Modern thermal barrier coatings obtained by electron-beam physical vapor deposition (review)
Kashin D.S., Stekhov P.A. Modern thermal barrier coatings obtained by electron-beam physical vapor deposition (review) // Proceedings of VIAM. 2018. No. 2. DOI: 10.18577/2307-6046-2018-0-2-10-10. URL: https://www.viam-works.ru/en/journal/2018/2/10
Keywords
YSZ, nickel alloys, ceramic layer, thermal barrier coating (TBC), thermal conductivity coefficient.
Abstract
Different compositions and technologies for obtaining heat-shielding coatings for gas turbine engine parts (GTE) are considered in the article. The analysis showed that in order to increase the working temperature of the ceramic layer of heat-shielding coating, the best method is to change the chemical composition of the ceramic by introducing an additional amount of rare-earth alloying elements. This provides the possibility of obtaining a certain level of the thermal coefficient of linear expansion, which leads to an increase in the operating time of the cooled GTE part before the destruction of the ceramic layer of the TBC.
Reference list
- Litye lopatki gazoturbinnyh dvigatelej: splavy, tehnologii, pokrytiya / pod obshh. red. E.N. Kablova. 2-e izd. [Cast blades of gas turbine engines: alloys, technologies, coverings / gen. ed. by E.N. Kablov. 2nd ed.]. M.: Nauka. 2006. 632 s.
- Kablov E.N., Petrushin N.V., Svetlov I.L., Demonis I.M. Nikelevye litejnye zharoprochnye splavy novogo pokoleniya [Nickel foundry heat resisting alloys of new generation] // Aviacionnye materialy i tehnologii. 2012. №S. C. 36–52.
- Chubarov D.A., Matveev P.V. Novye keramicheskie materialy dlya teplozashhitnyh pokrytij rabochih lopatok GTD [New ceramic materials for thermal barrier coating using in GTE turbine blades] // Aviacionnye materialy i tehnologii. 2013. №4. S. 43–46.
- Muboyadzhyan S.A., Budinovskij S.A., Gayamov A.M., Matveev P.V. Vysokotemperaturnye zharostojkie pokrytiya i zharostojkie sloi dlya teplozashhitnyh pokrytij [High-temperature heat resisting coverings and heat resisting layers for heat-protective coverings] // Aviacionnye materialy i tehnologii. 2013. №1. S. 17–20.
- Kablov E.N., Muboyadzhyan S.A. Zharostojkie i teplozashhitnye pokrytiya dlya lopatok turbiny vysokogo davleniya perspektivnyh GTD [Heat resisting and heat-protective coverings for turbine blades of high pressure of perspective GTE] // Aviacionnye materialy i tehnologii. 2012. №S. S. 60–70.
- Chubarov D.A., Budinovskij S.A., Smirnov A.A. Magnetronnyj sposob naneseniya keramicheskih sloev teplozashhitnyh pokrytij [Magnetron sputtering method for applying ceramic layers for thermal barrier coatings] // Aviacionnye materialy i tehnologii. 2016. №4. S. 23–30. DOI: 10.18577/2107-9140-2016-0-4-23-30.
- Terry S.G., Litty J.R., Levi C.G. Evolution of porosity and texture in thermal barrier coatings grown by EB-PVD /Elevated Temperature Coatings: Science and Technology III edited by J.M. Hampikian and N.B. Dahotre // The Minerals, Metals and Materials Society. 1999. P. 13–26.
- Kablov E.N. Materialy novogo pokoleniya [Materials of new generation] // Zashhita i bezopasnost. 2014. №4. S. 28–29.
- Tamarin Yu.A., Kachanov E.B. Elektronno-luchevaya tehnologiya naneseniya teplozashhitnyh pokrytij [Electron beam technology of drawing heat-protective coverings] // Novye tehnologicheskie processy i nadezhnost GTD / CIAM. 2008. №7. C. 144–158.
- Baranov D.A., Drevnyak V.O., Pashhenko G.T. Osobennosti tehnologii remonta teplozashhitnyh pokrytij [Features of technology of repair of heat-protective coverings] // Nauchnyj vestnik MGTU GA. 2012. №183. C. 59–62.
- Bychkov N.G., Hamidullin A.Sh., Pershin A.V. Ocenka napryazhennogo sostoyaniya teplozashhitnogo pokrytiya stolbchatoj struktury na soplovyh lopatkah turbin i segmentah zharovyh trub kamer sgoraniya s uchetom sil treniya mezhdu keramicheskim sloem i gazodinamicheskim potokom [Assessment of tension of heat-protective covering of stolbchaty structure on nozzle blades of turbines and segments of spherical pipes of combustion tubes taking into account friction forces between ceramic layer and gas dynamic flow] // Vestnik Samarskogo gosudarstvennogo aerokosmicheskogo universiteta. 2011. №3 (27). C. 253–257.
- Grechanyuk N.I., Kucherenko P.P., Grechanyuk I.N. i dr. Sovremennye teplozashhitnye pokrytiya dlya lopatok gazoturbinnyh dvigatelej i oborudovanie dlya ih polucheniya [Modern heat-protective coverings for blades of gas turbine engines and the equipment for their receiving] // Naukovі notatki. 2011. №31. S. 92–99.
- Electron beam vapor deposition apparatus and method of coating: pat. 8419857 US; publ. 16.04.13.
- Gurrappa I., Sambasiva Rao A. Thermal barrier coatings for enhanced efficiency of gas turbine engines // Surface & Coatings Technology. 2006. №201. P. 3016–3029.
- Spallation-resistant thermal barrier coating: pat. 9506140 US; publ. 29.11.16.
- Ceramic thermal barrier coating system with two ceramic layers: pat. 2385155 EP; publ. 24.06.15.
- Thermal barrier coatings with low thermal conductivity: pat. 6730422 US; publ. 04.05.04.
- Thermal barrier coating having low thermal conductivity: pat. 6764779 US; publ. 20.07.04.
- Article métallique ayant une couche formant barriére thermique et procédé pour sa fabrication: pat. 0902104 EP; publ. 27.12.00.
- High temperature insulative coating (XTR): pat. 2007087210 US; publ. 19.04.07.
- Thermal barrier coating material, thermal barrier member, and member coated with thermal barrier and method for manufacturing the same: pat. 7859100 US; publ. 28.12.10.
- Thermal barrier coating system and method of manufacturing the same: pat. 7785671 US; publ. 31.08.10.
- Method of applying a thermal barrier coating: pat. 8986792 US; publ. 24.03.15.
- Chubarov D.A., Budinovskij S.A. Vybor keramicheskogo materiala dlya teplozashhitnyh pokrytij lopatok aviacionnyh turbin na rabochie temperatury do 1400°C [Choosing ceramic materials for thermal barrier coating of GTE turbine blades on working temperatures up to 1400°С] // Trudy VIAM : elektron. nauch.-tehnich. zhurn. 2015. №4. St. 07. Available at: http://viam-works.ru (accessed: January 09, 2018). DOI: 10.18577/2307-6046-2015-0-4-7-7.