The manufacture of the «blisk» rotor design made from bimetallic combination of materials (review)
Ospennikova O.G., Lukin V.I., Afanasev-Khodykin A.N., Galushka I.A. The manufacture of the «blisk» rotor design made from bimetallic combination of materials (review) // Proceedings of VIAM. 2018. No. 10. DOI: 10.18577/2307-6046-2018-0-10-10-16. URL: https://www.viam-works.ru/en/journal/2018/10/2
Keywords
brazing, a diffusive brazing, brazing alloy, nickel super alloys, rotor design GTE
Abstract
Considered the perspective of a GTE rotor design that called «blisk», which allows to reduce the weight and increase the efficiency of the engine. Shown the advantages and disadvantages between a «blisk» rotor design and a traditional «fir tree» rotor design. The review of technologies that can be used to manufacture a bimetallic «blisk» design from nickel based superalloys – foundry intermetallide blades and a deformable disk was made. The full scale tests of a gas turbine engine rotor, manufactured with a high temperature diffusive brazing technology were shown.
Reference list
- Lomberg B.S., Ovsepyan S.V., Bakradze M.M. Vysokozharoprochnyye deformiruyemyye nikelevyye splavy dlya perspektivnykh gazoturbinnykh dvigateley i gazoturbinnykh ustanovok [High-strength wrought nickel alloys for promising gas-turbine engines and gas-turbine installations] // Vestnik MGTU im. N.E. Baumana. Ser.: Mashinostroyeniye, 2011. SP2. S. 98–103.
- Boguslayev V.A., Muravchenko F.M., Zhemanyuk P.D., Kolesnikov V.I. Tekhnologicheskoye obespecheniye ekspluatatsionnykh kharakteristik detaley GTD [Technological support of operational characteristics of parts of the GTE]. Zaporozhe: Motor Sich, 2003. Ch. II. 396 s.
- Falaleyev S.V. Sovremennyye problemy sozdaniya dvigateley letatelnykh apparatov: elektron. ucheb. posobiye. Samara: 2012. S. 91 [Elektronnyy resurs]. Available at: https://rucont.ru/efd/230195 (accessed: September 25, 2018).
- Magerramova L.A. Primeneniye bimetallicheskikh bliskov, izgotavlivayemykh metodom GIP iz granuliruyemykh i liteynykh nikelevykh supersplavov, dlya uvelicheniya nadezhnosti i resursa gazovykh turbin [Application of bimetallic blisks manufactured by the ISU method from granulated and foundry nickel superalloys to increase the reliability and service life of gas turbines] // Vestnik UGATU. 2011. №4 (44). S. 33–38.
- Magerramova L.A., Vasilyev B.E. Bimetallicheskiye bliski turbin s bandazhirovannymi lopatkami dlya gazoturbinnykh dvigateley [Bimetallic bliski turbines with shrouded blades for gas turbine engines] // Nauka i obrazovaniye: nauchnoye izdaniye MGTU im. N.E. Baumana, 2015. №6.S. 143–156.
- Kablov E.N., Petrushin N.V., Elyutin E.S. Monokristallicheskiye zharoprochnyye splavy dlya gazoturbinnykh dvigateley [Monocrystalline superalloys for gas turbine engines] // Vestnik MGTU im. N.E. Baumana. Spets. vyp.: Perspektivnyye konstruktsionnyye materialy i tekhnologii, 2011. S. 38–52.
- Lomberg B.S., Ovsepyan S.V., Bakradze M.M., Mazalov I.S. Vysokotemperaturnye zharo-prochnye nikelevye splavy dlya detalej gazoturbinnyh dvigatelej [High-temperature heat resisting nickel alloys for details of gas turbine engines] // Aviacionnye materialy i tehnologii. 2012. №S. S. 52–57.
- Povarova K.B., Valitov V.A., Ovsepyan S.V., Drozdov A.A., Bzyleva O.A., Valitova E.V. Izucheniye svoystv i vybor splavov dlya diskov s lopatkami («bliskov») i sposoba ikh soyedineniya [Valitova, E.V. Studying the properties and the choice of alloys for disks with blades («blisks») and the method of their combination] // Metally. 2014. №5. S. 61–70.
- Magerramova L., Zakharova T., Gromov M., Samarov V. Turbiny: s «blisk»om i bez [Elektronnyy resurs]. Available at: http://engine.aviaport.ru/02page32.html (accessed: September 25, 2018).
