Forecasting the strength properties of the skin cover of a deformable aluminum alloy V95o.ch.-T2 with the use of the integrated corrosion reduction coefficient

Kurs M.G.
Kurs M.G. Forecasting the strength properties of the skin cover of a deformable aluminum alloy V95o.ch.-T2 with the use of the integrated corrosion reduction coefficient // Proceedings of VIAM. 2018. No. 5. DOI: 10.18577/2307-6046-2018-0-5-101-109. URL: https://www.viam-works.ru/en/journal/2018/5/11
Keywords
corrosion, aluminum alloys, integral corrosion coefficient, field-accelerated tests.
Abstract

At present, the issue of developing methods for predicting the change in the strength properties of structural aluminum alloys used in the composition of structural elements in conditions of environmental factors for long periods of operation is topical. In this case, the key is to search for the principal approaches to predicting the corrosive behavior of aluminum alloys as materials for which uneven corrosion damage is characteristic, and assessing the complex effect of the most dangerous types of local corrosion on the change in the mechanical properties of aluminum alloys. The calculation of the integral coefficient of corrosion failure based on the predicted values of the main corrosion characteristics of aluminum alloys-loss of weight, depth of pitting and intercrystalline corrosion, as well as the tendency to delaminating corrosion, has been performed. It is shown that the application of the method of calculating the integral corrosion coefficient can be used to obtain the pred

