Investigation of the possibility of protection of intermetallic titanium alloy against fretting wear by ion-plasma coating

Gorlov D.S., Aleksandrov D.A., Zaklyakova O.V., Azarovskiy E.N.
Gorlov D.S., Aleksandrov D.A., Zaklyakova O.V., Azarovskiy E.N. Investigation of the possibility of protection of intermetallic titanium alloy against fretting wear by ion-plasma coating // Proceedings of VIAM. 2018. No. 4. DOI: 10.18577/2307-6046-2018-0-4-51-58. URL: https://www.viam-works.ru/en/journal/2018/4/6
Keywords
titanium intermetallic compounds, ion-plasma coatings, vacuum-arc coating, magnetron deposition, fretting, fretting wear, heat resistance, metallography, microrentgen-spectral analysis.
Abstract

Analyzing the causes of failures of units and units of GTE in the course of their long-term operation, as well as the results of bench tests, came to the conclusion that the main cause of the origin of most fatigue defects, leading to destruction, is fretting. Among the various methods of applying protective and hardening coatings on contacting surfaces to prevent fretting, the most technological are vacuum-plasma and ion-implant processing technologies, as well as their combinations. This work was carried out within the framework of strategic direction 17. «Comprehensive anticorrosive protection, hardening, wear-resistant protective and heat-protective coatings». Complex problem 17.3. «Multi-Layer heat-resistant and heat-protective coatings, nanostructured reinforcing erosion and corrosion-resistant, wear-resistant, antifretting coatings to protect parts of the hot tract and compressor GTE and GTU» («Strategic directions of development of materials and technologies for their processi

