Obtaining a positive microhardness gradient as a method of increasing the adhesion of electrolytic chromium coatings
Salakhova R.K., Tihobrazov A.B., Nazarkin R.M. Obtaining a positive microhardness gradient as a method of increasing the adhesion of electrolytic chromium coatings // Proceedings of VIAM. 2018. No. 3. DOI: 10.18577/2307-6046-2018-0-3-77-85. URL: https://www.viam-works.ru/en/journal/2018/3/9
Keywords
chrome plating, adhesive strength, microhardness, gradient chromium coating, metallography, coating thickness, residual internal stresses.
Abstract
A method is proposed for obtaining thick chrome coatings in a self-regulating electrolyte with chromium plating with a positive microhardness gradient in thickness. The adhesion strength of the graded chromium coating was estimated by the temperature change method and the impact method on the vertical copra U-2M and metallographic studies of the individual layers of chromium deposited under various electrolysis regimes. The results of the investigation of residual macrostresses by x-ray diffractometric method in chromium coatings of various microhardness are presented.
Reference list
- Dospehi dlya «Burana». Materialy i tehnologii VIAM dlya MKS «Energiya–Buran» / pod red. E.N. Kablova [Armor for «Buran». Materials and VIAM technologies for ISS of «Energiya–Buran» / ed. by E.N. Kablov. 3rd ed.]. M.: Nauka i zhizn, 2013. 128 s.
- Kablov E.N. Tendencii i orientiry innovacionnogo razvitiya Rossii: sb. inform. materialov. 3-e izd. [Tendencies and reference points of innovative development of Russia: collection of information materials. 3rd ed.]. M.: VIAM, 2015. 720 s.
- Kablov E.N. Innovacionnye razrabotki FGUP «VIAM» GNC RF po realizacii «Strategicheskih napravlenij razvitiya materialov i tehnologij ih pererabotki na period do 2030 goda» [In-novative developments of FSUE «VIAM» SSC of RF on realization of «Strategic directions of the development of materials and technologies of their processing for the period until 2030»] // Aviacionnye materialy i tehnologii. 2015. №1 (34). S. 3–33. DOI: 10.18577/2071-9140-2015-0-1-3-33.
- Salahova R.K., Tihoobrazov A.B. Fiziko-himicheskie svojstva oksalatno-sulfatnogo elektrolita hromirovaniya, soderzhashhego nanorazmernye chasticy oksidov metallov [Physical and chemical properties of oxalate-sulfate chromium plating electrolyte, containing metal oxide nanoparticles] // Aviacionnye materialy i tehnologii. 2016. №4 (45). S. 31–39. DOI: 10.18577/2071-9140-2016-0-4-31-39.
- Gubarevich G.P., Savchenko A.V., Fomichev V.T. Optimizaciya tehnologicheskih parametrov processa hromirovaniya iz samoreguliruyushhegosya elektrolita s kompleksnoj organo-neorganicheskoj dobavkoj [Optimization of technological parameters of process of chromizing from self-regulating electrolit with complex organo-inorganic additive] // VolgGASU: Internet-vestnik. 2015. Vyp. 4 (40). S. 1–5. URL: http://www.vestnik.vgasu.ru (data obrashheniya: 09.02.2018).
- Gubin A.F., Ilin V.I., Kolesnikov V.A. Razrabotka kompleksa specialnyh meropriyatij po povysheniyu himicheskoj bezopasnosti galvanicheskogo proizvodstva [Development of complex of special events for increase of chemical safety of galvanic production] // Himicheskaya i biologicheskaya bezopasnost. 2015. №1–2. S. 83–86.
- Vinogradov S.S., Nikiforov A.A., Balahonov S.V. Zamena kadmiya. Etap 1. Povyshenie zashhitnoj sposobnosti cinkovyh pokrytij: termoimmersionnoe i modificirovannoe pokrytiya [Cadmium replacement. Part 1. Improving of protective property of zinc coatings: thermo-immersed and modified coatings] // Aviacionnye materialy i tehnologii. 2015. №4 (37). S. 53–60. DOI: 10.18577/2071-9140-2015-0-4-53-60.
- Vinogradov S.S. Ekologicheski bezopasnoe galvanicheskoe proizvodstvo [Ecologically safe galvanic production]. M.: Globus, 1998. Vyp. 3. 298 s.
- Lisicyn V.E., Abdulina V.S., Karavaev A.V. i dr. Kriterij ekologichnosti elektroliticheskogo processa hromirovaniya [Criterion of environmental friendliness of electrolytic process of chromizing] // Vestnik TGU. 1999. T. 4. Vyp. 2. S. 240–241.
