Features and properties of solvent-free PMR-type polyimide resin

Zharinov M.A., Shimkin A.A., Akhmadieva K.R., Zelenina I.V.
Zharinov M.A., Shimkin A.A., Akhmadieva K.R., Zelenina I.V. Features and properties of solvent-free PMR-type polyimide resin // Proceedings of VIAM. 2018. No. 12. DOI: 10.18577/2307-6046-2018-0-12-46-53. URL: https://www.viam-works.ru/en/journal/2018/12/5
Keywords
polymer resins, polyimides, PMR-type polyimide resins, high-temperature carbon reinforced plastics, solvent-free binders, polymer matrix, thermal analysis, physical mechanical properties.
Abstract

Today among most widely used polymer resins for high-temperature composites are polyimide resins. Despite the significant successes achieved over recent decades in the field of optimization of polymerization type polyimide resin compositions, the problems of improving the processability, as well as increasing the working temperature and strength values remain urgent pressing.

The objects of the research are solvent-free polymerization type polyimide resin VS-51 (TU 1-595-12-1682-2017) developed in FSUE “VIAM” and carbon reinforced plastic. Selected monomers and synthetic conditions allowed us to achieve near solvent-free imide-forming mixture of components. The use of ethyl alcohol as a component makes it possible to significantly reduce the toxicity of polyimide resin VS-51. It should also be noted that due to the increased concentration of the  resin, the shelf life at -10 °C increases to at least 6 months.

Properties of the cured resin samples are investigated by thermal analysis. The glass transition temperature is 363 °C, the onset temperature of intensive thermal-oxidative degradation is 514 °C, and the mass loss at 500 °C is 3.0%. The heat resistance of cured resin is at the level of foreign and domestic analogues. Samples of carbon reinforced plastic based on the VTkU-2.200 carbon fabric were manufactured and investigated. Samples of carbon reinforced plastic are characterized by the following values of physical parameters: density 1.575-1.592 g/cm3; binder content 36-39%, porosity 0.4-0.6%.

The heat resistance of the obtained samples of carbon reinforced plastic was evaluated using DMA method. The glass transition temperature was 377 ° C, the temperature of the peak of the tangent of the angle of mechanical loss – 409 ° C.

Reference list
  1. Kablov E.N. Materialy i tekhnologii VIAM dlya «Aviadvigatelya» [Materials and technologies of VIAM for «Aviadvigatel»] // Permskiye aviatsionnyye dvigateli. 2014. №31. S. 43–47.
  2. Mikhaylin Yu.A. Tekhnologicheskiye i ekspluatatsionnyye kharakteristiki poliimidnykh svyazuyushchikh, prepregov i imidoplastov tipa PMR (obzor) [Technological and operational characteristics of polyimide binders, prepregs and imidoplast type PMR (review)] // Plasticheskiye massy. 1984. №3. S. 17–23.
  3. Preparation of polyimides from mixtures of monomeric diamines and esters of polycarboxylic acids: pat. US 3745149; field 29.09.71; publ. 10.07.73.
  4. Wilson D. PMR-15 Processing, Properties and Problems – a Review // British Polymer Journal 1988. No. 20. P. 405–416.
  5. Zheleznyak V.G., Muhametov R.R., Chursova L.V. Issledovanie vozmozhnosti sozdaniya termoreaktivnogo svyazujushhego na rabochuju temperaturu do 400°C [Study of possibility of thermoset binder creation for operating temperature up to 400°C] // Aviacionnye materialy i tehnologii. 2013. №S2. S. 58–61.
  6. Kablov E.N. Innovacionnye razrabotki FGUP «VIAM» GNC RF po realizacii «Strategicheskih napravlenij razvitiya materialov i tehnologij ih pererabotki na period do 2030 goda» [Innovative developments of FSUE «VIAM» SSC of RF on realization of «Strategic directions of the development of materials and technologies of their processing for the period until 2030»] // Aviacionnye materialy i tehnologii. 2015. №1 (34). S. 3–33. DOI: 10.18577/2071-9140-2015-0-1-3-33.
  7. Gulyaev I.N., Vlasenko F.S., Zelenina I.V., Raskutin A.E. Napravleniya razvitiya termostojkih ugleplastikov na osnove poliimidnyh i geterociklicheskih polimerov [Development Directions of heat-resistant carbon–fiber–reinforced–plastics based on polimide and heterocyclic polymers] // Trudy VIAM: elektron. nauch.-tehni. zhurn. 2014. №1. St. 04. Available at: http://www.viam-works.ru (accessed: November 23, 2018). DOI: 10.18577/2307-6046-2014-0-1-4-4.
  8. Mikhaylin Yu.A. Termoustoychivyye polimery i polimernyye materialy [Heat-resistant polymers and polymeric materials]. SPb.: Professiya, 2006. 624 s.
  9. Muhametov R.R., Dolgova E.V., Merkulova Yu.I., Dushin M.I. Razrabotka bismaleimidnogo termostoikogo svyazuiushchego dlya kompozitsionnyh materialov aviacionnogo naznacheniya [Development of heat-resistant bismaleimide binder for composites for aeronautical application] // Aviacionnye materialy i tehnologii. 2014. №4 (33). S. 53–57. DOI: 10.18577/2071-9140-2014-0-4-53-57.
  10. Kablov E.N., Chursova L.V., Babin A.N., Mukhametov R.R., Panina N.N. Razrabotki FGUP «VIAM» v oblasti rasplavnykh svyazuyushchikh dlya polimernykh kompozitsionnykh materialov [Developments of FSUE «VIAM» in the field of melt binders for polymer composite materials] // Polimernye materialy i tekhnologii. 2016. T. 2. №2. S. 37–42.
  11. Guseva M.A. Cianovye efiry – perspektivnye termoreaktivnye svyazujushhie (obzor) [Cyanic esters are prospective thermosetting binders (review)] // Aviacionnye materialy i tehnologii. 2015. №2 (35). S. 45–50.
  12. Pater R.H. The 316 C and 371 C composite properties of an improved PMR polyimide: LaRC-RP46 // The 36th International SAMPE Symposium and Exhibition. San Diego, CA. 1991. R. 15–18.
  13. Low toxicity high temperature PMR polyimides: pat. US 5171822 A; field 11.02.92; publ. 15.12.92.
  14. Low-toxcity, High-Temperature Polyimides: pat. US 6184333 B1; field 15.01.99; publ. 06.02.01.
  15. Kuznetsov A.A., Semenova G.K. Perspektivnyye vysokotemperaturnyye termoreaktivnyye cvyazuyushchiye dlya polimernykh kompozitsionnykh materialov [Perspective high-temperature thermosetting binders for polymer composite materials] // Rossiyskiy khimicheskiy zhurnal. 2010. T. 53. №4. S. 86–96.