Mechanical properties of aluminium-matrix composite materials reinforced with SiC particles, depending on the matrix alloy (review)
Stoyakina E.A., Kurbatkina E.I., Simonov V.N., Kosolapov D.V., Gololobov A.V. Mechanical properties of aluminium-matrix composite materials reinforced with SiC particles, depending on the matrix alloy (review) // Proceedings of VIAM. 2018. No. 2. DOI: 10.18577/2307-6046-2018-0-2-8-8. URL: https://www.viam-works.ru/en/journal/2018/2/8
Keywords
alumo-matrix composite material, aluminum alloy, matrix alloy, mechanical properties, silicon carbide, hardening particles.
Abstract
The paper reviews the mechanical properties of existing low-filled alumo-matrix composite materials with matrices of aluminum alloys 6XXX (6061, 6063, 6092), 2XXX (2024, 2009), 7XXX (7075, 7050) series and different percentages of silicon carbide hardening particles. The dependence of the change in properties is shown with a change in the percentage content of hardening particles in aluminum-matrix composite materials with different matrix alloys. It is shown that aluminum composites with matrix aluminum alloys 7XXX series have maximal mechanical characteristics. The chemical and phase compositions of matrix alloys are considered. Also, details and constructions, which are made of alumo-matrix composite materials, are considered.
Reference list
- Kablov E.N. Aviacionnoe materialovedenie v XXI veke. Perspektivy i zadachi [Aviation materials science in the XXI century. Perspectives and tasks] // Aviacionnye materialy. Izbrannye trudy «VIAM» 1932–2002. M.: MISIS–VIAM, 2002. S. 23–47.
- Kablov E.N. Osnovnye itogi i napravleniya razvitiya materialov dlya perspektivnoj aviacionnoj tehniki [The main results and the directions of development of materials for perspective aviation engineering] // 75 let. Aviacionnye materialy. Izbrannye trudy «VIAM» 1932–2007. M.: VIAM, 2007. S. 20–26.
- Alyuminievye splavy v aviakosmicheskoj tehnike / pod obshh. red. E.N. Kablova [Aluminum alloys in aerospace equipment / gen. ed. by E.N. Kablov]. M.: Nauka, 2001. 192 s.
- Kablov E.N. Materialy novogo pokoleniya [Materials of new generation] // Zashhita i bezopasnost. 2014. №4. S. 28–29.
- Duyunova V.A., Volkova E.F., Uridiya Z.P., Trapeznikov A.V. Dinamika razvitiya magnievyh i litejnyh alyuminievyh splavov [Dynamics of the development of magnesium and cast aluminum alloys] // Aviacionnye materialy i tehnologii. 2017. №S. S. 225–241. DOI: 10.18577/2071-9140-2017-0-S-225-241.
- Prusov E.S., Panfilov A.A., Kechin V.A. Perspektivy primeneniya alyumomatrichnyh kompozicionnyh splavov v mashinostroenii [Perspectives of application of alyumomatrichny composition alloys in mechanical engineering] // Litejshhik Rossii. 2012. №9. S. 16–19.
- Berezovskij V.V., Shavnev A.A., Lomov S.B., Kurganova Yu.A. Poluchenie i analiz struktury dispersno-uprochnennyh kompozicionnyh materialov sistemy Al–SiC s razlichnym soderzhaniem armiruyushhej fazy [Receiving and the analysis of structure of the disperse strengthened composite materials of Al–SiC system with the different maintenance of the reinforcing phase] // Aviacionnye materialy i tehnologii. 2014. №S6. S. 17–23. DOI: 10.185577/2071-9140-2014-0-S6-17-23.
- Grashhenkov D.V. Strategiya razvitiya nemetallicheskih materialov, metallicheskih kompozicionnyh materialov i teplozashhity [Strategy of development of non-metallic materials, metal composite materials and heat-shielding] // Aviacionnye materialy i tehnologii. 2017. №S. S. 264–271. DOI: 10.18577/2071-9140-2017-0-S-264-271.
- Kablov E.N., Shchetanov B.V., Grashhenkov D.V., Shavnev A.A., Nyafkin A.N. Metallomatrichnye kompozicionnye materialy na osnove Al–SiC [Metalmatrix composite materials on the basis of Al–SiC] // Aviacionnye materialy i tehnologii. 2012. №S. S. 373–380.
- Polmear I.J. Light Alloys: Metallurgy of the Light Metals. John Wiley & Sons, Australia, 1995. 235 p.
- Cottu J.-P., Couderc J.-J., Viguier B., Bernard L. Influence of SiC reinforcement on precipitation and hardening of a metal matrix composite // Journal of Materials Science. 1992. Vol. 27. No. 11. P. 3068–3074.
- Sidorov D.V., Shherbakova G.I. Vysokotehnologichnye komponenty kompozicionnyh materialov i specialnye volokna dlya shirokogo spektra primeneniya [Hi-tech components of composite materials and special fibers for application broad spectrum] // Himicheskaya tehnologiya. 2016. T. 17. №4. S. 183–192.
- Kablov E.N. Innovacionnye razrabotki FGUP «VIAM» GNC RF po realizacii «Strategicheskih napravlenij razvitiya materialov i tehnologij ih pererabotki na period do 2030 goda» [Innovative developments of FSUE «VIAM» SSC of RF on realization of «Strategic directions of the development of materials and technologies of their processing for the period until 2030»] // Aviacionnye materialy i tehnologii. 2015. №1 (34). S. 3–33. DOI: 10.18577/2071-9140-2015-0-1-3-33.
- Knowles A.J., Jiang X., Galano M., Audebert F. Microstructure and mechanical properties of 6061 Al alloy based composites with SiC nanoparticles // Journal of Alloys and Compounds. 2014. Vol. 615. P. S401–S405.
- Yao X., Zheng Y.F., Liang J.M. Microstructures and tensile mechanical properties of an ultrafine grained AA6063–5vol% SiC metal matrix nanocomposite synthesized by powder metallurgy // Materials Science and Engineering: A. 2015. Vol. 648. Р. 225–234.
- Alyuminievye kompozicionnye materialy [Aluminum composite materials]. Available at: http:www.dwa-usa.com (accessed: January 18, 2018).
- Li P.B., Chen T.J., Qin H. Effects of mold temperature on the microstructure and tensile properties of SiC p/2024 Al-based composites fabricated via powder thixoforming // Materials & Design. 2016. Vol. 112. P. 34–45.
- Erdemir F., Canakci A., Varol T. Microstructural characterization and mechanical properties of functionally graded Al2024/SiC composites prepared by powder metallurgy techniques // Transactions of Nonferrous Metals Society of China. 2015. Vol. 25. P. 3569–3577.
- Liu P., Wang A., Xie J., Hao S. Characterization and evaluation of interface in SiCp/2024 Al composite // Transactions of Nonferrous Metals Society of China. 2015. Vol. 25. P. 1410−1418.
- Majzoobi G.H., Atrian A., Bakhtiari H. Evaluation of mechanical properties of Al7075/SiC Nanocomposite Fabricated by Hot Uniaxial Pressing // Proceeding of the 5th International Conference on Nanostructures (ICNS5). March 2014. Available at: http://www.academia.edu/27325070/Evaluation_of_Mechanical_Properties_of_Al7075_SiC_Nanocomposite_Fabricated_by_Hot_Uniaxial_Pressing (January 23, 2018).