- Ilin V.I., Gubin A.F., Kolesnikov V.A. Minimizaciya obrazovaniya opasnyh himicheskih zhidkih othodov v galvanotehnike (obzor) [Minimization of formation of hazardous chemical liquid waste in galvanotechnics (overview)] // Himiya. Himicheskaya tehnologiya. 2011. №1. S. 29–42.
- Molchanov V.F. Effektivnost i kachestvo hromirovaniya detalej [Efficiency and quality of chromizing of details]. Kiev: Tehnika, 1979. 228 s.
- Kovenskij I.M., Povetkin V.V. Metallovedenie pokrytij [Metallurgical science of coverings]. M.: Intermet Inzhiniring, 1999. 296 s.
- Glyancev N.I., Kotov V.V., Stekolnikov Yu.A. Vliyanie hromirovaniya na fiziko-mehanicheskie svojstva metallov [Influence of chromizing on physicomechanical properties of metals] // Himiya i himicheskaya tehnologiya. 2006. T. 49. Vyp. 9. S. 74–78.
- Semenychev V.V., Salahova R.K. Ocenka adgezii nikel-kobaltovogo pokrytiya k steklo- i ugleplastiku metodom carapanya [Evaluation of nickel-cobalt coating adhesion to fiberglass and carbon fiber–reinforced plastic by scratching] // Trudy VIAM: elektron. nauch.-tehnich. zhurn. 2016. №7 (43). St. 06. Available at: http://www.viam-works.ru (accessed: February 09, 2018). DOI: 10.18577/2307-6046-2016-0-7-6-6.
- Pfeiffer W., Koplin C., Reisacher E., Wenzel J. Residual Stresses and Strength of Hard Chromium Coatings // Materials Science Forum. 2011. Vol. 681. Р. 133–138. DOI: 10.4028/www.scientific.net/MSF.681.133.
- Solodkova L.N., Kudryavcev V.N. Elektroliticheskoe hromirovanie [Electrolytic chromizing]. M.: Globus, 2007. 191 s.
- Truhanov E.M., Kolesnikov A.V., Loshkarev I.D. Dalnodejstvuyushhie napryazheniya v epitaksialnoj plenke, sozdannye dislokaciyami nesootvetstviya [Long-range tension in the epitaxial film, the discrepancies created by dislocations] // Materialy elektronnoj tehniki. 2014. №1 (65). S. 24–31.
- Elektrolit dlya hromirovaniya stalej, mednyh i titanovyh splavov: pat. 2187587 Ros. Federaciya [Electrolit for chromizing steel, copper and titanium alloys: pat. 2187587 Rus. Federation]; zayavl. 09.01.01; opubl. 20.08.02, Byul. №23.
- Tyurikov E.V., Tihoobrazov A.B., Salahova R.K. Issledovanie svojstv razbavlennogo samoreguliruyushhegosya elektrolita hromirovaniya, soderzhashhego nanorazmernye chas-ticy oksida alyuminiya [Research of properties of the diluted self-regulating chromium plating electrolyte with nano-scale aluminum oxide particles] // Trudy VIAM: elektron. nauch.-tehnich. zhurn. 2015. №6. St. 06. Available at: http://www.viam-works.ru (accessed: February 09, 2018). DOI: 10.18577/2307-6046-2015-0-6-6-6.
- Sposob naneseniya elektroliticheskih pokrytij na osnove hroma: pat. 2457288 Ros. Federaciya [Way of drawing electrolytic coverings on the basis of chrome: pat. 2457288 Russ. Federation]; zayavl. 31.05.11; opubl. 27.07.12, Byul. №21.
- Shluger M.A., Tok L.D. Galvanicheskie pokrytiya v mashinostroenii [Galvanic coverings in mechanical engineering]. M.: Mashinostroenie, 1985. T. 2. 248 s.
- Bekkert M., Klemm H. Sposoby metallograficheskogo travleniya: spravochnik [Ways of metallographic etching: directory]. M.: Metallurgiya, 1988. 398 s.
- Morgunov Yu.A., Saushkin B.P. Additivnye tehnologii dlya aviakosmicheskoj tehniki [The additive technologies for aerospace equipment ] // Additivnye tehnologii. 2016. №1. S. 30–38.
- Bogorad L.Ya. Hromirovanie [Chromizing]. L.: Mashinostroenie, 1984. 96 s.