Reference list
  1. Smyslov A.M., Selivanov K.S. Razrabotka i issledovanie tehnologicheskih metodov povysheniya fretting-stojkosti rabochih lopatok iz titanovyh splavov [Development and research of technological methods of increase fretting firmness of working blades from titani-um alloys] // Vestnik UGATU. Ser.: Mashinostroenie. T. 9. №1 (19). C. 77–83.
  2. Kablov E.N., Ospennikova O.G., Bazyleva O.A. Materialy dlya vysokoteplonagruzhennyh detalej gazoturbinnyh dvigatelej [Materials for the high-heatloaded details of gas turbine engines] // Vestnik MGTU im. N.E. Baumana. Ser.: Mashinostroenie. 2011. № SP2. S. 13–19.
  3. Kablov E.N. Litye lopatki gazoturbinnyh dvigatelej. Splavy, tehnologii, pokrytiya. 2-e izd. [Cast blades of gas turbine engines. Alloys, technologies, coverings. 2nd ed.]. M.: Nauka, 2006. S. 531–534.
  4. Muboyadzhyan S.A., Aleksandrov D.A., Gorlov D.S., Egorova L.P., Bulavinceva E.E. Zashhitnye i uprochnyayushhie ionno-plazmennye pokrytiya dlya lopatok i drugih otvetstvennyh detalej kompressora GTD [Protective and strengthening ion-plasma coverings for blades and other responsible details of the GTE compressor] // Aviacionnye materialy i tehnologii. 2012. №S. S. 71–81.
  5. Gorlov D.S., Skripak V.I., Muboyadzhyan S.A., Egorova L.P. Issledovanie fretting-iznosa tverdosmazochnogo, shlikernogo i ionno-plazmennogo pokrytij [The research of fretting-wear slip and ion-plasma coatings] // Trudy VIAM: elektron. nauch.-tehnich. zhurn. 2017. №3. St. 07. Available at: http://www.viam-works.ru (accessed: March 12, 2018). DOI: 10.18577/2307-6046-2017-0-3-7-7.
  6. Lesnevskij L.N. Fretting-korroziya pokrytij tipa «tverdaya smazka» v ekstremalnyh usloviyah ekspluatacii [Fretting corrosion of coverings of the solid lubricant type in extreme operating conditions] // Vestnik nauchno-tehnicheskogo razvitiya. 2009. №2 (18). S. 31–35.
  7. Putyrskij S.V., Arislanov A.A., Artemenko N.I., Yakovlev A.L. Razlichnye metody povysheniya iznosostojkosti titanovyh splavov i sravnitelnyj analiz ih effektivnosti primen-itelno k titanovomu splavu VT23M [Different methods of wear resistance increase of titanium alloys and comparative analysis of their efficiency for VT23M titanium alloy] // Aviacionnye materialy i tehnologii. 2018. №1. S. 19–24. DOI: 10.18577/2071-9240-2018-0-1-19-24.
  8. Muboyadzhyan S.A., Budinovskij S.A. Ionno-plazmennaja tehnologiya: perspektivnye processy, pokrytiya, oborudovanie [Ion-plasma technology: prospective processes, coatings, equipment] // Aviacionnye materialy i tehnologii. 2017. №S. S. 39–54. DOI: 10.18577/2071-9140-2017-0-S-39-54.
  9. Kablov E.N., Muboyadzhyan S.A., Budinovskij S.A., Pomelov Ya.A. Ionno-plazmennye zashhitnye pokrytiya dlya lopatok gazoturbinnyh dvigatelej [Ion-plasma protecting covers for blades of gas turbine engines] // Konversiya v mashinostroenii. 1999. №2. S. 42–47.
  10. Sibileva S.V., Kozlova L.S. Obzor tehnologij polucheniya pokrytij na titanovyh splavah plazmennym elektroliticheskim oksidirovaniem [Review of technologies of applying coatings to titanium alloys by plasma electrolytic oxidation] // Aviacionnye materialy i tehnologii. 2016. №S2 (44). S. 3–10. DOI: 10.18577/2071-9140-2016-0-S2-3-10.
  11. Selivanov K.S., Galiakbarov R.F. Povyshenie fretting-stojkosti detalej mashin kompleksnoj vakuumnoj plazmennoj obrabotkoj [Increase fretting firmness of details of machines com-plex vacuum plasma processing] // Aviacionno-kosmicheskaya tehnika i tehnologiya. 2011. №7 (84). S. 29–32.
  12. Kablov E.N., Nochovnaya N.A., Panin P.V., Alekseev E.B., Novak A.V. Issledovanie struktury i svojstv zharoprochnyh splavov na osnove alyuminidov titana s mikrodobavkami gadoliniya [Research of structure and properties of hot strength alloys on the basis of titanium aluminides with gadolinium microadditives] // Materialovedenie. 2017. №3. S. 3–10.
  13. Antipov V.V. Perspektivy razvitiya alyuminievyh, magnievyh i titanovyh splavov dlya izdelij aviacionno-kosmicheskoj tehniki [Prospects for development of aluminium, magnesium and titanium alloys for aerospace engineering] // Aviacionnye materialy i tehnologii. 2017. №S. S. 186–194. DOI: 10.18577/2107-9140-2017-0-S-186-194.
  14. Novak A.V., Alekseev E.B., Ivanov V.I., Dzunovich D.A. Izuchenie vliyaniya parametrov zakalki na strukturu i tverdost intermetallidnogo titanovogo orto-splava VTI-4 [The study of the quenching parameters influence on structure and hardness of orthorhombic titanium alu-minide alloy VТI-4] // Trudy VIAM: elektron. nauch.-tehnich. zhurn. 2018. №2. St. 05. Available at: http://www.viam-works.ru (accessed: March 12, 2018). DOI: 10.18577/2307-6046-2018-0-2-5-5.
  15. Kablov E.N. Innovacionnye razrabotki FGUP «VIAM» GNC RF po realizacii «Strategicheskih napravlenij razvitiya materialov i tehnologij ih pererabotki na period do 2030 goda» [Innovative developments of FSUE «VIAM» SSC of RF on realization of «Strategic directions of the development of materials and technologies of their processing for the period until 2030»] // Aviacionnye materialy i tehnologii. 2015. №1 (34). S. 3–33. DOI: 10.18577/2071-9140-2015-0-1-3-33.
  16. Kurzina I.A., Popova N.A., Nikonenko E.L. i dr. Formirovanie nanorazmernyh in-termetallidnyh faz v usloviyah implantacii ionami alyuminiya titanovyh mishenej [Forming of nanodimensional intermetallidny phases in the conditions of implantation by ions of aluminum of titanic targets ] // Izvestiya RAN. Ser.: Fizicheskaya. 2012. T. 76. №1. S. 74–78.