The features of the grains size changing in the P/M Ni-base superalloy for disks application produced via different technologies

Bakradze M.M., Volkov A.M., Shestakova A.A., Letnikov M.N., Bubnov M.V.
Bakradze M.M., Volkov A.M., Shestakova A.A., Letnikov M.N., Bubnov M.V. The features of the grains size changing in the P/M Ni-base superalloy for disks application produced via different technologies // Proceedings of VIAM. 2018. No. 2. DOI: 10.18577/2307-6046-2018-0-2-1-1. URL: https://www.viam-works.ru/en/journal/2018/2/1
Abstract

The processes of grain growth in the Ni-base superalloy are reviewed. The powder was produced via argon atomization and plasma rotating electrode process. The changing of grain size during solution treatment with various temperatures directly after hot isostatic pressing (HIP) and also after isothermal forging of the compacted material are analyzed. It is shown that grains of the material from argon atomization powder grow slower in comparison with the material from PREP-powder. More intensive grain growth during the increase of solutioning temperature is observed in the case of additional plastic deformation of the compacted material.

Reference list
  1. Kablov E.N. Innovacionnye razrabotki FGUP «VIAM» GNC RF po realizacii «Strategicheskih napravlenij razvitiya materialov i tehnologij ih pererabotki na period do 2030 goda» [Innovative developments of FSUE «VIAM» SSC of RF on realization of «Strategic directions of the development of materials and technologies of their processing for the period until 2030»] // Aviacionnye materialy i tehnologii. 2015. №1 (34). S. 3–33. DOI: 10.18577/2071-9140-2015-0-1-3-33.
  2. Kablov E.N. Aviacionnoe materialovedenie v XXI veke. Perspektivy i zadachi [Aviation materials science in the XXI century. Perspectives and tasks] // Aviacionnye materialy. Izbrannye trudy VIAM 1932–2002: yubil. nauch.-tehnich. sb. M.: MISIS–VIAM, 2002. S. 23–47.
  3. Kablov E.N., Ospennikova O.G., Lomberg B.S. Kompleksnaya innovacionnaya tehnologiya izotermicheskoj shtampovki na vozduhe v rezhime sverhplastichnosti diskov iz superzharoprochnyh splavov [Complex innovative technology of isothermal punching on air in mode of superplasticity of disks from superhot strength alloys] // Aviacionnye materialy i tehnologii. 2012. №S. S. 129–141.
  4. Ponomarenko D.A., Moiseev N.V., Skugorev A.V. Shtampovka diskov GTD iz zharoprochnykh splavov na izotermicheskikh pressakh [Punching of disks GTD from hot strength alloys on isothermal presses] // Aviacionnye materialy i tekhnologii. 2013. №1. S. 13–16.
  5. Bubnov M.V., Sidorov S.A., Bazhenov A.R., Chebotareva E.S. Razvitie teorii i praktiki proizvodstva shtampovok diskov GTD iz geterofaznyh zharoprochnyh nikelevyh splavov [Development of the theory and practice of production of punchings of disks of from gas turbine engines of heterophase nickel-based superalloys] // Novosti materialovedeniya. Nauka i tehnika: elektron. nauch.-tehnich. zhurn. 2017. №2 (26). St. 02. Available at: http://materialsnews.ru (February 02, 2018).
  6. Garibov G.S., Vostrikov A.V., Gric N.M., Fedorenko E.A. Razrabotka novyh granulirovannyh zharoprochnyh nikelevyh splavov dlya proizvodstva diskov i valov aviacionnyh dvigatelej [Development of new granulated heat-resistant nickel alloys for the production of disks and shafts of aircraft engines] // Tehnologiya legkih splavov. 2010. №2. S. 34–43.
