Investigation of the effect of surface preparation and ion-assisted deposition on the structure and properties of erosion-resistant ion-plasma coating

Aleksandrov D.A., Muboyadzhyan S.A., Juravleva P.L., Gorlov D.S.
Aleksandrov D.A., Muboyadzhyan S.A., Juravleva P.L., Gorlov D.S. Investigation of the effect of surface preparation and ion-assisted deposition on the structure and properties of erosion-resistant ion-plasma coating // Proceedings of VIAM. 2018. No. 10. DOI: 10.18577/2307-6046-2018-0-10-62-73. URL: https://www.viam-works.ru/en/journal/2018/10/8
Keywords
ion-plasma coatings, erosion-resistant coatings, ion-assisted deposition, coating for compressor blades.
Abstract

In this article, we investigated the influence of methods for preparing the sample surface before coating on the resistance to erosive wear of an ion-plasma coating of zirconium nitride. The effect on the structure of the zirconium nitride and erosion resistance of the compositions of «alloy–coating» assisted deposition, as well as the direction of rotation of the cathode spots of the vacuum arc along the annular trajectory on the surface of the cylindrical cathode is shown compared to the direction of rotation of the processed products on the planetary drive of the MAP-3 for ion-plasma coatings. The phase composition of the coatings were studied, the lattice periods and the size of coherent scattering regions, the magnitude of residual stresses were determined, and the erosion-wear resistance of «alloy–coating» compositions was tested. The influence of the studied process parameters on the erosion resistance of the ion-plasma coating of zirconium nitride has been established.

