The influence of chemical composition on structure and properties of Al–Mg–Si alloy

Kuznetsov A.O., Oglodkov M.S., Klimkina A.A.
Kuznetsov A.O., Oglodkov M.S., Klimkina A.A. The influence of chemical composition on structure and properties of Al–Mg–Si alloy // Proceedings of VIAM. 2018. No. 7. DOI: 10.18577/2307-6046-2018-0-7-3-9. URL: https://www.viam-works.ru/en/journal/2018/7/1
Keywords
Al–Mg–Si, aluminum alloys, microstructure, mechanical properties, alloying elements, sheets, Al–Mg–Si.
Abstract

The analysis of Russian and foreign literature in aluminum high-end corrosion resistant alloys area was made. Base ways of development of these alloys are stated. Estimation of modern investigation level was made. The influence of alloying elements additions on microstructure, mechanical and fatique properties of Al–Mg–Si alloy was investigated. It was found that Ti and Zr gaves a positive effect for microstructure and mechanical properties.

Reference list
  1. Kablov E.N. Aviakosmicheskoe materialovedenie [Aerospace materials science] // Vse materialy. Entsiklopedicheskij spravochnik. 2008. №3. S. 2–14.
  2. Kablov E.N. Rossii nuzhny materialy novogo pokoleniya [Materials of new generation are necessary to Russia] // Redkie zemli. 2014. №3. S. 8–13.
  3. Kablov E.N., Ospennikova O.G., Vershkov A.V. Redkie metally i redkozemelnye elementy – materialy sovremennyh i budushhih vysokih tehnologij [Rare metals and rare-earth elements are materials for modern and future high technologies] // Aviacionnye materialy i tehnologii. 2013. №S2. S. 3–10.
  4. Kablov E.N., Startsev O.V., Medvedev I.M. Obzor zarubezhnogo opyta issledovanij korrozii i sredstv zashhity ot korrozii [Review of international experience on corrosion and corrosion protection] // Aviacionnye materialy i tehnologii. 2015. №2 (35). S. 76–87. DOI: 10.18577/2071-9140-2015-0-2-76-87.
  5. Kablov E.N. Materialy novogo pokoleniya – osnova innovatsij, tekhnologicheskogo liderstva i natsionalnoj bezopasnosti Rossii [Materials of new generation – basis of innovations, technological leadership and national security of Russia] // Intellekt i tekhnologii. 2016. № 2 (14). S. 16–21.
  6. Klochkov G.G., Grushko O.E., Popov V.I., Ovchinnikov V.V., Shamraj V.F. Struktura, tehnologicheskie svojstva i svarivaemost listov iz splava V-1341 sistemy Al–Mg–Si [Structure, technological properties and bondability of sheets from alloy V-1341 of Al–Mg–Si system] // Aviacionnye materialy i tehnologii. 2011. №1. S. 3–8.
  7. Voronkov V.I., Potapenko K.E., Petrov P.A., Vydumkina S.V. Poluchenie utochnennykh dannykh po soprotivleniyu plasticheskoj deformatsii pri goryachej obemnoj shtampovke alyuminievykh splavov AD35 i AD31 [Obtaining specified data on plastic deformation resistance of aluminum alloys AD35 and AD31 at hot forging] // Aviacionnye materialy i tehnologii. 2017. №1 (46). S. 3–10. DOI: 10.18577/2071-9140-2017-0-1-3-10.
  8. Splav na osnove alyuminiya i izdelie, vypolnennoe iz nego: pat. 2215055 Ros. Federatsiya. №2001133680 [Alloy on the basis of aluminum and the product which has been executed of it: pat. 2215055 Rus. Federation. No. 2001133680]; zayavl. 17.12.01; opubl. 27.10.03.
  9. Deformiruemyj splav na osnove alyuminiya i izdelie, vypolnennoe iz etogo splava: pat. 2255133 Ros. Federatsiya. №2003136632 [Deformable alloy on the basis of aluminum and the product executed from this alloy: pat. 2255133 Rus. Federation. No. 2003136632]; zayavl. 19.12.03; opubl. 27.06.05.
  10. Sposob proizvodstva pressovannykh izdelij iz alyuminievogo splava serii 6000: pat. 2542183 Ros. Federatsiya. №2013131745 [Way of production of the pressed products from aluminum alloy of series 6000: pat. 2542183 Rus. Federation. No. 2013131745]; zayavl. 09.07.13; opubl. 20.02.15.
  11. Edwards G.A., Stiller K., Dunlop G.L., Couper M.J. The precipitation sequence in Al–Mg–Si alloys // Acta Materialia. 2010. Vol. 46. P. 3893–3904.
  12. Pogatscher S., Antrekowitsch H., Leitner H. et al. Mechanisms controlling the artificial aging of Al–Mg–Si Alloys // Acta Materialia. 2011. Vol. 59. P. 3352–3363.
  13. Chakrabarti D.J., Laughlin D.E. Phase relations and precipitation in Al–Mg–Si alloys with Cu additions // Progress in Materials Science. 2004. Vol. 49. P. 389–410.
  14. Gupta A.K., Lloyd D.J., Court S.A. Precipitation hardening in Al–Mg–Si alloys with and without excess Si // Materials Science and Engineering. 2001. Vol. A316. P. 11–17.
  15. Jacobs M.H. The structure of the metastable precipitates formed during ageing of an Al–Mg–Si alloy // Philosophical Magazine. 1972. Vol. 26 (1). P. 1–13.
  16. Kablov E.N. Innovacionnye razrabotki FGUP «VIAM» GNC RF po realizacii «Strategicheskih napravlenij razvitiya materialov i tehnologij ih pererabotki na period do 2030 goda» [Innovative developments of FSUE «VIAM» SSC of RF on realization of «Strategic directions of the development of materials and technologies of their processing for the period until 2030»] // Aviacionnye materialy i tehnologii. 2015. №1 (34). S. 3–33. DOI: 10.18577/2071-9140-2015-0-1-3-33.