  7. Garibov G.S. Perspektivy razvitiya otechestvennyh diskovyh granuliruemyh zharoprochnyh nikelevyh splavov dlya novyh obrazcov aviacionnoj tehniki [Problems of application of the granulated alloy in advanced gas turbine engines] // Tehnologiya legkih splavov. 2017. № 1. S. 7–28.
  8. Nozhnickij Yu.A. Problemy primeneniya granuliruemyh splavov v perspektivnyh GTD [Problems of application of the granulated alloy in advanced GTE] // Tehnologiya legkih splavov. 2007. №4. S. 13–20.
  9. Furrer D., Fecht H. Ni-Based Superalloys for Turbine Discs // Journal of Metals. 1999. Vol. 51. P. 14–17.
  10. Pollock T., Tin S. Nickel-Based Superalloys for Advanced Turbine Engines: Chemistry, Microstructure and Properties // Journal of Propulsion and Power. 2006. Vol. 22. No 2. P. 361–374.
  11. Fatkullin O.H., Eremenko V.I., Kolesnikov Yu.N. Osobennosti formirovaniya struktury v processe deformacii i termicheskoj obrabotki granuliruemogo splava EP741NP [Features of structure formation during deformation and heat treatment of granulated alloy EP741NP] // Tehnologiya legkih splavov. 1991. № 12. S. 71.
  12. Fatkullin O.H., Eremenko V.I., Vlasova O.N., Sklyarenko V.G. Povyshenie plastichnosti (vplot do sverhplastichnosti) granuliruemyh zharoprochnyh nikelevyh splavov [Increase of plasticity (up to superplasticity) of granulated heat-resistant nickel alloys] // Tehnologiya legkih splavov. 2002. №4. S. 105–118.
  13. Beresnev A.G., Logunov A.V., Logacheva A.I. Problemy povysheniya kachestva zharoprochnyh splavov, poluchaemyh metodom metallurgii granul [Problems of improving the quality of heat-resistant alloys produced by the method of metallurgy granules] // Vestnik MAI. 2008. T. 15. S. 83–89.
  14. Razuvaev E.I., Bubnov M.V., Bakradze M.M., Sidorov S.A. GIP i deformatsiia granulirovannykh zharoprochnykh nikelevykh splavov [HIP and deformation of the granulated heat resisting nickel alloys] // Aviatsionnye materialy i tekhnologii. 2016. №S1. S. 80–86. DOI: 10.18577/2071-9140-2016-0-S1-80-86.
  15. Evgenov A.G., Nerush S.V., Vasilenko S.A. Poluchenie i oprobovanie melkodispersnogo metallicheskogo poroshka vysokohromistogo splava na nikelevoj osnove primenitelno k lazernoj LMD-naplavke [The obtaining and testing of the fine-dispersed metal powder of the high-chromium alloy on nickel-base for laser metal deposition] // Trudy VIAM: elektron. nauch.-tehnich. zhurn. 2014. №5. St. 04. Available at: http://www.viam-works.ru (accessed: February 02, 2018). DOI: 10.18577/2307-6046-2014-0-5-4-4.
  16. Davydov A.K., Kononov S.A., Baturin A.I., Fatkullin O.X. Proizvodstvo turbinnyh diskov po tehnologii metallurgii granul [Production of turbine disks on technology of metallurgy of granules] // Kuznechno-shtampovochnoe proizvodstvo. Obrabotka materialov davleniem. 2008. №5.S. 21–22.
  17. Ospennikova O.G., Lomberg B.S., Moiseev N.V., Kapitanenko D.V. Izotermicheskaya deformaciya zharoprochnyh splavov [Isothermal deformation of heat-resistant alloys] // Metallurg. 2013. №10. S. 88–92.
  18. Volkov A.M., Vostrikov A.V. Obrazovanie i rost zeren v diskovyh granuliruemyh zharoprochnyh nikelevyh splavah [Nucleation and growth of grains in P/M Ni-base superalloys for disks application] // Novosti materialovedeniya. nauka i tehnika: elektron. nauch.-tehnich. zhurn. 2017. №2. (26). St. 01. Available at: http://materialsnews.ru (February 02, 2018).
  19. Wegmann G., Gerling R., Schimansky F. Temperature induced porosity in hot isostatically pressed gamma titanium aluminide alloy powders // Acta Materialia. 2003. Vol. 51. Issue 3. P. 741–752.