Influence of machining on mechanical and fatigue properties of sheets from aluminum-lithium alloys 1441 and V-1481

Grigoriev M.V., Oglodkov M.S.
Grigoriev M.V., Oglodkov M.S. Influence of machining on mechanical and fatigue properties of sheets from aluminum-lithium alloys 1441 and V-1481 // Proceedings of VIAM. 2018. No. 4. DOI: 10.18577/2307-6046-2018-0-4-20-27. URL: https://www.viam-works.ru/en/journal/2018/4/3
Keywords
aluminum-lithium alloys, laser-beam cutting, hydroabrasive cutting, machining, sheets.
Abstract

The state-of-the-art review of domestic and foreign literature on technologies of laser-beam and hydroabrasive cutting of semi-finished products from aluminum alloys is carried out. The main tendencies of development are revealed and the assessment of the current level of researches is carried out. Technological modes of milling, hydroabrasive and laser-beam cutting of sheets from alloy V-1481T1 1,5 and 3,0 mm thick and sheets from alloy 1441Т1 the 1,5 mm thick are investigated and fulfilled. It is established that at laser-beam cutting for sheets from alloy 1481 lack of defects (fin, not cuts) is provided at the radiant power not less than 3 and 4 kW respectively, thus the best quality of edges of the machine cut corresponds to the speed of 10 m/min. for both thickness, and for sheets from alloy 1441 – at the radiant power not less than 2 kW respectively, thus the best quality of edges of the machine cut corresponds to the speed of 7,5 m/min. The best quality of edge of leaf after

Reference list
  1. Kablov E.N. Aviakosmicheskoe materialovedenie [Aerospace materials science] // Vse materialy. Enciklopedicheskij spravochnik. 2008. №3. S. 2–14.
  2. Kablov E.N. Rossii nuzhny materialy novogo pokoleniya [Materials of new generation are necessary to Russia] // Redkie zemli. 2014. №3. S. 8–13.
  3. Kablov E.N., Ospennikova O.G., Vershkov A.V. Redkie metally i redkozemelnye elementy – materialy sovremennyh i budushhih vysokih tehnologij [Rare metals and rare-earth elements are materials for modern and future high technologies] // Aviacionnye materialy i tehnologii. 2013. №S2. S. 3–10.
  4. Kablov E.N. Materialy novogo pokoleniya – osnova innovacij, tehnologicheskogo liderstva i nacionalnoj bezopasnosti Rossii [Materials of new generation – basis of innovations, technological leadership and national security of Russia] // Intellekt i tehnologii. 2016. №2 (14). S. 16–21.
  5. Serebrennikova N.Yu., Antipov V.V., Senatorova O.G., Erasov V.S., Kashirin V.V. Gibridnye sloistye materialy na baze alyuminij-litievyh splavov primenitelno k panelyam kryla samoleta [Hybrid multilayer materials based on aluminum-lithium alloys applied to panels of plane wing] // Aviacionnye materialy i tehnologii. 2016. №3 (42). S. 3–8. DOI: 10.18577/2071-9140-2016-0-3-3-8.
  6. Fomina M.A., Kutyrev A.E., Klochkova Yu.Yu., Sbitneva S.V. Issledovanie korrozionnyh harakteristik vysokoprochnogo splava sistemy Al–Cu–Li v zavisimosti ot razlichnyh rezhimov termicheskoj obrabotki [Research of corrosion characteristics of high-strength alloy of Al–Cu–Li system depending on various modes of heat treatment] // Aviacionnye materialy i tehnologii. 2016. №S2. S. 39–48. DOI: 10.18577/2071-9140-2016-0-S2-39-48.
  7. Stepanova M.A. Vybor gaza dlya lazernoj rezki metallov [Gas choice for laser-beam cutting of metals] // RITM Mashinostroeniya. 2017. №4. S. 102–104.
  8. Gajdachuk V.E., Kostenko A.I. Analiz effektivnosti tehnologii lazernoj obrezki listovyh detalej iz alyuminievyh splavov v aviacionnom proizvodstve [The analysis of efficiency of technology laser scraps of sheet details from aluminum alloys in aviation production] // Voprosy proektirovaniya i proizvodstva konstrukcij letatelnyh apparatov: sb. nauch. tr. Nac. aerokosm. un-ta im. N.E. Zhukovskogo «HAI». 2010. Vyp. 2 (62). S. 85–97.
  9. Gajdachuk V.E., Kostenko A.I. Eksperimentalno-teoreticheskij metod optimizacii parametrov processa lazernoj rezki obrazcov materialov iz alyuminievyh splavov po kriteriyu maksimal'noj dolgovechnosti [Experimental and theoretical method of optimization of parameters of process of laser-beam cutting of samples of materials from aluminum alloys by criterion of the maximum durability] // Otkrytye informacionnye i kompyuternye integrirovannye tehnologii: sb. nauch. tr. Nac. aerokosm. un-ta im. N.E. Zhukovskogo «HAI». 2010. Vyp. 48. S. 53–61.
  10. Blinkov V.V. Analiz modelej lazernoj rezki metallov v srede neaktivnogo gaza [The analysis of models of laser-beam cutting of metals in the environment of inactive gas] // Tr. in-ta teor. i prikladnoj mehaniki SO RAN. 1999. T. 7 (24). №2. S. 133–150.
  11. Panchenko V.Ya., Golubev V.S., Vasilcov V.V. i dr. Lazernye tehnologii obrabotki materialov: sovremennye problemy fundamentalnyh issledovanij i prikladnyh razrabotok [Laser technologies of processing of materials: modern problems of basic researches and applied development]. M.: Fizmatlit, 2009. 664 s.
  12. Shmanev V.A., Shulepov A.P., Meshheryakov A.V. Strujnaya gidroabrazivnaya obrabotka detalej GTD [Jet hydroabrasive machining of details of GTE]. M.: Mashinostroenie, 1995. 350 s.
  13. Stepanov Yu.S., Barsukov G.V. Sovremennye tehnologicheskie processy mehanicheskogo i gidrostrujnogo raskroya tehnicheskih tkanej [Modern technological processes mechanical and hydrojet patterning technical fabrics]. M.: Mashinostroenie, 2004. 239 s.
  14. Stepanov Yu.S., Burnashov M.A., Golovin K.A. Progressivnye tehnologii gidrostrujnogo rezaniya materialov [Progressive technologies of hydrojet cutting of materials]. Tula: Izd-vo TulGU, 2009. 318 s.
  15. Kolobnev N.I., Hohlatova L.B., Antipov V.V. Perspektivnye alyuminij-litievye splavy dlya samoletnyh konstrukcij [Perspective aluminum-lithium alloys for aircraft designs] // Tehnologiya legkih splavov. 2007. №2. S. 35–38.
  16. Kablov E.N. Innovacionnye razrabotki FGUP «VIAM» GNC RF po realizacii «Strate-gicheskih napravlenij razvitiya materialov i tehnologij ih pererabotki na period do 2030 goda» [Innovative developments of FSUE «VIAM» SSC of RF on realization of «Strategic directions of the development of materials and technologies of their processing for the period until 2030»] // Aviacionnye materialy i tehnologii. 2015. №1 (34). S. 3–33. DOI: 10.18577/2071-9140-2015-0-1-3-33.