Nechaykina T.A., Blinovа N.E., Ivanov A.L., Kozlova O.Yu., Kozhekin A.E. Research of the effect of homogenization and quench hardening modes on the structure and mechanical properties of retail rings from alloy V95o.ch.-T2 // Proceedings of VIAM. 2018. No. 10. DOI: 10.18577/2307-6046-2018-0-10-27-36. URL: https://www.viam-works.ru/en/journal/2018/10/4
Keywords
high-strength aluminium alloys system Al–Zn–Mg–Cu, structure, mechanical properties, rolled rings.
Abstract

The research of manufacturing parameters influence on the structure and properties of the roll rings (R≤1500 mm) made of the high-strength alloy В95o.ch.-T2 (7475 Т7351-type) was conducted. For this purpose parameters of heat treatment were varied: the soak time during homogenization (24 and 36 hours), the soak time during quench heating (150 and 200 min) and the temperature of the hardening fluid (30 and 60°С). The optimal heat treatment conditions (homogenization and quenching hardening) were determined to provide the required level of properties (σв≥470 MPa, σ0,2≥380 MPa, δ≥6%).

Reference list
  1. Fridlyander I.N., Senatorova O.G., Tkachenko Ye.A., Molostova I.I. Razvitiye i primeneniye vysokoprochnykh splavov sistemy Al–Zn–Mg–Cu dlya aviakosmicheskoy tekhniki [Development and application of high-strength alloys of the Al – Zn – Mg – Cu system for aerospace engineering] // 75 let. Aviatsionnyye materialy. Izbrannyye trudy «VIAM» 1932–2007: yubil. nauch.-tekhnich. sb. M.: VIAM, 2007. S. 155–163.
  2. Illarionov E.I., Kolobnev N.I., Gorbunov P.Z., Kablov E.N. Alyuminiyevyye splavy v aviakosmicheskoy tekhnike [Aluminum alloys in aerospace]. M.: Nauka, 2001. 192 s.
  3. Antipov V.V., Blinova N.E., Senatorova O.G. et al. Investigations of properties and structure of V95och and V96Zr-3pch. alloys during stress ageing // Proceedings of ICAA-11. 2008. P. 1864–1868.
  4. Kablov E.N. Innovacionnye razrabotki FGUP «VIAM» GNC RF po realizacii «Strategicheskih napravlenij razvitiya materialov i tehnologij ih pererabotki na period do 2030 goda» [Innovative developments of FSUE «VIAM» SSC of RF on realization of «Strategic directions of the development of materials and technologies of their processing for the period until 2030»] // Aviacionnye materialy i tehnologii. 2015. №1 (34). S. 3–33. DOI: 10.18577/2071-9140-2015-0-1-3-33.
  5. Kablov E.N. Klyuchevaya problema – materialy [Tendencies and Guidelines for the Innovative Development of Russia] // Tendentsii i oriyentiry innovatsionnogo razvitiya Rossii. M.: VIAM, 2015. S. 458–464.
  6. Fridlyander I.N. Alyuminiyevyye splavy v letatelnykh apparatakh v period 1970–2015 gg. [Aluminum alloys in aircraft in the period 1970–2015] // Tekhnologiya legkikh splavov. 2002. №4. S. 12–17.
  7. Kablov E.N., Grinevich A.V., Lutsenko A.N., Erasov V.S., Nuzhnyy G.A., Gulina I.V. Issledovaniye kinetiki razrusheniya konstruktsionnykh alyuminiyevykh splavov pri dlitelnom vozdeystvii staticheskoy nagruzki i korrozionnoy sredy s ispolzovaniyem obraztsa novogo tipa [Investigation of the kinetics of destruction of structural aluminum alloys with prolonged exposure to static load and a corrosive environment using a new type of sample] // Deformatsiya i razrusheniye materialov. 2016. №10. S. 42–48.
  8. Antipov V.V., Senatorova O.G., Tkachenko E.A., Vahromov R.O. Alyuminievye deformiruemye splavy [Aluminum deformable alloys] // Aviacionnye materialy i tehnologii. 2012. №S. S. 167–182.