- Kablov E.N., Petrushin N.V., Svetlov I.L., Demonis I.M. Nikelevye litejnye zharoprochnye splavy novogo pokoleniya [Nickel foundry heat resisting alloys of new generation] // Aviacionnye materialy i tehnologii. 2012. №S. C. 36–52.
- Kablov E.N., Petrushin N.V., Svetlov I.L., Demonis I.M. Liteynyye zharoprochnyye splavy novogo pokoleniya [Foundry superalloys of new generation] // 75 let. Aviatsionnyye materialy: yubil. nauch.-tekhnich. sb. M.: VIAM, 2007. S. 27–44.
- Lomberg B.S., Ovsepjan S.V., Bakradze M.M., Letnikov M.N., Mazalov I.S. Primenenie novyh deformiruemyh nikelevyh splavov dlja perspektivnyh gazoturbinnyh dvigatelej [The application of new wrought nickel alloys for advanced gas turbine engines] // Aviacionnye materialy i tehnologii. 2017. №S. S. 116–129. DOI: 10.18577/2071-9140-2017-0-S-116-129.
- Kablov E.N. Strategicheskie napravleniya razvitiya materialov i tehnologij ih pererabotki na period do 2030 goda [The strategic directions of development of materials and technologies of their processing for the period to 2030] // Aviacionnye materialy i tehnologii. 2012. №S. S. 7–17.
- Lukin V.I., Kovalchuk V.G., Ioda E.N. Svarka plavleniyem – osnova svarochnogo proizvodstva [Fusion welding is a core of welding manufacturing] // Aviacionnyye materialy i tehnologii. 2017. №S. S. 130–143. DOI: 10.18577/2071-9140-2017-0-S-130-143.
- Magerramova L.A. Achievement of bimetallic blisks integrated dissimilar alloys for promising high temperature aviation gas turbine engines. 28th International congress of the aeronautical sciences. 2012 [Elektronnyy resurs]. Available at: http://www.icas.org/ICAS_ARCHIVE/ICAS2012/PAPERS/224.PDF (accessed: September 25, 2018).
- Lyushinskiy A.V. Diffuzionnaya svarka raznorodnykh materialov: ucheb. Posobie [Diffusion welding of dissimilar materials: tutorial]. M.: Akademiya, 2006. 208 s.
- Lukin V.I., Samorukov M.L. Osobennosti formirovaniya struktury svarnykh soyedineniy zharoprochnogo deformiruyemogo splava VZH175, poluchennykh rotatsionnoy svarkoy treniyem [Features of the formation of the structure of welded joints of the heat-resistant wrought alloy VZh175, obtained by rotational friction welding] // Svarochnoye proizvodstvo. 2017. №6. S. 12–18.
- Lashko N.F., Lashko S.V. Voprosy teorii i tekhnologii payki [Questions of the theory and technology of soldering]. Saratov: Izd-vo Sarat. un-ta, 1974. 248 s.
- Lashko N.F., Lashko S.V. Payka metallov [Soldering metals]. M.: Mashinostroyeniye, 1967. 368 s.
- Petrunin I.E., Bereznikov Yu.I., Bunkina R.R. i dr. Spravochnik po payke. 3-e izd. pererab. i dop. [Handbook of soldering. 3rd ed. rev. and add.]. M.: Mashinostroyeniye-1, 2003. 480 s.
- Petrunin I.E., Markova I.Yu., Ekatova A.S. Metallovedeniye payki [Metal science soldering]. M.: Metallurgiya, 1976. 264 s.
- Lukin V.I., Rylnikov V.S., Afanasyev-Khodykin A.N. Pripoi na nikelevoy osnove dlya payki zharoprochnykh splavov i staley [Nickel-based solders for brazing high-temperature alloys and steels] // Svarochnoye proizvodstvo. 2014. №7. S. 36–42.
- Ospennikova O.G., Lukin V.I., Afanasyev-Khodykin A.N., Galushka I.A., Shevchenko O.V. Perspektivnyye razrabotki v oblasti vysokotemperaturnoy payki zharoprochnykh splavov [Advanced developments in the field of the high-temperature soldering of heat resisting alloys] // Aviacionnyye materialy i tehnologii. 2017. №S. S. 144–158. DOI: 10.18577/2071-9140-2017-0-S-144-158.