., Marom G. et al. Dispersion and functionalization of carbon nanotubes for polymer-based nanocomposites // Composites Part A: Applied Science and Manufacturing. 2010. Vol. 41. No. 10. P. 1345–1367.
  20. Sandler J., Shaffer M., Prasse T. et al. Development of a dispersion process for carbon nanotubes in an epoxy matrix and the resulting electrical properties // Polymer. 1999. Vol. 40. No. 21. P. 5967–5971.
  21. Gojny F., Wichmann M., Kopke U. et al. Carbon nanotube reinforced epoxy-composites: enhanced stiffness and fracture toughness at low nanotube content // Composites science and technology. 2004. Vol. 64. No. 15. P. 2363–2371.
  22. Thostenson E.T., Chou T.W. Processing-structure-multi-functional property relationship in carbon nanotube/epoxy composites // Carbon. 2006. Vol. 44. No. 14. P. 3022–3029.
  23. Li Y., Shimizu H. High-shear melt processing of polymer–carbon nanotube composites // Polymer–Carbon Nanotube Composites. 2011. No. 5. P. 133–154.
  24. Puglia D., Valentini L., Kenny J.M. Analysis of the Cure Reaction of Carbon Nanotubes/Epoxy Resin Composites Through Thermal Analysis and Raman Spectroscopy // Journal of Applied Polymer Science. 2003. Vol. 88. P. 452–458.
  25. Valentini L., Armentano I., Puglia D., Kenny J.M. Dynamics of amine functionalized nanotubes/epoxy composites by dielectric relaxation spectroscopy // Carbon. 2004. Vol. 42. P. 323–329.
  26. Bae J., Jang J., Yoon S.-H. Cure Behavior of the Liquid-Crystalline Epoxy/Carbon Nanotube System and the Effect of Surface Treatment of Carbon Fillers on Cure Reaction // Macromolecular Chemistry Physics. 2002. Vol. 203. P. 2196–2204.
  27. Pykhtin A.A. Vysokotekhnologichnyye epoksidnyye nanodispersii i nanokompozity s reguliruyemoy strukturoy i kompleksom svoystv: dis. … kand. tekhn. nauk [High-tech epoxy nanodispersions and nanocomposites with adjustable structure and complex properties: thesis Dr. Sc. (Tech.)]. M., 2017. 125 c.