Reference list
  1. Kablov E.N., Ospennikova O.G., Petrushin N.V., Visik E.M. Monokristallicheskij zharoprochnyj nikelevyj splav novogo pokoleniya s nizkoj plotnostyu [Single-crystal nickel-based superalloy of a new generation with low-density] // Aviacionnye materialy i tehnologii. 2015. №2 (35). S. 14–25. DOI: 10.18577/2071-9140-2015-0-2-14-25.
  2. Kablov E.N. Marketing materialovedeniya, aviastroeniya i promyshlennosti: nastoyashchee i budushchee [Marketing of materials science, aircraft industry and industry: present and future] // Direktor po marketingu i sbytu. 2017. №5–6. S. 40–44.
  3. Aleksandrov D.A., Muboyadzhyan S.A., Gorlov D.S. Povyshenie svojstv uprochnjajushhih ionno-plazmennyh pokrytij pri pomoshhi assistirovannogo osazhdeniya [Increasing reinforcing properties of ion-plasma coatings using plasma assisted deposition] // Trudy VIAM: elektron. nauch.-tehnich. zhurn. 2015. №7. St. 07. Available at: http://www.viam-works.ru (accessed: October 09, 2018). DOI: 10.18577/2307-6046-2015-0-7-7-7.
  4. Aleksandrov D.A., Muboyadzhyan S.A., Lutsenko A.N., Zhuravleva P.L. Uprochnenie poverkhnosti titanovykh splavov metodom ionnoj implantatsii i ionnogo modifitsirovaniya [Hardening of the surface of titanium alloys by ion implantation method and ionic modification] // Aviacionnye materialy i tehnologii. 2018. №2 (51). S. 33–39. DOI: 10.18577/2071-9140-2018-0-2-33-39.
  5. Valesa S., Brito P. Influence of substrate pre-treatments by Xe+ ion bombardment and plasma nitriding on the behavior of TiN coatings deposited by plasma reactive sputtering on 100Cr6 steel // Materials Chemistry and Physics. 2016. Vol. 177. P. 156–163.
  6. Kablov E.N. Innovacionnye razrabotki FGUP «VIAM» GNC RF po realizacii «Strategicheskih napravlenij razvitiya materialov i tehnologij ih pererabotki na period do 2030 goda» [Innovative developments of FSUE «VIAM» SSC of RF on realization of «Strategic directions of the develop-ment of materials and technologies of their processing for the period until 2030»] // Aviacionnye materialy i tehnologii. 2015. №1 (34). S. 3–33. DOI: 10.18577/2071-9140-2015-0-1-3-33.
  7. Putyrskij S.V., Arislanov A.A., Artemenko N.I., Yakovlev A.L. Razlichnye metody povysheniya iznosostojkosti titanovyh splavov i sravnitelnyj analiz ih effektivnosti primenitelno k titanovomu splavu VT23M [Different methods of wear resistance increase of titanium alloys and comparative analysis of their efficiency for VT23M titanium alloy] // Aviacionnye materialy i tehnologii. 2018. №1. S. 19–24. DOI: 10.18577/2071-9240-2018-0-1-19-24.
  8. Smyslov A.M., Dyblenko Yu.M., Smyslova M.K. i dr. Novaya vakuumnaya ustanovka i tekhnologiya kombinirovannoj uprochnyayushchej obrabotki, naneseniya pokrytij na detali GTD i energeticheskih ustanovok [The new vacuum unit and technology of the combined strengthening processing, drawing coverings on detail of GTU and energy units] // Vestnik Ufimskogo gosudarstvennogo aviatsionnogo tekhnicheskogo universiteta. 2013. T. 17. №1 (54). S. 108–113.
  9. Zhuravleva P.L., Treninkov I.A., Sbitneva S.V., Alekseev A.A., Gorlov D.S. Issledovanie struktury odnoslojnyh pokrytij TiN i mnogoslojnyh pokrytij TiN/ZrN [Research of structure of single layer coatings of TiN and multilayer coatings of TiN/ZrN] // Rossijskie nanotekhnologii. 2010. T. 5. №9–10. S. 112–116.
  10. Vasyliev V.V., Kalinichenko A.I., Reshetnyak E.N. Experimental and modeling study on the role of Ar addition to the working gas on the development of intrinsic stress in TiN coatings produced by filtered vacuum-arc plasma // Thin Solid Films. 2017. Vol. 642. P. 207–213.
  11. Latushkina S.D., Zhizhchenko A.G., Posylkina O.I. Vakuumno-dugovye karbonitridtitanovye pokrytiya, osazhdennye iz separirovannyh plazmennyh potokov [The vacuum and arc karbonitridtitanic coverings besieged from separated plasma flows] // Elektronnaya obrabotka materialov. 2015. №4. S. 22–27.
  12. Lojko V.A., Semin E.V. Otsenka napryazhennogo sostoyaniya diskretnyh struktur uprochnyayushchih pokrytij, nanesennyh vakuumno-plazmennym napyleniem [Assessment of tension of discrete structures of the strengthening coverings put with vacuum and plasma dusting] // Vestnik Polotskogo gosudarstvennogo universiteta. Ser. V: Promyshlennost. Prikladnye nauki. 2014. №3.S. 29–34.
  13. Shekhtman S.R., Sukhova N.A. Producing multilayer composites based on metal-carbon by vacuum ion-plasma method // Journal of Physics: Conference Series. 2016. Vol. 729. P. 1–4.
  14. Vasyliev V.V., Luchaninov A.A., Reshetniak E. et al. Structure and properties of Ti–Al–Y–N coatings deposited from filtered cathodic-arc plasma in gas Ar and N2 mixture // 2017 IEEE 7th International Conference Nanomaterials: Application & Properties (NAP). 2017. DOI: 10.1109/NAP.2017.8190206.
  15. Vereschaka A.A.,Volosova M.A., Batako A.D., Vereshchaka A.S., Mokritskii B.Y. Development of wear-resistant coatings compounds for high-speed steel tool using a combined cathodic vacuum arc deposition // International Journal of Advanced Manufacturing Technology. 2016. Vol. 84. Issue 5–8. P. 1471–1482.
  16. Ovcharenko V.D., Kuprin A.S., Tolmachova G.N., Kolodiy I.V. Deposition of chromium nitride coatings using vacuum arc plasma in increased negative substrate bias voltage // Vacuum. 2015. Vol. 117. P. 27–34.
  17. Pogrebnjak A.D., Yakushchenko I.V., Bagdasaryan A.A., Bondar O.V. Microstructure, physical and chemical properties of nanostructured (Ti–Hf–Zr–V–Nb)N coatings under different deposition conditions // Materials Chemistry and Physics. 2014. Vol. 147. Issue 3. P. 1079–1091.
  18. Kosmin A.A., Budinovskij S.A., Gayamov A.M., Smirnov A.A. Zharostojkoe pokrytie dlya novogo perspektivnogo intermetallidnogo splava VIN3 [Heat-resistant coating for new intermetallic nickel-based superalloy VIN3] // Trudy VIAM: elektron. nauch.-tekhnich. zhurn. 2014. №4. St. 01. Available at: http://www.viam-works.ru (accessed: October 09, 2018). DOI: 10.18577/2307-6046-2014-0-4-1-1.
  19. Chubarov D.A., Budinovskij S.A., Smirnov A.A. Magnetronnyj sposob naneseniya keramicheskih sloev teplozashhitnyh pokrytij [Magnetron sputtering method for applying ceramic layers for thermal barrier coatings] // Aviacionnye materialy i tehnologii. 2016. №4. S. 23–30. DOI: 10.18577/2107-9140-2016-0-4-23-30.
  20. Kablov E.N., Sidorov V.V., Kablov D.E., Min P.G., Rigin V.E. Resursosberegayushchie tekhnologii vyplavki perspektivnyh litejnyh i deformiruemyh superzharoprochnyh splavov s uchetom pererabotki vsekh vidov othodov [Resource-saving smelting technologies of perspective cast and deformable superhot strength alloys taking into account processing of all types of waste] // Elektrometallurgiya. 2016. №9. S. 30–41.