Polymeric sound-absorbing material design for environmental noise abatement of aircraft engines
Shuldeshov Е.М., Kraev I.D., Petrova A.P. Polymeric sound-absorbing material design for environmental noise abatement of aircraft engines // Proceedings of VIAM. 2018. No. 2. DOI: 10.18577/2307-6046-2018-0-2-6-6. URL: https://www.viam-works.ru/en/journal/2018/2/6
Keywords
sound-absorbing material design, factor of sound absorption, water repellency, porous material.
Abstract
In this article questions of noise abatement of civil air vehicles, being actual in the light of toughening of requirements for environmental noise, are considered. The way of improvement of mass and acoustic characteristics of NDC through application of sound-absorbing material design (instead of glass-fiber-reinforced honeycomb) with a porous insert characterized by the preset thickness and located at a certain height is offered. The manufacturing technology of similar materials as well as characteristics of the produced material are shortly described.
Reference list
- Kopev V.F., Munin A.G., Ostrikov N.N. Problemy sozdaniya perspektivnyh magistralnyh samoletov, sposobnyh udovletvoryat normam IKAO po shumu na mestnosti [Problems of creation of the perspective main airplanes, capable to satisfy to norms of ICAO on noise on the district] // Trudy CAGI. 2014. №2739. S. 3.
- Kablov E.N. Iz chego sdelat budushhee? Materialy novogo pokoleniya, tehnologii ih sozdaniya i pererabotki – osnova innovacij [Of what to make the future? Materials of new generation, technology of their creation and processing – basis of innovations] // Krylya Rodiny. 2016. №5. S. 8–18.
- Kablov E.N. Innovacionnye razrabotki FGUP «VIAM» GNC RF po realizacii «Strategicheskih napravlenij razvitiya materialov i tehnologij ih pererabotki na period do 2030 goda» [Innovative developments of FSUE «VIAM» SSC of RF on realization of «Strategic directions of the development of materials and technologies of their processing for the period until 2030»] // Aviacionnye materialy i tehnologii. 2015. №1 (34). S. 3–33. DOI: 10.18577/2071-9140-2015-0-1-3-33.
- Kablov E.N. Materialy novogo pokoleniya [Materials of new generation] // Zashhita i bezopasnost. 2014. №4. S. 28–29.
- Petrovа A.P., Dementyevа L.A., Lukina N.F., Chursova L.V. [Adhesive binders for polymer composite materials based on carbon- and glass fillers] // Trudy VIAM: elektron. nauch.-tehnich. zhurn. 2015. №9. St. 11. Available at: http://www.viam-works.ru (accessed: December 11, 2017). DOI: 10.18577/2307-6046-2015-0-9-11-11
- Lukina N.F., Petrova A.P., Muhametov R.R., Kogtjonkov A.S. Novye razrabotki v oblasti kleyashhih materialov aviacionnogo naznacheniya [New developments in the field of adhesive aviation materials] // Aviacionnye materialy i tehnologii. 2017. №S. S. 452–459. DOI: 10.18577/2071-9140-2017-0-S-452-459.
- Zhelezina G.F., Shuldeshova P.M. Konstrukcionnye organoplastiki na osnove plenochnyh kleev [Influence of range of high-intensity source of sound on sound-proof properties of facings of resonance type] // Klei. Germetiki. Tehnologii. 2014. №2. S. 9–14.
- Nefedov N.I., Haskov M.A., Petrova A.P., Buznik V.M. Issledovanie termicheskih svojstv ftorparafinov i gidrofobnyh pokrytij na ih osnove [Study of the thermal properties of fluorinated paraffins and hydrophobic coatings on their base] // Trudy VIAM: elektron. nauch.-tehnich. zhurnal. 2017. №2. St. 11. Available at: http://www.viam-works.ru (accessed: December 11, 2017). DOI: 10.18577/2307-6046-2017-0-2-11-11.
- Kucherovskij A.I., Shul'deshova P.M., Zhelezina G.F., Gulyaev I.N. Razrabotka sistemy zashhity setchatoj konstrukcii fyuzelyazha ot negativnyh vozdejstvij vneshnih faktorov [Constructional organoplasty on the basis of film glues] // Vse materialy. Enciklopedicheskij spravochnik. 2016. №9. S. 29–35.
- Shuldeshova P.M., Zhelezina G.F. Vliyanie atmosfernyh uslovij i zapylennosti sredy na svojstva konstrukcionnyh organoplastikov [An influence of atmospheric condition and dust loading on properties of structural organic plastics] // Aviacionnye materialy i tehnologii. 2014. №1. S. 64–68. DOI: 10.18577/2071-9140-2014-0-1-64-68.
- Sobolev A.F., Ushakov V.G., Filippova R.D. Zvukopogloshhayushhie konstrukcii gomogennogo tipa dlya kanalov aviacionnyh dvigatelej [Sound-proof designs of homogeneous type for channels of aircraft engines] // Akusticheskij zhurnal. 2009. T. 55. №6. S. 749–759.
- Platonov M.M., Zhelezina G.F., Nesterova T.A. Poristovoloknistye polimernye materialy dlya izgotovleniya shirokodiapazonnyh ZPK i issledovanie ih akusticheskih svojstv [Porous fibrous polymer materials for wide range sound absorbing structures and investigation of their acoustical properties] // Trudy VIAM: elektron. nauch-tehnih. zhurn. 2014. №6. St. 09. Available at: http://viam-works.ru (accessed: December 11, 2017). DOI: 10.18577/2307-6046-2014-0-6-9-9.
- Shuldeshova P.M., Zhelezina G.F., Soloveva N.A., Shuldeshov E.M. Aramidnye organoplastiki dlya zvukopogloshhayushhih konstrukcij [Aramide organoplasty for sound-proof designs] // Voprosy materialovedeniya. 2016. №4. S. 42–49.
- Shashkeev K.A., Shuldeshov E.M., Popkov O.V., Kraev I.D., Yurkov G.Yu. Poristye zvukopogloshhayushhie materialy (obzor) [Porous sound-absorbing materials (review)] // Trudy VIAM: elektron. nauch.-tehnich. zhurn. 2016. №6. St. 06. Available at: http://www.viam-works.ru (accessed: December 11, 2017). DOI: 10.18577/2307-6046-2016-0-6-6-6.
- Polimernyj zvukopogloshhayushhij material i sposob izgotovleniya: pat. 2612674 Ros. Federaciya [Polymeric sound-proof material and way of manufacturing: pat. 2612674 Rus. Federation]; opubl. 13.03.17.
- Obrazcova E.P., Kraev I.D., Shuldeshov E.M., Yurkov G.Yu. Gibridnye funkcionalnye materialy, sochetayushhie v sebe zvukopogloshhayushhie i radiopogloshhayushhie svojstva [The hybrid functional materials combining sound-proof and radio absorbing properties] // Materialovedenie. 2016. №12. S. 19–24.
- Ipatov M.S., Ostroumov M.N., Sobolev A.F. Vliyanie spektra vysokointensivnogo istochnika zvuka na zvukopogloshhayushhie svojstva oblicovok rezonansnogo tipa [Influence of range of high-intensity source of sound on sound-proof properties of facings of resonance type] // Akusticheskij zhurnal. 2012. T. 58. №4. S. 465–472.