Features of structure and property of alloys on the basis of Ni3Al intermetallic compound, half-scientists method SLM

Evgenov A.G., Bazyleva O.A., Golovlev N.A., Zaysev D.V.
Evgenov A.G., Bazyleva O.A., Golovlev N.A., Zaysev D.V. Features of structure and property of alloys on the basis of Ni3Al intermetallic compound, half-scientists method SLM // Proceedings of VIAM. 2018. No. 12. DOI: 10.18577/2307-6046-2018-0-12-25-36. URL: https://www.viam-works.ru/en/journal/2018/12/3
Keywords
selective laser melting, crystallization rapidity, carbides, morphology, HIP, dendrite axes, cells.
Abstract

This paper is a work of investigating the structural features of VKNA-type Ni3Al-based alloys, made by selective laser melting (SLM) in several conditions: directly after synthesis, thermal and gas-static treated. The main features grain structure formation are shown depending on the content of carbon in the alloys. In previous scientific research it was established that crystallization for VIN5 and VKNA-1VR alloys obey the normal crystallization law. Right after the melting, matrix for VIN5 and VKNA-1VR is a g-solid solute, and dispersed pieces of the γ′-phase are uniformly distributed in the grain volume. Type VKNA25 (VKNA 25R) alloy has another crystallization mechanism: the distribution of  alloying elements changes. γ′-phase is now the matrix after synthesis.

The carbon influence and the amount of carbides on the recrystallization process and the formation of grains in the synthesized metal in the process of HIP are considered. It is shown that VKNA25 ( HIP) has practically equi-axed grain formation. Some grains contain twins, as the cause of the formation of which can be both the recrystallization process and micro strain in the process of comprehensive compression at the HIP. VKNA25 (R) has the preferred orientation of the elongated grains in the [001] direction. VIN5 and VKNA25 alloys after the HIP have the γ′-phase particles with a predominantly cubic morphology. VKNA25 (R) has irregular shapes of the γ′-phase parts.

The properties of the short-term strength of intermetallic alloys are determined in comparison with each other in different conditions (even casted). The values of the long-term strength of the synthesized materials right after melting and subsequent HIP are determined. It is shown that the long-term st