Reference list
  1. Kablov E.N. Innovacionnye razrabotki FGUP «VIAM» GNC RF po realizacii «Strategicheskih napravlenij razvitiya materialov i tehnologij ih pererabotki na period do 2030 goda» [Innovative developments of FSUE «VIAM» SSC of RF on realization of «Strategic directions of the development of materials and technologies of their processing for the period until 2030»] // Aviacionnye materialy i tehnologii. 2015. №1 (34). S. 3–33. DOI: 10.18577/2071-9140-2015-0-1-3-33.
  2. Antipov V.V. Strategiya razvitiya titanovyh, magnievyh, berillievyh i alyuminievyh splavov [Strategy of development of titanium, magnesium, beryllium and aluminum alloys] // Aviacionnye materialy i tehnologii. 2012. №S. S. 157–167.
  3. Kablov E.N., Startsev O.V., Medvedev I.M. Obzor zarubezhnogo opyta issledovanij korrozii i sredstv zashhity ot korrozii [Review of international experience on corrosion and corrosion protection] // Aviacionnye materialy i tehnologii. 2015. №2 (35). S. 76–87. DOI: 10.18577/2071-9140-2015-0-2-76-87.
  4. Samojlov I.A., Stradomskij O.Yu., Shapkin V.S. Sostoyanie grazhdanskoj aviatsionnoj tekhniki Rossii i prognoz ee obnovleniya do 2030 goda [Condition of civil aviation engineering of Russia and the forecast of its updating till 2030] // Nauchnyj vestnik MGTUGA. 2013. Vyp. 187. S. 7–18.
  5. Zubarev A.P., Lapaev A.V., Lapaev V.P. Ispolzovanie obobshchennogo parametra korrozionnogo porazheniya dlya otsenki dolgovechnosti elementov konstruktsij s korrozionnymi porazheniyami [Use of the generalized parameter of corrosion defeat for assessment of durability of elements of designs with corrosion defeats] // Nauchnyj vestnik MGTUGA. 2007. Vyp. 119. S. 30–32.
  6. Akopyan K.E., Lapaev A.V., Semin A.V. Analiz korrozionnogo sostoyaniya samoletov Tu-154M OAO Aviakompanii «AEROFLOT-RAL». Po dannym materialov tekhnicheskogo obsluzhivaniya v obeme formy «2» [Analysis of corrosion condition of the Tu-154М airplanes of JSC Airline company «AEROFLOT-RAL». According to materials of technical maintenance in form «2»] // Nauchnyj vestnik MGTUGA. 2007. Vyp. 119. S. 24–29.
  7. Fomina M.A., Karimova S.A. Analiz korrozionnogo sostoyaniya materialov planera samoletov tipa «Su» posle dlitelnykh srokov ekspluatatsii [The analysis of corrosion condition of materials of glider of airplanes of the SU type after long terms of operation] // Korroziya: materialy, zashchita. 2014. №9. S. 20–24.
  8. Bakshaev S.I., Gavrilov I.V. Klimaticheskie ispytaniya materialov i izdelij tekhniki [Climatic tests of materials and equipment products] // Korroziya, starenie i biostojkost materialov v morskom klimate: sb. dokl. II Mezhdunar. nauch.-tekhnich. konf. M.: VIAM, 2016. St. 02 (CD).
  9. Lavro N.A., Sukhoivanenko V.V., Dyudin V.B., Budyuk G.Yu. Analiz effektivnosti antikorrozionnoj zashchity samoletov Be-200CHS, ekspluatiruyushchikhsya v MCHS Rossii i PAO «TANTK im. G.M. Berieva» [The analysis of efficiency of anticorrosive protection of the Be-200ChS airplanes which are maintaining in Emercom of Russia and PAO «TANTK of G.M. Beriyev»] // Korroziya, starenie i biostojkost materialov v morskom klimate: sb. dokl. II Mezhdunar. nauch.-tekhnich. konf. M.: VIAM, 2016. St. 09 (CD).
  10. GOST 9.040–74 ESZKS. Metally i splavy. Raschetno-eksperimentalnyj metod uskorennogo opredeleniya korrozionnykh poter' v atmosfernykh usloviyakh [State Standard 9.040–74. Metals and alloys. Rated and experimental method of the accelerated definition of corrosion losses in atmospheric conditions]. M.: Izd-vo standartov, 1974. 14 s.
  11. Mikhajlov A.A., Panchenko YU.M., Igonin T.N., Kovtanyuk V.V. Atmosfernaya korroziya tsinka: kartografirovanie skorosti korrozii na evropejskoj territorii Rossijskoj Federatsii [Atmospheric corrosion of zinc: corrosion rate mapping in the European territory of the Russian Federation] // Korroziya: materialy, zashchita. 2012. №9. S. 1–5.
  12. Mikhajlov A.A., Panchenko Yu.M., Igonin T.N. i dr. Atmosfernaya korroziya uglerodistoj stali: modelirovanie i kartografirovanie territorii Rossijskoj Federatsii [Atmospheric corrosion of carbon steel: modeling and mapping of the territory of the Russian Federation] // Korroziya: materialy, zashchita. 2010. №11. S. 1–10.
  13. Lutsenko A.N., Kurs M.G., Laptev A.B. Obosnovanie srokov naturnykh klimaticheskikh ispytanij metallicheskikh materialov v atmosfere chernomorskogo poberezhya. Analiticheskij obzor [Justification of terms of natural climatic tests of metal materials in the atmosphere of the Black Sea coast. Analytical review] // Voprosy materialovedeniya. 2016. №3 (87). S. 126–137.
  14. Kurs M.G., Antipov V.V., Lutsenko A.N., Kutyrev A.E. Integralnyj koeffitsient korrozionnogo razrusheniya deformiruemykh alyuminievykh splavov [Integral figure of corrosion damage of deformed aluminum alloys] // Aviacionnye materialy i tehnologii. 2016. №3 (42). S. 24–32. DOI: 10.18577/2071-9140-2016-0-3-24-32.
  15. Kurs M.G., Antipov V.V., Kutyrev A.E. Prognozirovanie poter prochnostnykh svojstv listovykh deformiruemykh alyuminievykh splavov s primeneniem integralnogo koeffitsienta korrozionnogo razrusheniya [Forecasting of losses of strength properties of sheet deformable aluminum alloys using integral factor of corrosion destruction] // Fundamentalnye issledovaniya i poslednie dostizheniya v oblasti zashchity ot korrozii, stareniya i biopovrezhdenij materialov i slozhnykh tekhnicheskikh sistem v razlichnykh klimaticheskikh usloviyakh: sb. dokl. III Vseros. nauch.-tekhnich. konf. M.: VIAM, 2016. S. 09 (CD).
  16. Kurs M.G., Laptev A.B., Kutyrev A.E., Morozova L.V. Issledovanie korrozionnogo razrusheniya deformiruemykh alyuminievykh splavov pri naturno-uskorennykh ispytaniyakh. Chast 1 [Research of corrosion destruction of deformable aluminum alloys at natural accelerated tests. Part 1] // Voprosy materialovedeniya. 2016. №1 (85). S. 116–126.
  17. Aviatsionnye materialy: spravochnik v 13 t. / pod obshch. red. E.N. Kablova. T. 4: Alyuminievye i berillievye splavy, ch. 1: Deformiruemye alyuminievye splavy, kn. 2. [Aviation materials: directory in 13 vol. / gen ed. by E.N.Kablova. Vol. 4: Aluminum and beryllium alloys. P.1: Deformable aluminum alloys, book 2]. M.: VIAM, 2009. C. 49–50.
  18. Senatorova O.G., Grushko O.E., Tkachenko E.A., Antipov V.V. i dr. Novye vysokoprochnye alyuminievye splavy i materialy [New high-strength aluminum alloys and materials] // Tekhnologiya legkikh splavov. 2007. №2. S. 17–24.