  9. Antipov V.V. Perspektivy razvitiya alyuminievyh, magnievyh i titanovyh splavov dlya izdelij aviacionno-kosmicheskoj tehniki [Prospects for development of aluminium, magnesium and titanium alloys for aerospace engineering] // Aviacionnye materialy i tehnologii. 2017. №S. S. 186–194. DOI: 10.18577/2107-9140-2017-0-S-186-194.
  10. Fridlyander I.N., Senatorova O.G., Ryazanova N.A., Nikiforov A.O. Grain structure and superplasticity of strength Al–Zn–Mg–Cu alloys with different minor additions // Proceedings оf 1994 International Conference on Superplasticity in Advanced Materials (ICSAM-94). 1994. P. 345–349.
  11. Senatorova O.G., Sukhikh A.YU., Sidelnikov V.V. i dr. Razvitiye i perspektivy primeneniya vysokoprochnykh alyuminiyevykh splavov dlya katanykh polufabrikatov [Development and prospects for the use of high-strength aluminum alloys for rolled semi-finished products] // Tekhnologiya legkikh splavov. 2002. №4. S. 28–33.
  12. Milevskaya T.V., Ruschits S.V., Tkachenko E.A., Antonov S.M. Deformacionnoe povedenie vysokoprochnyh alyuminievyh splavov v usloviyah goryachej deformacii [Deformation behavior of high-strength aluminum alloys in conditions of hot deformation] // Aviacionnye materialy i tehnologii. 2015. №2 (35). S. 3–9. DOI: 10.18577/2071-9140-2015-0-2-3-9.
  13. OST1 90113–86. Profili pressovannyye iz alyuminiyevykh splavov. Tekhnicheskiye usloviya [Industry Standard 1 90113–86. Pressed profiles from aluminum alloys. Technical conditions]. M., 1987. 46 s.
  14. Kurs M.G. Prognozirovaniye prochnostnykh svoystv obshivki LA iz deformiruyemogo alyuminiyevogo splava V95o.ch.-T2 s primeneniyem integralnogo koeffitsiyenta korrozionnogo razrusheniya [Forecasting the strength properties of the skin cover of a deformable aluminum alloy В95о.ч.-Т2 with the use of the integrated corrosion reduction coefficient] // Trudy VIAM: elektron. nauch.-tehnich. zhurn. 2018. №5. St. 11Available at: http://www.viam-works.ru (accessed: October 04, 2018). DOI: 10.18577/2307-6046-2018-0-5-101-109.
  15. Kablov E.N. Iz chego sdelat budushcheye? Materialy novogo pokoleniya, tekhnologii ikh sozdaniya i pererabotki – osnova innovatsiy [What to make the future from? Materials of the new generation, technologies of their creation and processing – the basis of innovation] // Krylya Rodiny. 2016. №5. S. 8–18.
  16. GOST 4784–97. Alyuminiy i splavy alyuminiyevyye deformiruyemyye [State Standard 4784–97. Aluminum and wrought aluminum alloys]. M.: Standartinform, 2009. 15 s.
  17. Fridlyander I.N., Senatorova O.G., Novikov I.I. i dr. Sverkhplastichnost vysokoprochnykh splavov sistemy Al–Zn–Mg–Cu, legirovannykh skandiyem [Superplasticity of high-strength alloys of the Al–Zn–Mg–Cu system doped with scandium] // Tekhnologiya legkikh splavov. 1993. №7–8. S. 43–46.
  18. Fridlyander I.N. Vysokoprochnyye deformiruyemy alyuminiyevyye splavy [High strength wrought aluminum alloys]. M.: Oborongiz, 1960. S. 191–195.
  19. Beletskiy V.M., Krivov G.A. Alyuminiyevyye splavy (sostav, svoystva, tekhnologiya, primeneniye): spravochnik [Aluminum alloys (composition, properties, technology, application): handbook]. Kiev: Komintekh, 2005. S. 99.