Determination of oxygen and nitrogen in nickel alloy powders

Alekseev A.V., Rastegayeva G.Yu., Pahomkina T.N.
Alekseev A.V., Rastegayeva G.Yu., Pahomkina T.N. Determination of oxygen and nitrogen in nickel alloy powders // Proceedings of VIAM. 2018. No. 8. DOI: 10.18577/2307-6046-2018-0-8-112-119. URL: https://www.viam-works.ru/en/journal/2018/8/11
Keywords
powder metallurgy, nickel alloys, determination of oxygen, determination of nitrogen, method of infrared absorption spectroscopy, melting method in a current of an inert carrier gas.
Abstract

In this work, the determination of the oxygen and nitrogen content in powders of nickel alloys EP648, VPr50 and VG159 was carried out by reductive melting in a current of an inert carrier gas, followed by detection of oxygen in an infrared cell and nitrogen in a conductometric cell of a Leco TC-600 gas analyzer. During the experiments, various catalysts were used – tin and nickel, necessary for the complete extraction of oxygen and nitrogen from nickel alloy powders. Preparation of a sample for analysis is described.

Reference list
  1. Kablov E.N. Innovacionnye razrabotki FGUP «VIAM» GNC RF po realizacii «Strategicheskih napravlenij razvitiya materialov i tehnologij ih pererabotki na period do 2030 goda» [Innovative developments of FSUE «VIAM» SSC of RF on realization of «Strategic directions of the development of materials and technologies of their processing for the period until 2030»] // Aviacionnye materialy i tehnologii. 2015. №1 (34). S. 3–33. DOI: 10.18577/2071-9140-2015-0-1-3-33.
  2. Kablov E.N. Strategicheskie napravleniya razvitiya materialov i tehnologij ih pererabotki na period do 2030 goda [The strategic directions of development of materials and technologies of their processing for the period to 2030] // Aviacionnye materialy i tehnologii. 2012. №S. S. 7–17.
  3. Ospennikova O.G. Strategiya razvitiya zharoprochnyh splavov i stalej specialnogo naznacheniya, zashhitnyh i teplozashhitnyh pokrytij [Strategy of development of hot strength alloys and steels special purpose, protective and heat-protective coverings] // Aviacionnye materialy i tehnologii. 2012. №S. S. 19–36.
  4. Rodionov A.I., Efimochkin I.Ju., Bujakina A.A., Letnikov M.N. Sferoidizacija metallicheskih po-roshkov (obzor) [Sphereidizatsiya of metal powders (review)] // Aviacionnye materialy i tehnologii. 2016. №S1 (43). S. 60–64. DOI: 10.18577/2071-9140-2016-0-S1-60-64.
  5. Evgenov A.G., Gorbovec M.A., Prager S.M. Struktura i mehanicheskie svojstva zharoprochnyh splavov VZh159 i EP648, poluchennyh metodom selektivnogo lazernogo splavleniya [Structure and mechanical properties of heat resistant alloys VZh159 and EP648, prepared by selective laser fusing] // Aviacionnye materialy i tehnologii. 2016. №S1. S. 8–15. DOI: 10.18577/2071-9140-2016-0-S1-8-15.
  6. Kablov E.N. Sovremennye materialy – osnova innovatsionnoj modernizatsii Rossii [Modern materials – basis of innovative modernization of Russia] // Materialy Evrazii. 2012. №3. S. 10–15.
  7. Grashchenkov D.V., Shchetanov B.V. Efimochkin I.Yu. Razvitie poroshkovoj metallurgii zharoprochnykh splavov [Development of powder metallurgy of hot strength alloys] // Vse materialy. Entsiklopedicheskij spravochnik. 2011. №5. S. 13–26.
  8. Mazalov I.S., Evgenov A.G., Prager S.M. Perspektivy primeneniya zharoprochnogo strukturnostabilnogo splava VZh159 dlya additivnogo proizvodstva vysokotemperaturnyh detalej GTD [Perspectives of heat resistant structurally stable alloy VZh159 application for additive production of high-temperature parts of GTE] // Aviacionnye materialy i tehnologii. 2016. №S1. S. 3–7. DOI: 10.18577/2071-9140-2016-0-S1-3-7.
  9. Nerush S.V., Evgenov A.G. Issledovanie melkodispersnogo metallicheskogo poroshka zharoprochnogo splava marki EP648-VI primenitelno k lazernoj LMD-naplavke, a takzhe ocenka kachestva naplavki poroshkovogo materiala na nikelevoj osnove na rabochie lopatki TVD [Research of fine-dispersed metal powder of the heat resisting alloy of the EP648-VI brand for laser metal deposition (LMD) and also the assessment quality of welding of powder material on the nickel basis on working blades THP] // Trudy VIAM: elektron. nauch.-tehnich. zhurn. 2014. №3. St. 01. Available at: http://www.viam-works.ru (accessed: July 05, 2018). DOI: 10.18577/2307-6046-2014-0-3-1-1.
  10. Evgenov A.G., Nerush S.V., Vasilenko S.A. Poluchenie i oprobovanie melkodispersnogo metallicheskogo poroshka vysokohromistogo splava na nikelevoj osnove primenitelno k lazernoj LMD-naplavke [The obtaining and testing of the fine-dispersed metal powder of the high-chromium alloy on nickel-base for laser metal deposition] // Trudy VIAM: elektron. nauch.-tehnich. zhurn. 2014. №5. St. 04. Available at: http://www.viam-works.ru (accessed: July 05, 2018). DOI: 10.18577/2307-6046-2014-0-5-4-4.
  11. Kablov E.N., Chabina E.B., Morozov G.A., Muravskaya N.P. Otsenka sootvetstviya novykh materialov s ispolzovaniem SO i MI vysokogo urovnya [Assessment of compliance of new materials with use WITH and MI of high level] // Kompetentnost. 2017. №2. C. 40–46.
  12. GOST 17745–90. Stali i splavy. Metody opredeleniya gazov [State Standard 17745–90. There were also alloys. Methods of definition of gases]. M.: Izd-vo standartov, 1990. S. 12.
  13. GOST 22598–93. Nikel i nizkolegirovannye splavy nikelya. Metody opredeleniya kisloroda [State Standard 22598-93. Nickel and nickel low-doped alloys]. M.: Izd-vo standartov, 1994. S. 8.
  14. ASTME E1019-11. Standard Test Methods for Determination of Carbon, Sulfur, Nitrogen, and Oxygen in Steel, Iron, Nickel, and Cobalt Alloys by Various Combustion and Fusion Techniques. ASTM International, 2011. P. 24.
  15. Alekseev A.V., Rastegaeva G.Yu., Pakhomkina T.N. Opyt opredeleniya ugleroda, sery, kisloroda i azota v splavakh na osnove niobiya na gazoanalizatorakh firmy Leco [Experience of the determination of carbon, sulfur, oxygen and nitrogen in alloys based on niobium on the gas-analyzers of the Leco firm] // Trudy VIAM: elektron. nauch.-tehnich. zhurn. 2018. №1. St. 03. URL: http://www.viam-works.ru (accessed: July 05, 2018). DOI: 10.18557/2307-6046-2018-0-1-3-3.