Reference list
  1. Rayevskikh A.N., Chabina E.B., Filonova Ye.V., Belova N.A. Vozmozhnosti metoda difraktsii obratnootrazhennykh elektronov (DOE/EBSD) dlya issledovaniya osobennostey struktury nikelevykh zharoprochnykh splavov, poluchennykh selektivnym lazernym splavleniyem [Electron Back Scatter Diffraction (EBSD) method possibilities for selective laser melted nickel superalloys structure features investigation] // Trudy VIAM: elektron. nauch.-tekhnich. zhurn. 2017. №12 (60). St. 12. URL: http://www.viam-works.ru (accessed: October 29, 2018). DOI: 10.18577/2307-6046-2017-0-12-12-12.
  2. Lapteva M.A., Belova N.A., Raevskih A.N., Filonova E.V. Issledovanie zavisimosti sherohovatosti, morfologii poverhnosti i kolichestva defektov struktury ot moshhnosti lazera, skorosti skanirovaniya i tipa shtrihovki v zharoprochnom splave, sintezirovannom metodom SLS [Dependence of roughness, surface morphology structure and number of defects on the power of the laser, scanning speed and the type of hatching in the high-temperature alloys synthesized by SLS] // Trudy VIAM: elektron. nauch.-tehnich. zhurn. 2016. №9. St. 09. Available at: http://www.viam-works.ru (accessed: October 29, 2018). DOI: 10.18577/2307-6046-2016-0-9-9-9.
  3. Lukina E.A., Bazaleeva K.O., Petrushin N.V., Tsvetkova E.V. Osobennosti formirovaniya struktury zharoprochnogo nikelevogo splava ZHS6K-VI pri selektivnom lazernom splavlenii [Features of the formation of the structure of the heat-resistant nickel alloy ZhS6K-VI with selective laser alloying] // Tsvetnyye metally. 2016. №3. S. 57–63. DOI: 10.17580/tsm.2016.03.09.
  4. Medvedev P.N., Treninkov I.A., Filonova E.V., Razuvaev E.I. Formirovanie kristallograficheskoy tekstury i struktury zharoprochnykh nikelevykh splavov v protsesse SLS [Formation of crystallographic texture and structure of high-temperature nickel alloys in the process of SLS] // Sb. tr. III Mezhdunar. konf. «Additivnyye tekhnologii: nastoyashcheye i budushcheye». Available at: https://elibrary.ru/item.asp?id=29034328 (accessed: January 28, 2018).
  5. Lukina E.A., Filonova E.V., Treninkov I.A. Mikrostruktura i preimushhestvennye kristallograficheskie orientirovki zharoprochnogo nikelevogo splava, sintezirovannogo metodom SLS, v zavisimosti ot energeticheskogo vozdejstviya i termoobrabotki [The microstructure and preferential crystallographic orientation of nickel superalloy, synthesized by SLM method, depending of the energy impact and heat treatment] // Aviacionnye materialy i tehnologii. 2017. №1 (46). S. 38–44. DOI: 10.18577/2071-9140-2017-0-1-38-44.
  6. Basak A., Das S. A study on the effects of substrate crystallographic orientation on microstructural characteristics of rené n5 processed through scanning laser epitaxy // Superalloys-2016: proceedings of the 13th International Symposium on Superalloys. 2016. P. 1041–1049.
  7. Zavodov A.V., Petrushin N.V., Zaytsev D.V. Mikrostruktura i fazovyy sostav zharoprochnogo splava ZhS32 posle selektivnogo lazernogo splavleniya, vakuumnoy termicheskoy obrabotki i goryachego izostaticheskogo pressovaniya [The microstructure and phase composition of the heat-resistant ZhS32 alloy after selective laser alloying, vacuum heat treatment, and hot isostatic pressing] // Pisma o materialakh. 2017. №7 (2). S. 111–116.
  8. Kablov E.N. Iz chego sdelat budushchee? Materialy novogo pokoleniya, tekhnologii ikh sozdaniya i pererabotki – osnova innovatsiy [What to make the future from? Materials of the new generation, technologies of their creation and processing - the basis of innovation] // Krylya Rodiny. 2016. №5. S. 8–18.
  9. Kablov E.N. Materialy novogo pokoleniya – osnova innovatsiy, tekhnologicheskogo liderstva i natsionalnoy bezopasnosti Rossii [Materials of the new generation - the basis of innovation, technological leadership and national security of Russia] // Intellekt i tekhnologii. 2016. №2 (14). S. 16–21.
  10. Kablov E.N. Additivnye tekhnologii – dominanta natsionalnoy tekhnologicheskoy initsiativy [Additive technologies – the dominant of the national technology initiative] // Intellekt i tekhnologii. 2015. №2 (11). S. 52–55.
  11. Evgenov A.G., Bazyleva O.A., Korolev V.A., Arginbaeva E.G. Perspektivy primeneniya splava na osnove intermetallida Ni3Al tipa VKNU-4UR v additivnykh tekhnologiyakh [Prospects of Ni3Al-based intermetallic alloy VKNA-4UR application in additive technologies] // Aviacionnyye materialy i tehnologii. 2016. №S1 (43). S. 31–35. DOI: 10.18577/2071-9140-2016-0-S1-31-35.
  12. Raevskikh A.N., Petrushin N.V., Chabina E.B. Issledovanie struktury splava ZhS32, poluchennogo metodom selektivnogo lazernogo splavleniya, posle vysokotemperaturnykh mekhanicheskikh ispytaniy [Investigation of the structure of the alloy ZhS32, obtained by the method of selective laser alloying, after high-temperature mechanical tests] // Sb. tr. IV Mezhdunar. konf. «Additivnye tekhnologii: nastoyashchee i budushchee». M., 2018. S. 307–320.
  13. Evgenov A.G., Gorbovec M.A., Prager S.M. Struktura i mehanicheskie svojstva zharoprochnyh splavov VZh159 i EP648, poluchennyh metodom selektivnogo lazernogo splavleniya [Structure and mechanical properties of heat resistant alloys VZh159 and EP648, prepared by selective laser fusing] // Aviacionnye materialy i tehnologii. 2016. №S1. S. 8–15. DOI: 10.18577/2071-9140-2016-0-S1-8-15.
  14. Kablov E.N. Innovacionnye razrabotki FGUP «VIAM» GNC RF po realizacii «Strategicheskih napravlenij razvitiya materialov i tehnologij ih pererabotki na period do 2030 goda» [Innovative developments of FSUE «VIAM» SSC of RF on realization of «Strategic directions of the development of materials and technologies of their processing for the period until 2030»] // Aviacionnye materialy i tehnologii. 2015. №1 (34). S. 3–33. DOI: 10.18577/2071-9140-2015-0-1-3-33.
  15. Evgenov A.G., Korolev V.A., Shurtakov S.V. Perspektivy razrabotki vysokoproizvoditelnykh rezhimov selektivnogo lazernogo splavleniya zharoprochnykh splavov na osnove nikelya dlya izgotovleniya detaley GTD [Prospects for the development of high-performance modes of selective laser alloying of superalloy based on nickel for the manufacture of parts of the gas turbine engine] // Sb. tr. III Mezhdunar. konf. «Additivnye tekhnologii: nastoyashchee i budushchee». M., 2017. S. 23.
  16. Zhou X., Zhong Y., Shen Zh., Liu W. The surface-tansion-driven Benard conventions and unique sub-grain cellular microstructures in 316L steel selective laser melting // Applied Physics, Materials Science. January, 2018. P. 32. Available at: https://arXiv:1801.01408v1 (accessed: October 9, 2018).
  17. Flemings M. Protsessy zatverdevaniya [Processes of solidification]. M.: Mir, 1977. 423 s.
  18. Lukina E.A., Orlov M.R., Filonova E.V., Treninkov I.A., Zaytsev D.V. Issledovanie strukturno-fazovogo sostoyaniya zharoprochnykh nikelevykh splavov v protsesse selektivnogo lazernogo splavleniya [Investigation of the structural-phase state of high-temperature nickel alloys in the process of selective laser alloying] // Sb. dokladov III Vseros. nauch.-tekhnich. konf. «Rol fundamentalnykh issledovaniy pri realizatsii «Strategicheskikh napravleniy razvitiya materialov i tekhnologiy ikh pererabotki na period do 2030 goda». M.: VIAM, 2016. S. 22.