Experience of the determination of carbon, sulfur, oxygen and nitrogen in alloys based on niobium on the gas-analyzers of the LECO firm

Alekseev A.V., Rastegayeva G.Yu., Pahomkina T.N.
Alekseev A.V., Rastegayeva G.Yu., Pahomkina T.N. Experience of the determination of carbon, sulfur, oxygen and nitrogen in alloys based on niobium on the gas-analyzers of the LECO firm // Proceedings of VIAM. 2018. No. 1. DOI: 10.18577/2307-6046-2018-0-1-3-3. URL: https://www.viam-works.ru/en/journal/2018/1/3
Keywords
alloys based on Nb, determination of carbon, determination of sulfur, determination of oxygen, determination of nitrogen, method of infrared absorption spectroscopy, melting method in a current of an inert carrier gas.
Abstract

A study was made of the possibility of determining the mass fraction of carbon and sulfur in an alloy based on Nb by burning in an induction furnace a gas analyzer CS-444 from Leco, followed by detection in an infrared cell of a spectrometer. A catalyst is selected, with a specially selected composition, which allows full recovery of carbon and sulfur from the analyzed material. Determination of the content of the oxygen and nitrogen mass fraction in the Nb-based alloy was carried out by reductive melting in a stream of an inert carrier gas, followed by detection of oxygen in an infrared cell and nitrogen in a conductometric cell of a TC-600 from Leco gas analyzer. The catalysts required for the complete extraction of these elements from an Nb-based alloy were selected

Reference list
  1. Kablov E.N. Materialy novogo pokoleniya [Materials of new generation] // Zashhita i bezopasnost. 2014. №4. S. 28–29.
  2. Kablov E.N., Petrushin N.V., Svetlov I.L., Demonis I.M. Nikelevye litejnye zharoprochnye splavy novogo pokoleniya [Nickel foundry heat resisting alloys of new generation] // Aviacionnye materialy i tehnologii. 2012. №S. C. 36–52.
  3. Kablov E.N., Bondarenko Yu.A., Echin A.B., Surova V.A. Razvitie processa napravlennoj kristallizacii lopatok GTD iz zharoprochnyh splavov s monokristallicheskoj i kompozicionnoj strukturoj [Development of process of the directed crystallization of blades of GTE from hot strength alloys with single-crystal and composition structure] // Aviacionnye materialy i tehnologii. 2012. №1. S. 3–8.
  4. Kablov E.N., Sidorov V.V., Kablov D.E., Rigin V.E., Goryunov A.V. Sovremennye tehnologii polucheniya prutkovyh zagotovok iz litejnyh zharoprochnyh splavov novogo pokoleniya [Modern technologies of receiving the bar stock preparations from foundry heat resisting alloys of new generation] // Aviacionnye materialy i tehnologii. 2012. №S. S. 97–105.
  5. Kablov E.N., Svetlov I.L., Efimochkin I.Yu. Vysokotemperaturnye Nb–Si-kompozity [High-temperature Nb-Si-composites] // Vestnik MGTU im. N.E. Baumana. Ser.: Mashinostroenie. 2011. №SP2. S. 164–173.
  6. Min P.G., Sidorov V.V. Opyt pererabotki litejnyh othodov splava ZhS32-VI na nauchno-proizvodstvennom komplekse VIAM po izgotovleniyu lityh prutkovyh (shihtovyh) zagotovok [The experience of GS32-VI alloy scrap recycling at the VIAM scientific and production complex for cast bars production] // Aviacionnye materialy i tehnologii. 2013. №4. S. 20–25.
  7. Sidorov V.V., Timofeeva O.B., Kalitsev V.A., Goryunov A.V. Vliyanie mikrolegirovanija RZM na svojstva i strukturno-fazovye prevrashheniya v intermetallidnom splave VKNA-25-VI [Influence of microalloying of RZM on properties and structural phase changes in intermetallidny alloy VKNA-25-VI] // Aviacionnye materialy i tehnologii. 2012. №4. S. 8–13.
  8. Svetlov I.L., Abuzin Yu.A., Babich B.N. i dr. Vysokotemperaturnye Nb–Si kompozity, uprochnennye silicidami niobiya [High-temperature Nb–Si the composites strengthened by silicides of niobium] // Zhurnal funkcionalnyh materialov. 2007. T. 1. №2. S. 48–52.
  9. Bewlay B.P., Jackon M.R., Zhao H.C. et al. Ultrahigh-Temperature Nb-Silicide-Based Composites // Mrs. Bulletin. Spt., 2003. P. 646–653.
  10. High Temperature Niobium alloy: pat. 7632455 US; publ. 15.12.09.
  11. Lomberg B.S., Ovsepyan S.V., Bakradze M.M., Mazalov I.S. Vysokotemperaturnye zharo-prochnye nikelevye splavy dlya detalej gazoturbinnyh dvigatelej [High-temperature heat resisting nickel alloys for details of gas turbine engines] // Aviacionnye materialy i tehnologii. 2012. №S. S. 52–57.
  12. Lomberg B.S., Ovsepjan S.V., Bakradze M.M. Osobennosti legirovaniya i termicheskoj obrabotki zharoprochnyh nikelevyh splavov dlja diskov gazoturbinnyh dvigatelej novogo pokolenija [Features of alloying and thermal processing of heat resisting nickel alloys for disks of gas turbine engines of new generation] //Aviacionnye materialy i tehnologii. 2010. №2. S. 3–8.
  13. Alekseev A.V., Yakimovich P.V., Min P.G. Opredelenie primesej v splave na osnove Nb metodom ISP-MS. Chast I [Determination of impurities in Nb-based alloy by ICP-MS method. Part I] // Trudy VIAM: elektron. nauch.-tehnich. zhurn. 2015. №6. St. 04. Available at: http://www.viam-works.ru (accessed: December 08, 2017). DOI: 10.18557/2307-6046-2015-0-6-4-4.
  14. Alekseev A.V., Yakimovich P.V., Min P.G. Opredelenie primesej v splave na osnove niobiya metodom ISP-MS. Chast II [Determination of impurity in alloy based on Nb by ICP-MS. Part II] // Trudy VIAM: elektron. nauch.-tehnich. zhurn. 2015. №7. St. 03. Available at: http://www.viam-works.ru (accessed: December 08, 2017). DOI: 10.18557/2307-6046-2015-0-7-3-3.
  15. ASTME E1019-08. Standard Test Methods for Determination of Carbon, Sulfur, Nitrogen, and Oxygen in Steel, Iron, Nickel, and Cobalt Alloys by Various Combustion and Fusion Techniques. 2008. 21 p.